# US 2026/0101493 A1 · Semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0101493 A1
- Document ID: US20260101493A1
- Status: Published application
- Kind: A1
- Application number: 19/406,269
- Filed: 2025-12-02
- Published: 2026-04-09
- Earliest claimed: 2022-08-02
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Jongmyung YOO
- Web page: https://patentgrep.com/patent/US20260101493A1

## CPC

- H10B 12/033: {the capacitor extending over the transistor}
- H10B 12/315: {with the capacitor higher than a bit line}
- H10D 1/042: {using deposition processes to form electrode extensions}
- H10D 1/696: {comprising multiple layers, e.g. comprising a barrier layer and a metal layer (barrier layers to prevent diffusion of hydrogen or oxygen in perovskite based capacitors H10D1/688)}
- H10D 1/716: {having vertical extensions}
- H10B 12/053: {the transistor being at least partially in a trench in the substrate (vertical transistor in combination with a capacitor formed in a substrate trench H10B12/0383)}
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of manufacturing a semiconductor device includes forming a lower electrode trench extending in a vertical direction on a substrate, and forming a mold structure pattern defining the lower electrode trench, forming a liner film on the lower electrode trench of the mold structure pattern, forming a lower electrode on the liner film within the lower electrode trench of the mold structure pattern, removing a portion of the mold structure pattern to expose a part of a sidewall of the lower electrode, forming a dielectric layer covering an exposed surface of the sidewall of the lower electrode and an exposed surface of a remaining portion of the mold structure pattern and forming an upper electrode covering the dielectric layer.

## Claims

### Claim 1

A method of manufacturing a semiconductor device comprising:
forming a lower electrode trench extending in a vertical direction on a substrate, and forming a mold structure pattern defining the lower electrode trench;
forming a liner film on the lower electrode trench of the mold structure pattern;
forming a lower electrode on the liner film within the lower electrode trench of the mold structure pattern;
removing a portion of the mold structure pattern to expose a part of a sidewall of the lower electrode;
forming a dielectric layer covering an exposed surface of the sidewall of the lower electrode and an exposed surface of a remaining portion of the mold structure pattern; and
forming an upper electrode covering the dielectric layer,
wherein the lower electrode comprises a first metal nitride comprising a first metal,
wherein the liner film comprises a second metal nitride comprising a second metal,
wherein a first ratio of the first metal in the first metal nitride is higher than a second ratio of the second metal in the second metal nitride, and
wherein a third ratio of nitrogen atoms in the first metal nitride is lower than a fourth ratio of nitrogen atoms in the second metal nitride.

### Claim 2 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein the third ratio of nitrogen atoms in the first metal nitride is about 30 at% or higher and is less than about 50 at%, and
wherein the fourth ratio of nitrogen atoms in the second metal nitride is about 50 at% or higher and is about 70 at% or less.

### Claim 3 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein forming the liner film onto the lower electrode trench of the mold structure pattern comprises forming the liner film by applying the second metal nitride by a Chemical Vapor Deposition (CVD), Plasma Enhanced Chemical Vapor Deposition (PECVD), Metal Organic Chemical Vapor Deposition (MOCVD), or Atomic Layer Deposition (ALD) process.

### Claim 4 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein forming the lower electrode on the liner film within the lower electrode trench of the mold structure pattern comprises forming the lower electrode by applying the first metal nitride by a Chemical Vapor Deposition (CVD), Plasma Enhanced Chemical Vapor Deposition (PECVD), Metal Organic Chemical Vapor Deposition (MOCVD), or Atomic Layer Deposition (ALD) process.

### Claim 5 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein forming the liner film comprises forming a pre-liner film by applying the second metal nitride on the lower electrode trench;
wherein forming the lower electrode comprises forming a pre-lower electrode on the pre-liner film within the lower electrode trench of the mold structure pattern; and
wherein the method further comprises removing portions of the pre-liner film and the pre-lower electrode to expose an upper surface of the mold structure pattern.

### Claim 6 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein a top surface of the liner film is on a same plane as a top surface of the lower electrode.

### Claim 7 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein the mold structure pattern comprises a first mold pattern, a lower supporter, a second mold pattern, and an upper supporter sequentially stacked, and
wherein the first mold pattern and the second mold pattern comprise an oxide film, a nitride film, or a combination thereof.

### Claim 8 (depends on 7)

The method of manufacturing a semiconductor device of claim 7, wherein a portion of the mold structure pattern removed to expose a part of a sidewall of the lower electrode comprises the first mold pattern and the second mold pattern.

### Claim 9 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein a horizontal width of an upper portion of the lower electrode surrounded by the liner film is greater than a horizontal width of a lower portion of the lower electrode, the lower portion of the lower electrode not being surrounded by the liner film.

### Claim 10 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein at least some portion of side surfaces of the liner film have a slope different from that of at least side surfaces of the lower electrode.

