# US 2026/0098148 A1 · Polypropylene composition for cable insulation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0098148 A1
- Document ID: US20260098148A1
- Status: Published application
- Kind: A1
- Application number: 19/113,968
- Filed: 2023-09-26
- Published: 2026-04-09
- Earliest claimed: 2022-09-28
- Assignees: Borealis AG
- Applicants: Borealis AG
- Inventors: Katja Klimke; Per-Ola Hagstrand; Ulf Nilsson; Thomas Gkourmpis; Lars Efraimsson; Anette Johansson; Kristian Dahlén; Gerhard Hubner
- Web page: https://patentgrep.com/patent/US20260098148A1

## CPC

- C08L 23/12: Polypropene
- C08L 23/142: {at least partially crystalline copolymers of propene with other olefins}
- H01B 3/441: {from alkenes}
- C08L 2203/202: use in electrical wires or wirecoating
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/035: containing four or more polymers in a blend
- C08L 2207/02: Heterophasic composition
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

The present invention relates to a cable comprising a polypropylene composition comprising (A) from 80.0 to 99.0 wt.-%, preferably from 82.5 to 97.2 wt. %, most preferably from 85.0 to 95.0 wt.-% of a copolymer of propylene and comonomer units selected from ethylene and alpha-olefins having from 4 to 12 carbon atoms having a total amount of comonomer units of from 10.0 to 16.0 wt %, preferably from 11.0 to 15.0 wt %, most preferably from 12.0 to 14.0 wt %, based on the total amount of monomer units of the copolymer of propylene (A); a melt flow rate MFR2 of from 0.5 to 2.5 g/10 min, preferably from 0.8 to 2.3 g/10 min, still more preferably from 1.0 to 2.0 g/10 min and most preferably from 1.2 to 1.7 g/10 min; a xylene cold soluble (XCS) fraction in a total amount of from 25.0 to 50.0 wt %, preferably from 27.5 to 45.0 wt %, more preferably from 30.0 to 42.5 wt % and most preferably from 32.5 to 40.0 wt %, based on the total weight amount of the copolymer of propylene (A); and (B) from 1.0 to 20.0 wt.-%, preferably from 2.5 to 17.5 wt %, most preferably from 5.0 to 15.0 wt.-% of a copolymer of ethylene and comonomer units selected from alpha-olefins having from 4 to 12 carbon atoms obtainable in the presence of a single site catalyst and having a density of from 860 to 930 kg/m3, preferably from 865 to 925 kg/m3, most preferably from 870 to 920 kg/m3, determined according to ISO 1183.

## Claims

### Claim 1

A cable comprising at least one layer comprising a polypropylene composition comprising:
(A) from 80.0 to 99.0 wt.-%, based on the total weight of the polypropylene composition, of a copolymer of propylene and comonomer units selected from ethylene and alpha-olefins having from 4 to 12 carbon atoms having
a total amount of comonomer units of from 10.0 to 16.0 wt %, based on the total amount of monomer units of the copolymer of propylene (A), determined by quantitative 13C{H} NMR measurement;
a melt flow rate MFR2 of from 0.5 to 2.5 g/10 min, determined according to ISO 1133 at 230° C. and 2.16 kg;
a xylene cold soluble (XCS) fraction in a total amount of from 25.0 to 50.0 wt %, based on the total weight amount of the copolymer of propylene (A) and determined according to ISO16152; and
(B) from 1.0 to 20.0 wt.-%, based on the total weight of the polypropylene composition, of a copolymer of ethylene and comonomer units selected from alpha-olefins having from 4 to 12 carbon atoms obtainable in the presence of a single site catalyst and having a density of from 860 to 930 kg/m3, determined according to ISO 1183.

### Claim 2 (depends on 1)

The cable according to claim 1, wherein the copolymer of propylene (A) is a heterophasic copolymer of propylene which comprises a matrix phase and an elastomeric phase dispersed in said matrix phase, which preferably comprises two glass transition temperatures attributed to the matrix phase and the elastomeric phase, wherein the glass transition temperature attributed to the matrix phase Tg (matrix) is in the range of from −1.0 to −15.0° C., and/or the glass transition temperature attributed to the elastomeric phase Tg (EP) is in the range of from −40.0 to −55.0° C., wherein Tg (matrix) and Tg (EP) are determined by dynamic mechanical analysis.

### Claim 3 (depends on 1)

The cable according to claim 1, wherein xylene cold soluble (XCS) fraction of the copolymer of propylene (A) has an amount of comonomer units, preferably of ethylene, of from 23.0 to 35.0 wt %, based on the total amount of monomer units in the xylene cold soluble (XCS) fraction and determined by quantitative 13C{1H} NMR measurement, and/or an intrinsic viscosity of from 150 to 350 cm3/g, measured in decalin according to ISO 1628-3.

### Claim 4 (depends on 1)

The cable according to claim 1, wherein the copolymer of propylene (A) has a fraction insoluble in cold xylene (XCI) in a total amount of from 50.0 to 75.0 wt %, based on the total weight amount of the copolymer of propylene (A) and determined according to ISO16152, and wherein the fraction insoluble in cold xylene (XCI) preferably has an amount of comonomer units, preferably of ethylene, of from 3.0 to 9.0 wt %, based on the total amount of monomer units in the fraction insoluble in cold xylene (XCI) and determined by quantitative 13C{1H} NMR measurement, and/or an intrinsic viscosity of preferably from 185 to 350 cm3/g, measured in decalin according to ISO 1628-3.

