# US 2026/0098328 A1 · Double annealed zinc-coated press-hardenable steels

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0098328 A1
- Document ID: US20260098328A1
- Status: Published application
- Kind: A1
- Application number: 19/351,500
- Filed: 2025-10-07
- Published: 2026-04-09
- Earliest claimed: 2024-10-07
- Applicants: United States Steel Corporation
- Inventors: Matthew Michael McCosby; Ghazal Seyed Mousavi
- Web page: https://patentgrep.com/patent/US20260098328A1

## CPC

- C22C 38/04: containing manganese
- C21D 1/673: for die quenching
- C21D 8/0242: {Flattening; Dressing; Flexing}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 9/46: for sheet metals
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C25D 11/00: Electrolytic coating by surface reaction, i.e. forming conversion layers
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

Double-annealed zinc-coated press-hardenable steel with controlled composition and microstructure is provided that achieves galvanic protection and addresses challenges related to liquid metal embrittlement. The double-annealed zinc-coated steel exhibits favorable properties when press hardened. Direct hot press forming may be performed at reduced temperatures where the zinc-based coating is fully solidified. The resultant DHPF zinc-coated sheet products have been found to possess favorable mechanical properties and corrosion resistance.

## Claims

### Claim 1

A method of producing a coated press hardenable steel sheet product comprising from 0.16 to 0.33 weight percent C and from 1.2 to 3.5 weight percent Mn, the method comprising:
subjecting the steel sheet product to a first step annealing process to achieve a predominantly martensite microstructure;
subjecting the steel sheet product to a second step annealing process to achieve a predominantly tempered martensite microstructure; and
applying a coating comprising zinc on the steel sheet product to form a coated steel sheet product.

### Claim 2 (depends on 1)

The method of claim 1, wherein the steel sheet product further comprises from 0.001 to 0.008 weight percent B.

### Claim 3 (depends on 2)

The method of claim 2, wherein the steel sheet product further comprises at least one of from 0.03 to 0.18 weight percent V, from 0.01 to 0.08 weight percent Ti, and from 0.01 to 0.08 weight percent Nb.

### Claim 4 (depends on 2)

The method of claim 2, wherein the steel sheet product further comprises from 0.03 to 0.18 weight percent Mo.

### Claim 5 (depends on 2)

The method of claim 2, wherein the steel sheet product further comprises from 0.01 to 0.12 weight percent Al.

### Claim 6 (depends on 2)

The method of claim 2, wherein the steel sheet product further comprises from 0.01 to 0.04 weight percent P.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first step annealing process is performed at a temperature of at least 800° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first step annealing process is performed at a temperature of from 820 to 950° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein the second step annealing process is performed at a temperature of less than 800° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the second step annealing process is performed at a temperature of from 550 to 775° C.

### Claim 11 (depends on 1)

The method of claim 1, wherein the zinc coating is applied on the steel sheet product at a temperature of from 400 to 500° C.

### Claim 12 (depends on 1)

The method of claim 1, wherein the zinc coating is applied on the steel sheet product at a temperature of from 440 to 480° C.

### Claim 13 (depends on 1)

The method of claim 1, wherein the zinc coating has a thickness of from 1 to 100 microns.

### Claim 14 (depends on 1)

The method of claim 1, wherein the zinc coating has a thickness of from 5 to 40 microns.

### Claim 15 (depends on 1)

The method of claim 1, further comprising hot press forming the double-annealed zinc-coated steel sheet product to austenitize the coated steel sheet product.

### Claim 16 (depends on 15)

The method of claim 15, wherein the hot press forming is performed at a temperature below Ac1.

### Claim 17 (depends on 15)

The method of claim 15, wherein the austenitization is performed at a temperature below 820° C. during hot press forming.

### Claim 18 (depends on 17)

The method of claim 17, wherein the austenitization is performed for a time of less than 300 seconds during hot press forming.

### Claim 19 (depends on 15)

The method of claim 15, wherein after the hot press forming the coating comprises at least 15 volume percent Γ-Fe3Zno based on the volume of the coating.

### Claim 20

A double-annealed coated press hardenable steel sheet product comprising from 0.16 to 0.33 weight percent C and from 1.2 to 3.5 weight percent Mn having a predominantly tempered martensite microstructure and a coating comprising zinc, wherein the steel sheet product has an ultimate tensile strength of at least 700 MPa.

### Claim 21 (depends on 20)

A press hardened coated steel sheet product produced from the double-annealed zinc-coated press hardenable steel sheet product of claim 20, wherein the zinc coating comprises at least 15 volume percent Γ-Fe3Zn10 based on the volume of the coating.

### Claim 22 (depends on 20)

The press hardened coated steel sheet product of claim 20, wherein the zinc coating is from 5 to 40 microns thick.

### Claim 23 (depends on 20)

The press hardened coated steel sheet product of claim 20, wherein the press hardened zinc-coated steel sheet product has an ultimate tensile strength of at least 900 MPa.

### Claim 24 (depends on 20)

The press hardened coated steel sheet product of claim 20, wherein the press hardened zinc-coated steel sheet product has an ultimate tensile strength of up to 2500 MPa.