# US 2026/0101625 A1 · Perovskite solar cell and its preparation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0101625 A1
- Document ID: US20260101625A1
- Status: Published application
- Kind: A1
- Application number: 19/219,029
- Filed: 2025-05-27
- Published: 2026-04-09
- Earliest claimed: 2024-10-08
- Assignees: City University of Hong Kong
- Applicants: City University of Hong Kong
- Inventors: Zonglong Zhu; Danpeng Gao; Bo Li
- Web page: https://patentgrep.com/patent/US20260101625A1

## CPC

- H10K 30/85: Layers having high electron mobility, e.g. electron-transporting layers or hole-blocking layers
- C23C 16/407: {of zinc, germanium, cadmium, indium, tin, thallium or bismuth}
- C23C 16/4408: {by purging residual gases from the reaction chamber or gas lines}
- C23C 16/45527: {characterized by the ALD cycle, e.g. different flows or temperatures during half-reactions, unusual pulsing sequence, use of precursor mixtures or auxiliary reactants or activations}
- C23C 16/45557: {Pulsed pressure or control pressure}
- H10K 30/50: Photovoltaic [PV] devices
- H10K 30/82: Transparent electrodes, e.g. indium tin oxide [ITO] electrodes
- H10K 30/88: Passivation; Containers; Encapsulations
- H10K 71/12: using liquid deposition, e.g. spin coating
- H10K 71/40: Thermal treatment, e.g. annealing in the presence of a solvent vapour
- H10K 85/50: Organic perovskites; Hybrid organic-inorganic perovskites [HOIP], e.g. CH3NH3PbI3
- Y02E 10/549: Organic PV cells
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A perovskite solar cell includes an electron transport layer between an anode and a cathode, wherein the electron transport layer comprises of first and second portions of tin oxide (SnOx). A method for preparing the perovskite solar cell includes depositing an electron transport layer having first and second portions of tin oxide (SnOx) on a surface passivated perovskite active layer.

## Claims

### Claim 1

A perovskite solar cell comprising an electron transport layer between an anode and a cathode, wherein the electron transport layer comprises of first and second portions of tin oxide (SnOx).

### Claim 2 (depends on 1)

The perovskite solar cell as claimed in claim 1, wherein the first and the second portions of tin oxide (SnOx) have different stoichiometry.

### Claim 3 (depends on 2)

The perovskite solar cell as claimed in claim 2, wherein the x of SnOx in the first and second portions is from about 1.81 to 1.98.

### Claim 4 (depends on 1)

The perovskite solar cell as claimed in claim 1, wherein the first portion of tin oxide is arranged on the second portion of tin oxide.

### Claim 5 (depends on 4)

The perovskite solar cell as claimed in claim 4, wherein the first and second portions of tin oxide have different thickness.

### Claim 6 (depends on 5)

The perovskite solar cell as claimed in claim 5, wherein the thickness of the first and second portions of tin oxide is in the range from about 2 nm to about 50 nm.

### Claim 7 (depends on 4)

The perovskite solar cell as claimed in claim 4, wherein the thickness of the first portion of tin oxide is less than that of the second portion.

### Claim 8 (depends on 4)

The perovskite solar cell as claimed in claim 4, wherein x of SnOx in the first portion is smaller than that of the second portion.

### Claim 9 (depends on 8)

The perovskite solar cell as claimed in claim 8, wherein x of SnOx in the first portion is about 1.83 and x of SnOx in the second portion is about 1.96.

### Claim 10

The perovskite solar cell as claimed in 7, wherein the thickness of the first portion is about 2 nm to about 10 nm and the thickness of the second portion is about 15 nm to about 50 nm.

### Claim 11 (depends on 1)

The perovskite solar cell as claimed in claim 1 further comprising a passivation layer between the electron transport layer and a perovskite active layer.

### Claim 12 (depends on 11)

The perovskite solar cell as claimed in claim 11, wherein the passivation layer is arranged under the first portion of the electron transport layer.

### Claim 13 (depends on 11)

The perovskite solar cell as claimed in claim 11, wherein the passivation layer comprises phenylethylamine salt and perylene diimide-based compound.

