# US 2026/0098334 A1 · Method for making alloy thin film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0098334 A1
- Document ID: US20260098334A1
- Status: Published application
- Kind: A1
- Application number: 19/415,938
- Filed: 2025-12-11
- Published: 2026-04-09
- Earliest claimed: 2023-06-13
- Assignees: Jiangsu Leadmicro Nano-Technology Co.,Ltd.
- Applicants: Jiangsu Leadmicro Nano Technology Co.,Ltd.
- Inventors: Xiang LI; Weimin LI; Hongxia YUAN; Ke MI; Suochang XU; Xuebo WANG; Hui QIANG; Ping HAN
- Web page: https://patentgrep.com/patent/US20260098334A1

## CPC

- C23C 16/06: characterised by the deposition of metallic material
- H10D 64/01: Manufacture or treatment
- C23C 16/45527: {characterized by the ALD cycle, e.g. different flows or temperatures during half-reactions, unusual pulsing sequence, use of precursor mixtures or auxiliary reactants or activations}
- C23C 16/45544: {characterized by the apparatus}
- C23C 16/4557: {Heated nozzles}
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for making an alloy thin film, includes: providing a reaction chamber, wherein a spraying device and a supporting platform are disposed in the reaction chamber; disposing a pre-processed structure on a surface of the supporting platform; forming an alloy thin film with a characteristic atomic ratio of a first element to an M-th element on a surface of the pre-processed structure, wherein the spraying device is set to have a characteristic temperature, a characteristic distance is set between the spraying device and the supporting platform, a flow-stabilizing device is set to have a characteristic flow, a first precursor to an M-th precursor are introduced into the reaction chamber, and M is an integer greater than or equal to 2; and adjusting the characteristic atomic ratio by adjusting any one or more selected from the group consisting of the characteristic temperature, the characteristic distance, and the characteristic flow.

## Claims

### Claim 1

A method for making an alloy thin film comprising a first element to an M-th element, comprising:
providing a reaction chamber, wherein the reaction chamber is provided with a spraying device and a supporting platform;
disposing a pre-processed structure on a surface of the supporting platform;
forming an alloy thin film with a characteristic atomic ratio of the first element to the M-th element on a surface of the pre-processed structure, comprising:
setting the spraying device to have a characteristic temperature;
setting a characteristic distance between the spraying device and the supporting platform;
setting a flow-stabilizing device to have a characteristic flow rate; and
introducing a first precursor to an M-th precursor into the reaction chamber through the spraying device under conditions of the characteristic temperature, the characteristic distance, and the characteristic flow rate; wherein M is an integer greater than or equal to 2; and any m-th precursor comprises an m-th element, and m is an integer greater than or equal to 1 and less than or equal to M; and
adjusting the characteristic atomic ratio by adjusting any one or more selected from the group consisting of the characteristic temperature, the characteristic distance, and the characteristic flow rate.

### Claim 2 (depends on 1)

The method for making the alloy thin film according to claim 1, wherein any m1-th element and any m2-th element of the first element to the M-th element have different atomic activity, each of m1 and m2 is the integer greater than or equal to 1 and less than or equal to M, and m1 is not equal to m2; and
the characteristic atomic ratio of the m1-th element to the m2-th element increases as the characteristic temperature increases, the characteristic atomic ratio of the m1-th element to the m2-th element decreases as the characteristic distance increases, and the characteristic atomic ratio of the m1-th element to the m2-th element decreases as the characteristic flow rate increases.

### Claim 3 (depends on 1)

The method for making the alloy thin film according to claim 1, wherein M is equal to 2, and the alloy thin film comprises a titanium element and an aluminum element;
the introducing the first precursor to the M-th precursor into the reaction chamber through the spraying device under conditions of the characteristic temperature, the characteristic distance, and the characteristic flow rate, comprises:
introducing a titanium-containing precursor and an aluminum-containing precursor into the reaction chamber through the spraying device under the conditions of the characteristic temperature, the characteristic distance, and the characteristic flow rate;
the adjusting the characteristic atomic ratio by adjusting any one or more selected from the group consisting of the characteristic temperature, the characteristic distance, and the characteristic flow rate, comprises:
adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic temperature; and/or
adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic distance; and/or
adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic flow rate.

