# US 2026/0098314 A1 · Method for Thermal Processing Bullets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0098314 A1
- Document ID: US20260098314A1
- Status: Published application
- Kind: A1
- Application number: 18/904,308
- Filed: 2024-10-02
- Published: 2026-04-09
- Earliest claimed: 2019-12-06
- Applicants: Law Office of Jerry Joseph, PLC
- Inventors: Peter Paulin
- Web page: https://patentgrep.com/patent/US20260098314A1

## CPC

- C21D 1/613: Gases; Liquefied or solidified normally gaseous material
- F42B 12/72: characterised by the material (heat treatment for explosive shells C21D9/16)
- F42B 33/14: Surface treatment of cartridges or cartridge cases {(F42B33/004 takes precedence)}
- C21D 2201/05: Grain orientation
- C21D 2281/02: temperature gradient
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- F42B: EXPLOSIVE CHARGES, e.g. FOR BLASTING, FIREWORKS, AMMUNITION (explosive compositions C06B; fuzes F42C; blasting F42D)

## Abstract

A method for thermal processing bullets to reduce adhesive stress, the method includes obtaining one or more bullets configured to be propelled down a gun barrel, disposing the one or more bullets within a chamber having a temperature gradient between ambient temperature and cryogenic temperature, the chamber having a plurality of temperature zones, moving the one or more bullets between the plurality of temperature zones of the chamber, and returning the one or more bullets to the ambient temperature to reduce adhesive stress between the bullets and the gun barrel.

## Claims

### Claim 1

A method for thermal processing bullets to reduce adhesive stress, the method comprising:
obtaining one or more bullets configured to be propelled down a gun barrel;
disposing the one or more bullets within a chamber having a temperature gradient between ambient temperature and cryogenic temperature, the chamber having a plurality of temperature zones;
moving the one or more bullets between the plurality of temperature zones of the chamber; and
returning the one or more bullets to the ambient temperature to reduce adhesive stress between the bullets and the gun barrel.

### Claim 2 (depends on 1)

The method of claim 1, wherein the plurality of temperature zones includes a first temperature zone ranging from about 60° F. to about 80° F., a second temperature zone ranging from about 0° F., and a third temperature zone ranging from about −200° F. to about −500° F.

### Claim 3 (depends on 1)

The method of claim 1, wherein the chamber includes a temperature reducing agent.

### Claim 4 (depends on 1)

The method of claim 1, wherein the temperature reducing agent group including liquid nitrogen, gaseous nitrogen, dry ice.

### Claim 5 (depends on 1)

The method of claim 1, wherein the one or more bullets are moved between the plurality of temperature zones of the chamber using a mechanical means including a ball screw mechanism, a pulley mechanism, and a conveyor mechanism.

### Claim 6 (depends on 5)

The method of claim 5, wherein the one or more bullets are moved at a predetermined rate of less than 5 degrees per minute.

### Claim 7 (depends on 6)

The method of claim 6, wherein internal structures of the one or more bullets are stress relieved after being moved between the plurality of temperature zones and then back to the ambient temperature.

### Claim 8 (depends on 1)

The method of claim 1, wherein an adhesive stress between the bullets and the gun barrel is reduced causing an increase in sealing capacities between the bullets and the gun barrel.

### Claim 9 (depends on 8)

The method of claim 8, wherein the increase in sealing capacities between the bullets and the gun barrel results in higher travel velocity, axial symmetry and concentricity of the bullet in flight.

### Claim 10 (depends on 9)

The method of claim 9, wherein an external perimeter of the one or more bullets has a uniform compressive stress after being moved between the plurality of temperature zones and then back to the ambient temperature.

### Claim 11

A system for thermal processing bullets to yield a refined grain structure, the system comprising:
a chamber containing a plurality of cooling agents to form a plurality of temperature zones, with temperatures getting progressively cooler at each deeper temperature zone;
a bullet carrier configured to hold one or more bullets to be moved through the plurality of temperature zones, each bullet comprising a bullet cartridge case detachably affixed to a bullet lead core jacketed with a gilding metal such that, upon firing the bullet, the bullet lead core with gilding metal jacket is propelled down a bore of a gun barrel; and
a mechanical mechanism configured to first lower the bullet carrier holding the one or more bullets through the plurality of temperature zones and then raise the carrier holding the one or more bullets back up through the plurality of temperature zones,
wherein the bullet carrier and the one or more bullets held in the bullet carrier are moved through the plurality of temperature zones at a predetermined rate and wherein at least one of the plurality of temperature zones is predetermined to cause a grain size of the bullet lead core with gilding metal jacket of the one or more bullets to become less than 50 microns.

### Claim 12 (depends on 11)

The system of claim 11, wherein the plurality of temperature zones includes a first temperature zone ranging from 60° F. to 80° F., a second temperature zone intermediate of 60° F. and −200° F. and a third temperature zone ranging from −200° F. to −459.67° F.

### Claim 13

The system of claim l1, wherein the chamber includes a temperature reducing agent.

### Claim 14 (depends on 13)

The system of claim 13, wherein the temperature reducing agent comprises at least one of liquid nitrogen, gaseous nitrogen, and dry ice.

### Claim 15 (depends on 11)

The system of claim 11, wherein the mechanical mechanism configured to lower and raise the bullet carrier holding the one or more bullets through the plurality of temperature zones comprises at least one of a ball screw mechanism, a pulley mechanism, and a conveyor mechanism.

### Claim 16 (depends on 11)

The system of claim 11, wherein the predetermined rate is less than 5° F. per minute.

### Claim 17 (depends on 16)

The system of claim 16, wherein internal structures of the one or more bullets are stress relieved after being moved between the plurality of temperature zones and then back to an ambient temperature.

### Claim 19 (depends on 17)

The system of claim 17, wherein an external perimeter of the one or more bullets has a uniform compressive stress after being moved between the plurality of temperature zones and then back to the ambient temperature.

### Claim 20

A system for thermal processing bullets to yield a refined grain structure, each bullet comprising a bullet cartridge case detachably affixed to a bullet lead core jacketed with a gilding metal such that, upon firing the bullet, the bullet lead core with gilding metal jacket is propelled down a bore of a gun barrel; the system comprising:
a chamber configured to have a first temperature zone and a different second temperature zone, wherein the second temperature zone is predetermined to cause a grain size of the bullet lead core with gilding metal jacket of each of the one or more bullets to be less than 50 microns; and
a bullet carrier configured to hold one or more bullets to be moved through the first and second temperature zones,
wherein the bullet carrier and the one or more bullets held in the bullet carrier are moved through the first and temperature zones at a predetermined rate and wherein the second temperature zone is predetermined to cause a grain size of the bullet lead core with gilding metal jacket of the one or more bullets to become less than 50 microns.