# US 2026/0099094 A1 · Photoresist coating method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0099094 A1
- Document ID: US20260099094A1
- Status: Published application
- Kind: A1
- Application number: 18/931,015
- Filed: 2024-10-29
- Published: 2026-04-09
- Earliest claimed: 2024-10-09
- Assignees: United Semiconductor (Xiamen) Co., Ltd.
- Applicants: United Semiconductor(Xiamen)Co., Ltd.
- Inventors: Cheng Qun Fang; XIONGWU HE; QingZhang Zhang; WEN YI TAN
- Web page: https://patentgrep.com/patent/US20260099094A1

## CPC

- G03F 7/162: {Coating on a rotating support, e.g. using a whirler or a spinner}
- G03F 7/168: {Finishing the coated layer, e.g. drying, baking, soaking}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

The invention provides a photoresist coating method, which comprises the following steps: providing a wafer, keeping the wafer at a first rotation speed, spraying a photoresist on a surface of the wafer, performing a high rotation speed step, increasing the rotation speed of the wafer to a second rotation speed, and moving part of the photoresist to an edge region on the wafer, performing a first wafer edge cleaning step on the edge region of the wafer, reducing the rotation speed of the wafer to a third rotation speed, and performing a second wafer edge cleaning step on the edge region of the wafer.

## Claims

### Claim 1

A photoresist coating method, characterized in that:
providing a wafer to maintain in a first rotation speed;
spraying a photoresist on a surface of the wafer;
performing a high rotation speed step to increase the rotation speed of the wafer to a second rotation speed, and moving part of the photoresist to an edge region on the wafer;
performing a first wafer edge cleaning step on the edge region of the wafer after the above steps are performed;
reducing the rotation speed of the wafer to a third rotation speed after the above steps are performed; and
performing a second wafer edge cleaning step on the edge region of the wafer after the above steps are performed.

### Claim 2 (depends on 1)

The photoresist coating method according to claim 1, wherein the first wafer edge cleaning step is performed within 10 seconds after the rotation speed of the wafer is increased to the second rotation speed.

### Claim 3 (depends on 1)

The photoresist coating method according to claim 1, wherein after the first wafer edge cleaning step, the rotation speed is reduced to the third rotation speed and maintained at the third rotation speed for more than 10 seconds.

### Claim 4 (depends on 1)

The photoresist coating method according to claim 1, wherein a photoresist bump is formed in the edge region of the wafer after the rotation speed of the wafer is increased to the second rotation speed.

### Claim 5 (depends on 4)

The photoresist coating method according to claim 4, wherein the photoresist bump is removed after the first wafer edge cleaning step.

### Claim 6 (depends on 1)

The photoresist coating method according to claim 1, wherein the photoresist is in a flowable state when the first wafer edge cleaning step is performed.

### Claim 7 (depends on 1)

The photoresist coating method according to claim 1, wherein the photoresist is in a dry state during the second wafer edge cleaning step.

### Claim 8 (depends on 1)

The photoresist coating method according to claim 1, wherein before spraying the photoresist on the wafer, a solvent is sprayed on the wafer, and then the photoresist is sprayed and dissolved in the solvent.

### Claim 9 (depends on 1)

The photoresist coating method according to claim 1, wherein before the first wafer edge cleaning step, one side surface of the wafer in the edge region is covered by the photoresist.

### Claim 10 (depends on 9)

The photoresist coating method according to claim 9, wherein after the first wafer edge cleaning step is completed, the side surface in the edge region of the wafer is exposed.

### Claim 11 (depends on 1)

The photoresist coating method according to claim 1, wherein the first rotation speed is between 500 RPM and 1000 RPM, the second rotation speed is between 2500 RPM and 3500 RPM, and the third rotation speed is between 800 RPM and 1200 RPM.

### Claim 12 (depends on 1)

The photoresist coating method according to claim 1, wherein when the wafer is maintained at the first rotation speed, a thickness of the photoresist is between 1700 angstroms and 2300 angstroms.

### Claim 13 (depends on 1)

The photoresist coating method according to claim 1, wherein when the wafer is maintained at the second rotation speed, a thickness of the photoresist is between 400 angstroms and 600 angstroms.

### Claim 14 (depends on 13)

The photoresist coating method according to claim 13, wherein when the wafer is maintained at the third rotation speed, a thickness of the photoresist is between 300 angstroms and 500 angstroms, and at this time, the thickness of the photoresist is smaller than the thickness of the photoresist when the wafer is maintained at the second rotation speed.

### Claim 15 (depends on 1)

The photoresist coating method according to claim 1, wherein after the first wafer edge cleaning step is completed, a central region of the wafer is covered with the photoresist, and the photoresist in the central region has an uneven surface.

### Claim 16 (depends on 15)

The photoresist coating method according to claim 15, wherein after the first wafer edge cleaning step, an interface between the central region and the edge region of the wafer has a stepped cross-sectional structure.

### Claim 17 (depends on 15)

The photoresist coating method according to claim 15, wherein the wafer comprises a pattern, wherein the pattern is located in the central region but not in the edge region.

### Claim 18 (depends on 1)

The photoresist coating method according to claim 1, wherein after the second wafer edge cleaning step is completed, a central region and the edge region of the wafer are covered with the photoresist, and the photoresists in the central region and the edge region have a flat surface.