### Claim 4 (depends on 3)

The method for making the alloy thin film according to claim 3, wherein the adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic temperature, comprises:
increasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by increasing the characteristic temperature; or
decreasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by decreasing the characteristic temperature.

### Claim 5 (depends on 3)

The method for making the alloy thin film according to claim 3, wherein the adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic distance, comprises:
decreasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by increasing the characteristic distance; or
increasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by decreasing the characteristic distance.

### Claim 6 (depends on 3)

The method for making the alloy thin film according to claim 3, wherein the adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic flow rate, comprises:
decreasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by increasing the characteristic flow rate; or
increasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by decreasing the characteristic flow rate.

### Claim 7 (depends on 1)

The method for making the alloy thin film according to claim 1, wherein during forming different alloy thin films with different characteristic atomic ratios, a flow rate of any m-th precursor remains unchanged, a temperature of the reaction chamber remains unchanged, pulse time of any m-th precursor remains unchanged, and a flow rate of carrier gas remains unchanged in a case where the m-th precursor is introduced into the reaction chamber.

### Claim 8 (depends on 1)

The method for making the alloy thin film according to claim 1, wherein a process for forming the alloy thin film with the characteristic atomic ratio of the first element to the M-th element on the surface of the pre-processed structure, comprises: an atomic layer deposition process;
the introducing the first precursor to the M-th precursor into the reaction chamber through the spraying device under conditions of the characteristic temperature, the characteristic distance, and the characteristic flow rate, comprises:
performing a plurality of consecutive sub-cycle depositions;
wherein any one of the plurality of sub-cycle depositions is configured to allow a single atomic layer film to be deposited; in any one of the plurality of sub-cycle depositions, the first precursor to the M-th precursor are alternately introduced into the reaction chamber through the spraying device under the conditions of the characteristic temperature, the characteristic distance, and the characteristic flow rate; and a purging operation is further performed between introducing different precursors.

### Claim 9 (depends on 1)

The method for making the alloy thin film according to claim 1, wherein the characteristic temperature ranges from 120° C. to 220° C.;
the characteristic distance ranges from 2 mm to 15 mm; and
the characteristic flow rate ranges from 500 sccm to 1100 sccm.

### Claim 10 (depends on 3)

The method for making the alloy thin film according to claim 3, wherein a temperature of the titanium-containing precursor before being introduced into the spraying device ranges from 18° C. to 35° C., and a temperature of the aluminum-containing precursor before being introduced into the spraying device ranges from 40° C. to 115° C.

### Claim 11 (depends on 1)

The method for making the alloy thin film according to claim 1, wherein the reaction chamber comprises a first reaction sub-chamber and a second reaction sub-chamber disposed in the first reaction sub-chamber, a heating device is disposed between the first reaction sub-chamber and the second reaction sub-chamber, and the supporting platform is disposed in the second reaction sub-chamber.

### Claim 12 (depends on 1)

The method for making the alloy thin film according to claim 1, wherein the alloy thin film is a metal gate layer;
the pre-processed structure comprises a substrate layer, a high dielectric gate dielectric layer disposed on a surface of the substrate layer, and a barrier layer disposed on a surface of the high dielectric gate dielectric layer away from the substrate layer; and
the metal gate layer is disposed on a surface of the barrier layer away from the substrate layer.