### Claim 11

A method of manufacturing a semiconductor device comprising:
forming a lower electrode trench extending in a vertical direction on a substrate, and forming a mold structure pattern defining the lower electrode trench;
forming a pre-liner film on the lower electrode trench of the mold structure pattern;
forming a pre-lower electrode on the pre-liner film within the lower electrode trench of the mold structure pattern;
removing portions of the pre-liner film and the pre-lower electrode to expose an upper surface of the mold structure pattern, thereby forming a liner film and a lower electrode;
removing a portion of the mold structure pattern to expose a part of a sidewall of the lower electrode;
forming a dielectric layer covering an exposed surface of the sidewall of the lower electrode and an exposed surface of a remaining portion of the mold structure pattern; and
forming an upper electrode covering the dielectric layer,
wherein the lower electrode comprises a first metal nitride comprising a first metal,
wherein the liner film comprises a second metal nitride comprising a second metal,
wherein a first ratio of the first metal in the first metal nitride is higher than a second ratio of the second metal in the second metal nitride, and
wherein a third ratio of nitrogen atoms in the first metal nitride is lower than a fourth ratio of nitrogen atoms in the second metal nitride.

### Claim 12 (depends on 11)

The method of manufacturing a semiconductor device of claim 11, wherein a horizontal width of an upper portion of the lower electrode surrounded by the liner film is greater than a horizontal width of a lower portion of the lower electrode, the lower portion of the lower electrode not being surrounded by the liner film.

### Claim 13 (depends on 11)

The method of manufacturing a semiconductor device of claim 11, wherein a first point corresponding to a largest horizontal width of the liner film is located farther from the substrate than a second point corresponding to a smallest horizontal width of the liner film.

### Claim 14 (depends on 11)

The method of manufacturing a semiconductor device of claim 11, wherein a process of applying the second metal nitride to form the pre-liner film uses the same method as a process of applying the first metal nitride to form the pre-lower electrode.

### Claim 15 (depends on 11)

The method of manufacturing a semiconductor device of claim 11, an upper surface of the pre-liner film is covered by the pre-lower electrode.

### Claim 16 (depends on 11)

The method of manufacturing a semiconductor device of claim 11, wherein a top surface of the liner film is on a same plane as a top surface of the lower electrode.

### Claim 17 (depends on 11)

The method of manufacturing a semiconductor device of claim 11, wherein the mold structure pattern comprises a first mold pattern, a lower supporter, a second mold pattern, and an upper supporter sequentially stacked, and
wherein a portion of the mold structure pattern removed to expose a part of a sidewall of the lower electrode comprises the first mold pattern and the second mold pattern.

### Claim 18

A method of manufacturing a semiconductor device comprising:
forming a lower electrode trench extending in aa vertical direction on a substrate, and forming a mold structure pattern defining the lower electrode trench;
forming a liner film on the lower electrode trench of the mold structure pattern;
forming a lower electrode on the liner film within the lower electrode trench of the mold structure pattern;
removing a portion of the mold structure pattern to expose a part of a sidewall of the lower electrode;
forming a dielectric layer covering an exposed surface of the sidewall of the lower electrode and an exposed surface of a remaining portion of the mold structure pattern; and
forming an upper electrode covering the dielectric layer,
wherein the lower electrode comprises a first metal nitride comprising a first metal,
wherein the liner film comprises a second metal nitride comprising a second metal,
wherein the first metal and the second metal comprise a same type of metal element,
wherein a first ratio of the first metal in the first metal nitride is higher than a second ratio of the second metal in the second metal nitride,
wherein a third ratio of nitrogen atoms in the first metal nitride is about 30 at% or higher and is less than about 50 at%, and
wherein a fourth ratio of nitrogen atoms in the second metal nitride is about 50 at% or higher and is about 70 at% or less.

### Claim 19 (depends on 18)

The method of manufacturing a semiconductor device of claim 18, wherein the mold structure pattern comprises a first mold pattern, a lower supporter, a second mold pattern, and an upper supporter sequentially stacked,
wherein the lower supporter and the upper supporter each comprise a silicon nitride film (SiN), a silicon carbon nitride film (SiCN), a silicon boron nitride film (SiBN), or a combination thereof,
wherein the first mold pattern and the second mold pattern each comprise an oxide film, a nitride film, or a combination thereof, and
wherein the first mold pattern and the second mold pattern have higher etch rates than the lower supporter and the upper supporter with respect to an etchant including ammonium fluoride (NH4F), hydrofluoric acid (HF), and water.

### Claim 20 (depends on 18)

The method of manufacturing a semiconductor device of claim 18, wherein a top surface of the liner film is on a same plane as a top surface of the lower electrode, and
wherein a horizontal width of an upper portion of the lower electrode surrounded by the liner film is greater than a horizontal width of a lower portion of the lower electrode, the lower portion of the lower electrode not being surrounded by the liner film.