# US 2026/0100360 A1 · Positive electrode active material, positive electrode, secondary battery, electronic device, and vehicle

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0100360 A1
- Document ID: US20260100360A1
- Status: Published application
- Kind: A1
- Application number: 19/365,357
- Filed: 2025-10-22
- Published: 2026-04-09
- Earliest claimed: 2020-04-10
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Applicants: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Kunihiko SUZUKI; Yohei MOMMA; Mayumi MIKAMI; Tatsuyoshi TAKAHASHI; Yuji IWAKI
- Web page: https://patentgrep.com/patent/US20260100360A1

## CPC

- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01G 11/06: with one of the electrodes allowing ions to be reversibly doped thereinto, e.g. lithium ion capacitors [LIC]
- H01G 11/30: characterised by their material
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode active material with high charge and discharge capacity is provided. A positive electrode active material with high charge and discharge voltage is provided. A secondary battery which hardly deteriorates is provided. A highly safe power storage device is provided. A novel secondary battery is provided. The positive electrode active material contains cobalt, oxygen, and fluorine and includes a bond of the cobalt and the fluorine in a surface portion or the vicinity of a grain boundary. By having the bond with fluorine, at least part of cobalt is high-spin (paramagnetic) Co2+. Thus, in ESR analysis, the spin concentration at 113 K is higher than the spin concentration at 300 K by 1.1×10−5 spins/g or more.

## Claims

### Claim 1

(canceled)

### Claim 2

A manufacturing method of a positive electrode active material, comprising the steps of:
mixing a lithium source and a cobalt source;
performing a heating of the first mixture to obtain a lithium cobalt oxide;
mixing the lithium cobalt oxide and a fluorine source; and
performing a heating of the second mixture,
wherein the heating of the first mixture is performed at a temperature higher than or equal to 800° C. and lower than 1100° C., and for longer than or equal to 2 hours and shorter than or equal to 20 hours, and
wherein when an approximate straight line with three or more measured values at temperatures of higher than or equal to 113 K and lower than or equal to 300 K is drawn in a graph of the inverse of the temperature and a spin concentration per cobalt ion, the slope of the straight line is more than or equal to 5×10−6 and less than or equal to 4×10−5.

### Claim 3 (depends on 2)

The manufacturing method of a positive electrode active material according to claim 2, wherein the heating of the second mixture is performed at a temperature higher than or equal to 500° C. and lower than 1130° C.

### Claim 4 (depends on 2)

The manufacturing method of a positive electrode active material according to claim 2, wherein the positive electrode active material comprises a bond of the cobalt and the fluorine in a surface portion or a vicinity of a grain boundary.

### Claim 5

A manufacturing method of a positive electrode active material, comprising the steps of:
mixing a lithium source and a cobalt source;
performing a heating of the first mixture to obtain a lithium cobalt oxide;
mixing the lithium cobalt oxide and a fluorine source; and
performing a heating of the second mixture,
wherein the heating of the first mixture is performed at a temperature higher than or equal to 800° C. and lower than 1100° C., and for longer than or equal to 2 hours and shorter than or equal to 20 hours, and
wherein in a range of a g value obtained in an electron spin resonance spectrum of the positive electrode active material of greater than or equal to 2.068 and less than or equal to 2.233, a spin concentration at a temperature of 113 K is higher than a spin concentration at a temperature of 300 K by 1.1×10−5 spins/g or more.

### Claim 6 (depends on 5)

The manufacturing method of a positive electrode active material according to claim 5, wherein the heating of the second mixture is performed at a temperature higher than or equal to 500° C. and lower than 1130° C.

### Claim 7 (depends on 5)

The manufacturing method of a positive electrode active material according to claim 5, wherein the positive electrode active material comprises a bond of the cobalt and the fluorine in a surface portion or a vicinity of a grain boundary.

### Claim 8

A manufacturing method of a positive electrode active material, comprising the steps of:
mixing a lithium source and a cobalt source;
performing a heating of the first mixture to obtain a lithium cobalt oxide;
mixing the lithium cobalt oxide and a fluorine source; and
performing a heating of the second mixture,
wherein the heating of the first mixture is performed at a temperature higher than or equal to 800° C. and lower than 1100° C., and for longer than or equal to 2 hours and shorter than or equal to 20 hours, and
wherein in a range of a g value obtained in an electron spin resonance spectrum of the positive electrode active material of greater than or equal to 2.068 and less than or equal to 2.233, a difference between a spin concentration at a temperature of 300K and a spin concentration at a temperature of 113 K is higher than or equal to 4.0×10−5 spins/g.

### Claim 9 (depends on 8)

The manufacturing method of a positive electrode active material according to claim 8, wherein the heating of the second mixture is performed at a temperature higher than or equal to 500° C. and lower than 1130° C.

### Claim 10 (depends on 8)