# US 2026/0099089 A1 · Reflective mask blank and method for manufacturing reflective mask blank

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0099089 A1
- Document ID: US20260099089A1
- Status: Published application
- Kind: A1
- Application number: 19/347,150
- Filed: 2025-10-01
- Published: 2026-04-09
- Earliest claimed: 2024-10-03
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Applicants: Shin-Etsu Chemical Co., Ltd.
- Inventors: Takuro KOSAKA; Yukio INAZUKI; Taiga OGOSE
- Web page: https://patentgrep.com/patent/US20260099089A1

## CPC

- G03F 1/24: Reflection masks; Preparation thereof
- G03F 1/54: Absorbers, e.g. of opaque materials
- G03F 1/58: having two or more different absorber layers, e.g. stacked multilayer absorbers
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A reflective mask blank used in EUV lithography using EUV light as exposure light comprising at least a substrate 10; a multilayer reflective film 50 that is formed on the substrate 10 and reflects exposure light; and a multilayer film 200 containing tantalum (Ta). The multilayer film 200 has a TaN part 210, a TaO part 230, and a Ta part 220 provided between the TaN part 210 and the TaO part 230. A density of the Ta part 220 is higher than densities of the TaN part 210 and the TaO part 230. The density of the Ta part 220 is 13 g/cm3 or more.

## Claims

### Claim 1

A reflective mask blank used in EUV lithography using EUV light as exposure light comprising at least a substrate; a multilayer reflective film that is formed on the substrate and reflects exposure light; and a multilayer film containing tantalum (Ta),
wherein the multilayer film has a TaN part, a TaO part, and a Ta part provided between the TaN part and the TaO part,
wherein a density of the Ta part is higher than densities of the TaN part and the TaO part, and
wherein the density of the Ta part is 13 g/cm3 or more.

### Claim 2 (depends on 1)

The reflective mask blank according to claim 1,
wherein the TaN part, the Ta part, and the TaO part are laminated in this order from the substrate side in the multilayer film.

### Claim 3 (depends on 1)

The reflective mask blank according to claim 1,
wherein a film thickness of the Ta part is 1 nm or more and less than 3 nm.

### Claim 4 (depends on 1)

The reflective mask blank according to claim 1,
wherein the TaN part is substantially free of oxygen and contains less than 70 atom % of tantalum (Ta) and more than 30 atom % of nitrogen (N).

### Claim 5 (depends on 1)

The reflective mask blank according to claim 1,
wherein the TaO part is substantially free of nitrogen (N), and contains less than 70 atom % of tantalum (Ta) and more than 30 atom % of oxygen (O) or wherein the TaO part contains less than 5 atom % of any one or more kinds of boron (B), carbon (C), hydrogen (H), and silicon (Si) in addition to tantalum (Ta) and oxygen (O).

### Claim 6 (depends on 1)

The reflective mask blank according to claim 1,
wherein the Ta part contains substantially no element other than tantalum (Ta), or
wherein a total content of nitrogen (N) and oxygen (O) is less than 20 atom % in the Ta part.

### Claim 7 (depends on 1)

The reflective mask blank according to claim 1,
wherein the multilayer film functions as an absorber film.

### Claim 8 (depends on 7)

The reflective mask blank according to claim 7 further comprising a hard mask film that is used as an etching mask during processing of the multilayer film functioning as the absorber film,
wherein the hard mask film contains chromium (Cr).

### Claim 9 (depends on 1)

The reflective mask blank according to claim 1,
wherein the multilayer film has a first multilayer film having a first TaN part, a first TaO part, and a first Ta part provided between the first TaN part and the first TaO part, and a second multilayer film having a second TaN part, a second TaO part, and a second Ta part provided between the second TaN part and the second TaO part,
wherein the first multilayer film functions as an absorber film,
wherein the second multilayer film functions as a hard mask film used as an etching mask during processing of the first multilayer film that is the absorber film,
wherein a film thickness of the first multilayer film is 55 nm or more and less than 70 nm, and
wherein a film thickness of the second multilayer film is 20 nm or less.

### Claim 10 (depends on 1)

A method for manufacturing the reflective mask blank according to claim 1,
wherein the Ta part is formed between the TaN part and the TaO part by forming a film of Ta under oxygen-and nitrogen-free atmosphere.

### Claim 11 (depends on 10)

The method for manufacturing the reflective mask blank according to claim 10,
wherein the film of Ta is formed under the oxygen-and nitrogen-free atmosphere to form the Ta part after the TaN part is formed, and
wherein a surface of the Ta part on a side away from the substrate is oxidized to form the TaO part.