# US 2026/0101727 A1 · Methods of forming semiconductor structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0101727 A1
- Document ID: US20260101727A1
- Status: Published application
- Kind: A1
- Application number: 18/911,056
- Filed: 2024-10-09
- Published: 2026-04-09
- Earliest claimed: 2024-10-09
- Assignees: Nanya Technology Corporation
- Applicants: Nanya Technology Corporation
- Inventors: Wei-Chuan FANG
- Web page: https://patentgrep.com/patent/US20260101727A1

## CPC

- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- H10D 1/68: Capacitors having no potential barriers
- H10D 1/692: {Electrodes}
- H10P 50/282: {of inorganic materials}
- H10P 50/73: {using masks for insulating materials}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present disclosure provides a method of forming a semiconductor structure. The method includes the following operations. A diamond-like carbon hard mask layer is formed on a substrate, in which an absorbance of the diamond-like carbon hard mask layer is smaller than or equal to 0.5. A dielectric anti-reflective coating layer is formed on the diamond-like carbon hard mask layer. A bottom anti-reflective coating layer is formed on the dielectric anti-reflective coating layer.

## Claims

### Claim 1

A method of forming a semiconductor structure, comprising:
forming a diamond-like carbon hard mask layer on a substrate, wherein an absorbance of the diamond-like carbon hard mask layer is smaller than or equal to 0.5;
forming a dielectric anti-reflective coating layer on the diamond-like carbon hard mask layer; and
forming a bottom anti-reflective coating layer on the dielectric anti-reflective coating layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the diamond-like carbon hard mask layer comprises: providing C2H2 and an inert gas; and reacting the C2H2 to form the diamond-like carbon hard mask layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein a ratio of a flow rate of the C2H2 to a flow rate of the inert gas is from 1:20 to 1:50.

### Claim 4 (depends on 2)

The method of claim 2, wherein a flow rate of the C2H2 is from 290 SCCM to 390 SCCM.

### Claim 5 (depends on 1)

The method of claim 1, wherein forming the diamond-like carbon hard mask layer is performed at a pressure from 1.3 Torr to 3.1 Torr.

### Claim 6 (depends on 1)

The method of claim 1, wherein forming the diamond-like carbon hard mask layer is performed at a temperature from 150° C. to 400° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein a stress of the diamond-like carbon hard mask layer is from −750 MPa to −350 MPa.

### Claim 8 (depends on 1)

The method of claim 1, wherein a thickness of the diamond-like carbon hard mask layer is smaller than or equal to 150 nm.

### Claim 9 (depends on 1)

The method of claim 1, wherein an etch selectivity of an oxide material relative to the diamond-like carbon hard mask layer is from 15:1 to 25:1.

### Claim 10

A method of forming a semiconductor structure, comprising:
forming an amorphous carbon hard mask layer on first electrodes of capacitors on a substrate, wherein an absorbance of the amorphous carbon hard mask layer is smaller than or equal to 0.5, and an oxide layer is disposed between the first electrodes;
forming a photoresist layer having an opening on the amorphous carbon hard mask layer; and
etching the amorphous carbon hard mask layer through the opening of the photoresist layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein etching the amorphous carbon hard mask layer is performed till the oxide layer disposed between the first electrodes of the capacitors is exposed, and the method further comprises etching the oxide layer and forming dielectric layers and second electrodes on the first electrodes.

### Claim 12 (depends on 10)

The method of claim 10, further comprising:
before or during forming the photoresist layer having the opening on the amorphous carbon hard mask layer, using a light shining on and reflecting from the amorphous carbon hard mask layer to determine positions of the first electrodes for aligning the opening of the photoresist layer with a position between two of the first electrodes.

### Claim 13 (depends on 10)

The method of claim 10, wherein etching the amorphous carbon hard mask layer comprises using an anisotropic dry etching method.

### Claim 14 (depends on 10)

The method of claim 10, wherein a stress of the amorphous carbon hard mask layer is from −750 MPa to −350 MPa.

### Claim 15 (depends on 10)

The method of claim 10, wherein a thickness of the amorphous carbon hard mask layer is smaller than or equal to 150 nm.