### Claim 14 (depends on 13)

The perovskite solar cell as claimed in claim 13, wherein the phenylethylamine salt is selected from the group consisting of PEAI (phenylethylammonium iodide), PEABr (phenylethylammonium bromide), PEACl (phenylethylammonium chloride), mF-PEAI (meta-fluorophenylethylammonium iodide), o-F-PEAI (ortho-fluorophenylethylammonium iodide), CF3-PEAI (trifluoromethylphenylethylammonium iodide), CH3O-PEAI (4-methoxyphenylethylammonium iodide), and 4F-PEAI (4-fluorophenylethylammonium iodide), and a combination thereof.

### Claim 15 (depends on 13)

The perovskite solar cell as claimed in claim 13, wherein the perylene diimide-based compound is selected from the group consisting of PDINN (N,N′-bis{3-[3-(dimethylamino)propylamino]propyl}perylene-3,4,9,10-tetracarboxylic diimide), PDIN (N,N′-bis{3-[3-(dimethylamino)propyl]amino}perylene-3,4,9,10-tetracarboxylic diimide), PDINO (N,N′-bis{3-[3-(dimethylamino)propyl]amino}perylene-3,4,9,10-tetracarboxylic diimide N-oxide), NDI-N(N,N′-bis{3-[3-(dimethylamino)propyl]amino}naphthalene-1,4,5,8-tetracarboxylic diimide), and a combination thereof.

### Claim 16 (depends on 13)

The perovskite solar cell as claimed in claim 13, wherein the phenylethylamine salt and the perylene diimide-based compound have a molar concentration ratio from about 4:1 to about 1:4.

### Claim 17 (depends on 11)

The perovskite solar cell as claimed in claim 11, wherein the perovskite active layer comprises a perovskite material having a formula of CsxMAyFA1-x-ySnzPb1-zI3-mBrm, with x being 0-0.5, y being 0-0.5, z being 0-0.5, m being 0-1.5.

### Claim 18 (depends on 17)

The perovskite solar cell as claimed in claim 17, wherein the perovskite material is doped with a hole transport material selected from the group consisting of 2PACz, MeO-2PACz (methoxy-2PACz), Me-4PACz (methyl-4PACz), Br-2PACz (bromo-2PACz), CbzBF, 4PADBC, and CbzBT, and a combination thereof.

### Claim 19 (depends on 1)

The perovskite solar cell as claimed in claim 1, wherein the anode comprises a conductive material deposited on a transparent substrate, the conductive material is selected from the group consisting of indium tin oxide (ITO), fluorine-doped tin oxide (FTO), niobium-doped titanium dioxide (NTO), aluminum-doped zinc oxide (AZO), gallium-doped zinc oxide (GZO), and a combination thereof.

### Claim 20 (depends on 1)

The perovskite solar cell as claimed in claim 1, wherein the cathode comprises a metal selected from the group consisting of gold, silver, copper, aluminium, nickel, and a combination thereof.

### Claim 21 (depends on 1)

The perovskite solar cell as claimed in claim 1 is an inverted perovskite solar cell.

### Claim 22 (depends on 1)

A method for preparing the perovskite solar cell as claimed in claim 1, comprising the step of depositing an electron transport layer which comprises of first and second portions of tin oxide (SnOx) on a surface passivated perovskite active layer.

### Claim 23 (depends on 22)

The method as claimed in claim 22, wherein the deposition is conducted by way of atomic layer deposition.

### Claim 24 (depends on 23)

The method as claimed in claim 23, wherein the atomic layer deposition comprises the steps of:
(a) contacting the surface passivated perovskite active layer with a pulse of tin in vapor phase in a reaction space followed by contacting the surface passivated perovskite active layer with a pulse of oxygen in vapor phase in the reaction space to form the first portion of tin oxide; and
(b) contacting the first portion of tin oxide with a pulse of tin in vapor phase in the reaction space followed by contacting the first portion of tin oxide with a pulse of oxygen in vapor phase in the reaction space to form the second portion of tin oxide.

### Claim 25 (depends on 24)

The method as claimed in claim 24, wherein step (a) is repeated for 10 to 50 cycles.