### Claim 13

A method for making an alloy thin film comprising a first element to an M-th element, comprising:
providing a reaction chamber, wherein the reaction chamber is provided with a spraying device and a supporting platform;
disposing a pre-processed structure on a surface of the supporting platform, wherein the pre-processed structure comprises a substrate layer, a high dielectric gate dielectric layer disposed on a surface of the substrate layer, and a barrier layer disposed on a surface of the high dielectric gate dielectric layer away from the substrate layer;
forming an alloy thin film with a characteristic atomic ratio of the first element to the M-th element on a surface of the pre-processed structure, comprising:
setting the spraying device to have a characteristic temperature;
setting a characteristic distance between the spraying device and the supporting platform;
setting a flow-stabilizing device to have a characteristic flow rate; and
introducing a first precursor to an M-th precursor into the reaction chamber through the spraying device under conditions of the characteristic temperature, the characteristic distance, and the characteristic flow rate; wherein M is an integer greater than or equal to 2; and any m-th precursor comprises an m-th element, and m is an integer greater than or equal to 1 and less than or equal to M; and
adjusting the characteristic atomic ratio by adjusting any one or more selected from the group consisting of the characteristic temperature, the characteristic distance, and the characteristic flow rate.

### Claim 14 (depends on 13)

The method for making the alloy thin film according to claim 13, wherein any m1-th element and any m2-th element of the first element to the M-th element have different atomic activity, each of m1 and m2 is the integer greater than or equal to 1 and less than or equal to M, and m1 is not equal to m2; and
the characteristic atomic ratio of the m1-th element to the m2-th element increases as the characteristic temperature increases, the characteristic atomic ratio of the m1-th element to the m2-th element decreases as the characteristic distance increases, and the characteristic atomic ratio of the m1-th element to the m2-th element decreases as the characteristic flow rate increases.

### Claim 15 (depends on 13)

The method for making the alloy thin film according to claim 13, wherein M is equal to 2, and the alloy thin film comprises a titanium element and an aluminum element;
the introducing the first precursor to the M-th precursor into the reaction chamber through the spraying device under conditions of the characteristic temperature, the characteristic distance, and the characteristic flow rate, comprises:
introducing a titanium-containing precursor and an aluminum-containing precursor into the reaction chamber through the spraying device under the conditions of the characteristic temperature, the characteristic distance, and the characteristic flow rate;
the adjusting the characteristic atomic ratio by adjusting any one or more selected from the group consisting of the characteristic temperature, the characteristic distance, and the characteristic flow rate, comprises:
adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic temperature; and/or
adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic distance; and/or
adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic flow rate.

### Claim 16 (depends on 15)

The method for making the alloy thin film according to claim 15, wherein the adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic temperature, comprises:
increasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by increasing the characteristic temperature; or
decreasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by decreasing the characteristic temperature.

### Claim 17 (depends on 15)

The method for making the alloy thin film according to claim 15, wherein the adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic distance, comprises:
decreasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by increasing the characteristic distance; or
increasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by decreasing the characteristic distance.

### Claim 18 (depends on 15)

The method for making the alloy thin film according to claim 15, wherein the adjusting the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by adjusting the characteristic flow rate, comprises:
decreasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by increasing the characteristic flow rate; or
increasing the characteristic atomic ratio of the titanium element to the aluminum element of the alloy thin film by decreasing the characteristic flow rate.

### Claim 19 (depends on 13)

The method for making the alloy thin film according to claim 13, wherein during forming different alloy thin films with different characteristic atomic ratios, a flow rate of any m-th precursor remains unchanged, a temperature of the reaction chamber remains unchanged, pulse time of any m-th precursor remains unchanged, and a flow rate of carrier gas remains unchanged in a case where the m-th precursor is introduced into the reaction chamber.

### Claim 20 (depends on 13)

The method for making the alloy thin film according to claim 13, wherein a process for forming the alloy thin film with the characteristic atomic ratio of the first element to the M-th element on the surface of the pre-processed structure, comprises: an atomic layer deposition process;
the introducing the first precursor to the M-th precursor into the reaction chamber through the spraying device under conditions of the characteristic temperature, the characteristic distance, and the characteristic flow rate, comprises:
performing a plurality of consecutive sub-cycle depositions;
wherein any one of the plurality of sub-cycle depositions is configured to allow a single atomic layer film to be deposited; in any one of the plurality of sub-cycle depositions, the first precursor to the M-th precursor are alternately introduced into the reaction chamber through the spraying device under the conditions of the characteristic temperature, the characteristic distance, and the characteristic flow rate; and a purging operation is further performed between introducing different precursors.