# US 2026/0100382 A1 · Composite current collector and its preparation method, electrode and battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0100382 A1
- Document ID: US20260100382A1
- Status: Published application
- Kind: A1
- Application number: 19/405,796
- Filed: 2025-12-02
- Published: 2026-04-09
- Earliest claimed: 2023-06-06
- Assignees: REPT BATTERO Energy Co., Ltd.; Shanghai Ruipu Energy Co., Ltd.
- Applicants: Rept Battero Energy Co., Ltd.; Shanghai Ruipu Energy Co., Ltd.
- Inventors: Hui CAO; Xuexiang SHAO; Min HOU; Tingting LI; Chan LIU
- Web page: https://patentgrep.com/patent/US20260100382A1

## CPC

- C23C 14/20: on organic substrates
- H01M 4/668: {Composites of electroconductive material and synthetic resins}
- C23C 14/24: Vacuum evaporation
- C23C 28/00: Coating for obtaining at least two superposed coatings either by methods not provided for in a single one of groups C23C2/00 - C23C26/00 or by combinations of methods provided for in subclasses C23C and C25C or C25D
- C23C 28/02: only coatings {only including layers} of metallic material
- C23C 28/021: {including at least one metal alloy layer}
- C23C 28/023: {only coatings of metal elements only}
- C25D 7/00: Electroplating characterised by the article coated
- H01M 4/662: {Alloys (collectors of lead alloys H01M4/685)}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 4/82: Multi-step processes for manufacturing carriers for lead-acid accumulators
- Y02E 60/10: Energy storage using batteries
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to a composite current collector and its preparation method, electrodes, and batteries. The composite current collector includes an insulating substrate, a first metal layer set on both surfaces of the thickness direction of the insulating substrate, and a second metal layer set on the surface away from the insulating substrate on the first metal layer. Multiple colloidal particles are attached to the surface of the first metal layer away from the insulating substrate, with the colloidal particles evenly distributed. The second metal layer is set on the first metal layer, and the second metal layer encapsulates the evenly distributed colloidal particles. By setting the composite current collector with specific structures of the colloidal particles, it overcomes the issues of low electrode peel strength and capacity drop in long cycle batteries, significantly enhancing the stability of long cycle battery electrodes.

## Claims

### Claim 1

A composite current collector, characterized in that the composite current collector comprises an insulating substrate, a first metal layer provided on both surfaces in the thickness direction of the insulating substrate, and a second metal layer provided on the surface of the first metal layer away from the insulating substrate;
The first metal layer has a plurality of spaced-apart colloidal particles attached to the surface of the side of the first metal layer away from the insulating substrate.

### Claim 2 (depends on 1)

The composite current collector according to claim 1, characterized in that the thickness of the insulating substrate is 1 to 20 μm;
In the thickness direction of the insulating substrate, the thickness of the first metal layer located on one side of the insulating substrate is 0.1 to 500 nm;
In the thickness direction of the insulating substrate, the thickness of the second metal layer located on the side of the first metal layer away from the insulating substrate is 0.05 to 3 μm.

### Claim 3 (depends on 1)

The composite current collector according to claim 1, characterized in that the metal material of the first and second metal layers independently includes any one or at least two combinations of gold, silver, copper, zinc, chromium, aluminum, nickel and tungsten.

### Claim 4 (depends on 1)

The composite current collector according to claim 1, characterized in that the material of the colloidal particles comprises any one or a combination of at least two of styrene-butadiene rubber, polytetrafluoroethylene, polyvinylidene fluoride, polyolefin, polyacrylic acid, polyacrylonitrile, fluorinated rubber and polyurethane;
The density of the colloidal particles attached to the first metal layer is 100 to 400 per square inch.

### Claim 5 (depends on 1)

The composite current collector according to claim 1, characterized in that the colloidal particles adhere to the surface of the first metal layer, with at least a portion of each colloidal particle located within the second metal layer; and along the thickness direction of the insulating substrate, at least a portion of each colloidal particle is exposed on the surface of the second metal layer away from the insulating substrate.

### Claim 6 (depends on 1)

A method for preparing the composite current collector according to claim 1, characterized in that the preparation method comprises the following steps:
(1) Deposit a first metal layer on at least one surface in the thickness direction of the insulating substrate;
(2) Roll the colloidal solution on the surface of the first metal layer away from the insulating substrate so as to attach and form colloidal particles on the surface of the first metal layer;
(3) Deposit a second metal layer on the surface of the first metal layer attached to the side away from the insulating substrate to obtain the composite current collector.

### Claim 7 (depends on 6)

The preparation method according to claim 6, characterized in that the roller coating in step (2) is carried out by a mesh roller;
The mesh number of the mesh roller is 100˜400 mesh.

### Claim 8 (depends on 6)

The preparation method according to claim 6, characterized in that the deposition in step (1) is carried out by vacuum evaporation;
The deposition described in step (3) is carried out by electroplating.

### Claim 9 (depends on 1)

An electrode, characterized in that the electrode contains a composite current collector as claimed in claim 1.

### Claim 10 (depends on 1)

A battery, characterized in that the battery contains a composite current collector or an electrode as claimed in claim 1.