# US 2026/0098192 A1 · Polymer composition for lamination and laminated body using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0098192 A1
- Document ID: US20260098192A1
- Status: Published application
- Kind: A1
- Application number: 19/418,124
- Filed: 2025-12-12
- Published: 2026-04-09
- Earliest claimed: 2019-06-24
- Assignees: Japan Polyethylene Corporation
- Applicants: Japan Polyethylene Corporation
- Inventors: Masahiro UENO; Makoto YANAGIE; Masahiro UEMATSU
- Web page: https://patentgrep.com/patent/US20260098192A1

## CPC

- C08F 210/02: Ethene
- C09J 133/08: Homopolymers or copolymers of acrylic acid esters
- B32B 15/085: comprising polyolefins
- B32B 15/09: comprising polyesters
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- B32B 27/18: characterised by the use of special additives
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 27/36: comprising polyesters
- C08F 8/44: Preparation of metal salts or ammonium salts
- C08L 23/0869: with unsaturated acids, e.g. [meth]acrylic acid; with unsaturated esters, e.g. [meth]acrylic acid esters
- C09J 7/385: {Acrylic polymers}
- B32B 2255/06: on metal layer
- B32B 2307/30: having particular thermal properties
- B32B 2307/31: Heat sealable
- B32B 2307/54: Yield strength; Tensile strength
- B32B 2307/558: Impact strength, toughness
- B32B 2307/704: Crystalline
- B32B 2307/748: Releasability
- B32B 2553/00: Packaging equipment or accessories not otherwise provided for
- C09J 2423/04: Presence of homo or copolymers of ethene
- C09J 2433/00: Presence of (meth)acrylic polymer
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A polymer composition for lamination consists of (X1) 100 to 60% by weight of an ionomer characterized in that at least a part of a carboxyl group and/or a dicarboxylic anhydride group in a copolymer (P) containing a structural unit (A) derived from ethylene and/or an α-olefin having 3 to 20 carbon atoms and a structural unit (B) derived from a monomer having a carboxyl group and/or a dicarboxylic anhydride group as essential constitutional units being converted into a metal-containing carboxylic acid salt containing at least one kind of a metal ion(s) selected from Group 1, Group 2 or Group 12 of the periodic table, and a phase angle δ of the ionomer at an absolute value G*=0.1 MPa of a complex modulus of elasticity measured by a rotary rheometer is a range of 50 degrees to 75 degrees, and (X2) 40 to 0% by weight of an ethylene-based copolymer.

## Claims

### Claim 1

A polymer composition for lamination characterized in that the composition: consists of
(X1) 100 to 60% by weight of an ionomer characterized in that at least a part of a carboxyl group and/or a dicarboxylic anhydride group in a copolymer (P) containing a structural unit (A) derived from ethylene and/or an α-olefin having 3 to 20 carbon atoms and a structural unit (B) derived from a monomer having a carboxyl group and/or a dicarboxylic anhydride group as essential constitutional units being converted into a metal-containing carboxylic acid salt containing at least one kind of a metal ion(s) selected from Group 1, Group 2 or Group 12 of the periodic table, and a phase angle δ of the ionomer at an absolute value G*=0.1 MPa of a complex modulus of elasticity measured by a rotary rheometer is a range of 50 degrees to 75 degrees, and
(X2) 40 to 0% by weight of an ethylene-based copolymer containing ethylene by high-pressure radical polymerization as an essential monomer, and has a melt flow rate of 1.0 to 100 g/10 min.

### Claim 2 (depends on 1)

The polymer composition for lamination according to claim 1 characterized in that a number of methyl branches calculated by 13C-NMR of the copolymer (P) is 50 or less per 1,000 carbons.

### Claim 3 (depends on 1)

The polymer composition for lamination according to claim 1 characterized in that a number of methyl branches calculated by 13C-NMR of the copolymer (P) is 5 or less per 1,000 carbons.

### Claim 4 (depends on 1)

The polymer composition for lamination according to claim 1 characterized in that the copolymer (P) contains 2 to 20 mol % of the structural unit (B) in the copolymer.

### Claim 5 (depends on 1)

The polymer composition for lamination according to claim 1 characterized in that the structural unit (A) is a structural unit derived from ethylene.

### Claim 6 (depends on 1)

The polymer composition for lamination according to claim 1 characterized in that the copolymer (P) is produced by using a transition metal catalyst containing a transition metal(s) of Group 8 to 11 of the periodic table.

### Claim 7 (depends on 6)

The polymer composition for lamination according to claim 6 characterized in that the transition metal catalyst is a transition metal catalyst comprising phosphorus sulfonic acid or phosphorus phenol ligand and nickel or palladium.

### Claim 8 (depends on 1)

The polymer composition for lamination according to claim 1 characterized in that the (X2) ethylene-based copolymer by high-pressure radical polymerization is an ethylene homopolymer.

### Claim 9 (depends on 1)

A laminated body which is a laminated body constituted by at least a first layer composed of a base material layer and a second layer composed of a sealant layer, wherein the sealant layer comprises the polymer composition for lamination according to claim 1.