### Claim 5 (depends on 1)

The cable according to claim 1, wherein the copolymer of propylene (A) has one or more of the following properties:
a flexural modulus of from 130 MPa to 400 MPa, determined according to ISO 178 method A; and/or
a Charpy notched impact strength at 23° C. of from 50 to 110 kJ/m2, determined according to to ISO 179-1/1eA; and/or
a Charpy notched impact strength at −20° C. of from 5.0 to 10.0 kJ/m2, determined according to to ISO 179-1/1eA.

### Claim 6 (depends on 1)

The cable according to claim 1, wherein the copolymer of ethylene (B) is a copolymer of ethylene and 1-octene or a copolymer of ethylene and 1-butene.

### Claim 7 (depends on 1)

The cable according to claim 1, wherein the copolymer of ethylene (B) is a copolymer of ethylene with 1-octene having one or more of the following properties:
a density of from 860 to 895 kg/m3, determined according to ISO 1183; and/or
a crystallinity of from 10.0 to 40.0%; and/or
a melt flow rate MFR2 of from 1.0 to 50.0 g/10 min, determined according to ISO 1133 at 190° C. and 2.16 kg; and/or
a glass transition temperature Tg of from −60 to −40° C., preferably from −57 to −42° C., most preferably from −55 to −45° C., determined by dynamic mechanical analysis; and/or
a melting temperature Tm of from 40 to 85° C., determined by differential scanning calorimetry; and/or
a flexural modulus of from 1 to 50 MPa, determined according to ISO 178 method A.

### Claim 8 (depends on 1)

The cable according to claim 1, wherein the copolymer of ethylene (B) is polyethylene wax being a copolymer of ethylene and 1-butene and having one or more of the following properties:
a density of from 900 to 930 kg/m3, determined according to ISO 1183; and/or
a crystallinity of from 40.0 to 65.0%; and/or
a weight average molecular weight Mw of from 1000 to 5000 g/mol, determined by GPC; and/or
a melting temperature Tm of from 90 to 110° C., determined by differential scanning calorimetry; and/or
a melt viscosity at 140° C. of from 100 to 500 mPas.

### Claim 9 (depends on 1)

The cable according to claim 1, wherein the polypropylene composition has
a total amount of units derived from propylene of from 70.0 to 87.5 wt %
a total amount of units derived from ethylene of from 12.5 to 35.0 wt %; and
a total amount of units derived from alpha-olefins having from 4 to 12 carbon atoms of from 0.1 to 10.0 wt %,
all based on the total amount monomer units of the polypropylene composition and determined using quantitative 13C{1H} NMR measurement.

### Claim 10 (depends on 1)

The cable according to claim 1, wherein the polypropylene composition has a xylene cold soluble (XCS) fraction, which has
a total amount of units derived from propylene of from 47.5 to 75.0 wt %;
a total amount of units derived from ethylene of from 25.0 to 47.5 wt %; and
a total amount of units derived from alpha-olefins having from 4 to 12 carbon atoms of from 0.1 to 12.5 wt %,
all based on the total amount monomer units of the xylene cold soluble (XCS) fraction and determined using quantitative 13C{1H} NMR measurement; and/or
a fraction insoluble in cold xylene (XCI), which has
a total amount of units derived from propylene of from 80.0 to 96.5 wt %;
a total amount of units derived from ethylene of from 3.5 to 20.0 wt %; and
a total amount of units derived from alpha-olefins having from 4 to 12 carbon atoms of from 0 to 2.5 wt %,
all based on the total amount monomer units of the having fraction insoluble in cold xylene (XCI) and determined using quantitative 13C{1H} NMR measurement.

### Claim 11 (depends on 1)

The cable according to claim 1, wherein the polypropylene composition has one or more of the following properties:
a melt flow rate MFR2 of 0.5 to 7.5 g/10 min, determined according to ISO 1133 at 230° C. and 2.16 kg; and/or
a melting temperature Tm of from 140 to 159° C., determined by differential scanning calorimetry; and/or
a crystallization temperature Tc of from 85 to 130° C., determined by differential scanning calorimetry; and/or
a difference of the melting temperature to the crystallization temperature Tm-Tc is preferably in the range of from 20 to 65° C.; and/or
a glass temperature attributed to the matrix phase Tg (matrix) in the range of from −1.0 to −15.0° C., determined by dynamic mechanical analysis; and/or
a glass temperature attributed to the elastomeric phase Tg (EP) of from −40.0 to −55.0° C., determined by dynamic mechanical analysis; and/or
shear thinning index SH1/100 of from 2.5 to 20.0, determined by dynamic shear measurements; and/or
a polydispersity index PI of from 1.0 to 4.5 s−1, determined by dynamic shear measurements; and/or
a flexural modulus of from 150 MPa to 350 MPa, determined according to ISO 178 method A; and/or
a Charpy notched impact strength at 23° C. of from 50 to 110 kJ/m2, determined according to to ISO 179-1/1eA; and/or
a Charpy notched impact strength at −20° C. of from 3.5 to 25.0 kJ/m2, determined according to to ISO 179-1/1eA.

### Claim 12 (depends on 1)

The cable according to claim 1, wherein the polypropylene composition is free of a dielectric fluid.

### Claim 13 (depends on 1)

The cable according to claim 1, wherein the at least one layer is an insulation layer.

### Claim 14 (depends on 1)

The cable according to claim 1 being a medium voltage cable or high voltage cable, comprising an insulation layer comprising the polypropylene composition.

### Claim 15 (depends on 1)

The cable according to claim 1 being a cable comprising an insulation layer comprising the polypropylene composition and having a Weibull alpha-value of from 35.0 to 65.0 kV/mm, measured on a 10 kV cable in agreement with CENELEC HD 605 5.4.15.3.4 for 6/10 kV cables.