### Claim 26 (depends on 24)

The method as claimed in claim 24, wherein step (b) is repeated for 50 cycles to 500 cycles.

### Claim 27 (depends on 24)

The method as claimed in claim 24, wherein the pulse of tin in vapor phase is in contact with the surface passivated perovskite active layer in step (a) for about 120 ms to about 400 ms.

### Claim 28 (depends on 24)

The method as claimed in claim 24, wherein the pulse of oxygen in vapor phase is in contact with the surface passivated perovskite active layer in step (a) for about 5 ms to about 20 ms.

### Claim 29 (depends on 24)

The method as claimed in claim 24, wherein the pulse of tin in vapor phase is in contact with the first portion of tin oxide in step (b) for about 20 ms to about 100 ms.

### Claim 30 (depends on 24)

The method as claimed in claim 24, wherein the pulse of oxygen in vapor phase is in contact with the first portion of tin oxide in step (b) for about 10 ms to about 40 ms.

### Claim 31 (depends on 24)

The method as claimed in claim 24, wherein each of step (a) and step (b) further includes the step of purging the reaction space.

### Claim 32 (depends on 31)

The method as claimed in claim 31, wherein the step of purging the reaction space comprises of performing purging after application of the pulse of tin in vapor phase and before application of the pulse of oxygen in vapor phase; and performing purging after the application of the pulse of oxygen in vapor phase.

### Claim 33 (depends on 25)

The method as claimed in claim 25, wherein purging the reaction space in step (a) is different between a first cycle and a second cycle.

### Claim 34 (depends on 33)

The method as claimed in claim 33, wherein the number of cycles is divided into a first set, a second set and a third set, the time for purging the reaction space increases from the first set to the third set.

### Claim 35 (depends on 31)

The method as claimed in claim 31, wherein time for purging the reaction space after application of the pulse of tin in vapor phase in step (a) is about 20 seconds.

### Claim 36 (depends on 24)

The method as claimed in claim 24, wherein the atomic layer deposition is conducted at a temperature from about 85° C. to about 125° C.

### Claim 37 (depends on 24)

The method as claimed in claim 24, wherein the tin in vapor phase comprises tetrakis(dimethylamino)tin and the oxygen in vapor phase comprises water.

### Claim 38 (depends on 31)

The method as claimed in claim 31 further comprising the steps of:
(i) providing an anode including a conductive material;
(ii) depositing a perovskite active layer on the anode;
(iii) subjecting the perovskite active layer to surface passivation treatment; and
(iv) providing the cathode on the electron transport layer by way of thermal evaporation.

### Claim 39 (depends on 38)

The method as claimed in claim 38, wherein step (ii) includes the steps of:
providing a precursor solution comprising CsI, FAI, MAI, MABr, PbBr2, PbI2, and SnI2 according to the formula of CsxMAyFA1-x-ySnzPb1-zI3-mBrm, with x being 0-0.5, y being 0-0.5, z being 0-0.5, m being 0-1.5, and a hole transport material;
spin-coating the precursor solution on the anode; and
annealing the spin-coated anode to form the perovskite active layer thereon.

### Claim 40 (depends on 39)

The method as claimed in claim 39, wherein the hole transport material has a concentration of about 0.15 mg/mL to about 1.2 mg/mL in the precursor solution.

### Claim 41 (depends on 38)

The method as claimed in claim 38, wherein step (iii) comprising the steps of:
spin-coating a surface passivating solution including a phenylethylamine salt and a perylene diimide-based compound on the perovskite active layer obtained in step (ii); and
annealing the spin-coated perovskite active layer to form a passivation layer thereon.

### Claim 42 (depends on 41)

The method as claimed in claim 41, wherein the phenylethylamine salt has an initial concentration of about 0.5 mg/mL to about 4 mg/mL, and the perylene diimide-based compound has an initial concentration of about 0.5 mg/mL to about 8 mg/mL.

### Claim 43 (depends on 42)

The method as claimed in claim 42, wherein the phenylethylamine salt and the perylene diimide-based compound have a volume ratio of 1:1.