# US 2026/0100478 A1 · Solid-state electrolyte slurry mixing and coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0100478 A1
- Document ID: US20260100478A1
- Status: Published application
- Kind: A1
- Application number: 19/347,625
- Filed: 2025-10-01
- Published: 2026-04-09
- Earliest claimed: 2024-10-03
- Assignees: A123 Systems, Inc.
- Applicants: A123 Systems LLC
- Inventors: Ethan Boeding; John Flynn; David Laughman
- Web page: https://patentgrep.com/patent/US20260100478A1

## CPC

- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 4/0404: {by coating on electrode collectors}
- H01M 10/0562: Solid materials
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 50/414: Synthetic resins, e.g. thermoplastics or thermosetting resins
- H01M 50/426: Fluorocarbon polymers
- H01M 50/431: Inorganic material
- H01M 50/443: Particulate material
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Methods are disclosed herein for preparing a smooth solid electrolyte slurry and coating the slurry onto a substrate to form a separator of a solid-state battery. In one example, the method includes combining solid electrolyte, solvent, and a binder solution to form a slurry, followed by mixing the slurry to form a smooth slurry. Mixing the slurry includes a combination of mixing under non-vacuum conditions, mixing under vacuum conditions, and milling under vacuum and/or non-vacuum conditions.

## Claims

### Claim 1

A method of preparing a solid state battery separator, comprising:
pre-mixing a first portion of a solid electrolyte and a solvent to form a mixture;
first mixing a binder solution, a second portion of the solid electrolyte, and the mixture under non-vacuum conditions to form a slurry;
second mixing the slurry under vacuum conditions to form a mixed slurry;
alternating milling and second mixing the mixed slurry to form a smooth slurry with particles smaller than a threshold particle size;
coating a substrate with the smooth slurry to produce a coated substrate; and
drying the coated substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein milling occurs under vacuum conditions.

### Claim 3 (depends on 1)

The method of claim 1, wherein milling occurs under non-vacuum conditions.

### Claim 4 (depends on 1)

The method of claim 1, wherein the threshold particle size is within a range of 1-50 μm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the smooth slurry is approximately 50-80 wt % solids.

### Claim 6 (depends on 1)

The method of claim 1, wherein the solid electrolyte is an ionically conductive powder, the solvent is a non-polar solvent, and the binder solution comprises a dilution solvent and a rubber binder.

### Claim 7 (depends on 6)

The method of claim 6, wherein the rubber binder is nitrile butadiene rubber, hydrogenated nitrile butadiene rubber, styrene-butadiene copolymer, styrene-butadiene-styrene, polyvinylidene fluoride, and/or hexafluoroporpylene.

### Claim 8 (depends on 1)

The method of claim 1, wherein the threshold particle size is one third or less of a coating thickness of the smooth slurry on the substrate.

### Claim 9

A method of preparing a casted separator, comprising:
combining a solid electrolyte, a solvent, and a binder solution to form a slurry;
mixing the slurry to form a smooth slurry, wherein mixing the slurry includes second mixing under vacuum conditions, followed by basket milling under vacuum and/or non-vacuum conditions;
coating the smooth slurry onto a substrate to form a coated substrate; and
drying the coated substrate to form the casted separator.

### Claim 10 (depends on 9)

The method of claim 9, wherein mixing further includes third mixing under vacuum conditions after basket milling under vacuum and/or non-vacuum conditions and before coating.

### Claim 11 (depends on 9)

The method of claim 9, wherein coating includes slot-die coating, curtain coating, slide coating, knife over roll coating, tape casting, or comma coating.

### Claim 12 (depends on 9)

The method of claim 9, wherein the solid electrolyte is sulfide powder, the solvent comprises hexyl butyrate, toluene, xylene, anisole, heptane, or butyl butyrate, the binder solution comprises a non-polar solvent and a rubber binder, and the substrate is an aluminum foil, an anode, or a cathode.

### Claim 13 (depends on 9)

The method of claim 9, wherein the casted separator is incorporated in a solid-state battery.

### Claim 14 (depends on 9)

The method of claim 9, wherein second mixing under vacuum conditions and basket milling under non-vacuum conditions are repeated in an alternating pattern until a maximum particle size of the smooth slurry is less than a threshold particle size and a viscosity of the smooth slurry is less than a threshold viscosity.

### Claim 15 (depends on 14)

The method of claim 14, wherein the threshold viscosity is within a range of 1-50 μm.

### Claim 16 (depends on 14)

The method of claim 14, wherein the threshold particle size is approximately one third or less of a thickness of the casted separator.

### Claim 17

A method of mixing a slurry for a solid state battery separator, comprising:
first mixing a solvent, a solid electrolyte, and a binder solution under non-vacuum conditions to form a slurry;
second mixing the slurry under vacuum conditions to form a mixed slurry;
basket milling the mixed slurry under non-vacuum conditions to form a milled slurry;
if the largest particle size of the milled slurry is not less than a threshold particle size, repeatedly second mixing the milled slurry under vacuum conditions followed by basket milling the milled slurry under non-vacuum conditions until the largest particle size of the milled slurry is less than the threshold particle size; and
third mixing the milled slurry under vacuum conditions to form a smooth slurry with a viscosity below a threshold viscosity.

### Claim 18 (depends on 17)

The method of claim 17, wherein the method further comprises coating an aluminum foil, an anode, or a cathode with the smooth slurry to form a coated substrate and drying the coated substrate to form a casted separator.

### Claim 19 (depends on 18)

The method of claim 18, wherein the threshold particle size is approximately one third or less of a thickness of the casted separator.

### Claim 20 (depends on 17)

The method of claim 17, wherein the threshold particle size is within a range of 1-50 μm.