# US 2026/0098130 A1 · Pc supported interface additive masterbatch and use thereof in pc solvent resistance modification

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0098130 A1
- Document ID: US20260098130A1
- Status: Published application
- Kind: A1
- Application number: 18/998,904
- Filed: 2023-12-29
- Published: 2026-04-09
- Earliest claimed: 2022-12-29
- Assignees: Beijing Aerospace Kaien New Material Co., Ltd.
- Applicants: Beijing Aerospace Kaien New Material Co., Ltd.
- Inventors: Junchi ZHENG; Tao FANG; Chaoyang LIU; Yue JIA; Zheng MENG; Zhaoyi SUN; Jing QIAN; Junying AN; Yaguang YANG; Bangjian SHU
- Web page: https://patentgrep.com/patent/US20260098130A1

## CPC

- C08J 3/226: {using a polymer as a carrier}
- C08F 2/06: Organic solvent
- C08F 220/14: Methyl esters {, e.g. methyl (meth)acrylate}
- C08J 2369/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- C08J 2433/12: Homopolymers or copolymers of methyl methacrylate
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A method for preparing a PC masterbatch loaded with an interfacial conditioning aid and a method for preparing a PC composite are provided. An interfacial conditioning aid is polymerized by methyl acrylate (MA) or an itaconate derivativer, glycidyl methacrylate (GMA), and methyl methacrylate (MMA) as three types of raw material. The interfacial conditioning aid and PC solution are mixed, and co-precipitated to obtain a PC masterbatch loaded with an interfacial conditioning aid. The PC masterbatch loaded with an interfacial conditioning aid, PC, and a polyester are mixed and performed a blend extrusion on the mixed system to obtain the PC composite. The PC composite has good solvent resistance, little color change, good transparency, and excellent physical properties.

## Claims

### Claim 1

A method for preparing a PC masterbatch loaded with an interfacial conditioning aid, including:
S1, preparing an interfacial conditioning aid by polymerizing by an itaconate derivative or methyl acrylate, glycidyl methacrylate and methyl methacrylate as raw materials; and
S2, mixing the interfacial conditioning aid with a polycarbonate solution, and performing co-precipitation to prepare the PC masterbatch loaded with the interfacial conditioning aid.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, in step S1, glycidyl methacrylate, methyl acrylate, methyl methacrylate and a solvent are added into a reactor,
a temperature is raised to 60-80° C. under a protective atmosphere, and
an initiator is added, and stirring is performed under a protective atmosphere to obtain the interfacial conditioning aid.

### Claim 3 (depends on 2)

The method according to claim 2, wherein, after the temperature is raised to 60-80° C. under the protective atmosphere and is maintained for 30-60 min under the protective atmosphere, the initiator is added, wherein, the initiator being an azo initiator;
wherein an amount of the initiator is 0.1 wt % of a sum of the amounts of glycidyl methacrylate, methyl acrylate and methyl methacrylate;
after the initiator is added, a reaction is carried out under stirring for 6-12 h to obtain the interfacial conditioning aid.

### Claim 4 (depends on 1)

The method according to claim 1, wherein, an amount of glycidyl methacrylate is 2-30 wt % of a mass of methyl methacrylate;
wherein an amount of methyl acrylate is 2-15 wt % of the mass of methyl methacrylate; and
wherein an amount of methyl methacrylate is 3-20 wt % of the amount of the solvent.

### Claim 5 (depends on 1)

The method according to claim 1,
wherein in step S2, a content of polycarbonate in the polycarbonate solution is 5-25 wt %.

### Claim 6 (depends on 1)

The method according to claim 1, wherein, in step S2,
the polycarbonate is first dissolved in a first solvent to obtain a first solution; the interfacial conditioning aid is added into the first solution for mixing to obtain a second mixed solution; and the second mixed solution is added into a second solvent to separate out a precipitate of PC loaded with the interfacial conditioning aid; wherein a performance of the second solvent in dissolving PC and the interfacial conditioning aid is lower than that of the first solvent;
the precipitate is subjected to suction filtration, and a filter residue is then washed with the second solvent, and a washed filter residue is dried to obtain the PC masterbatch loaded with the interfacial conditioning aid; and
wherein the second solvent is a small molecule alcohol.

### Claim 7 (depends on 6)

The method according to claim 6, wherein, the second solvent washed with the precipitant is dried at a temperature of 60-100° C. for 10-16 h to obtain the PC masterbatch loaded with the interfacial conditioning aid.

### Claim 8 (depends on 1)

The method according to claim 1, wherein, in step S1, the interfacial conditioning aid is polymerized by an itaconate derivative, glycidyl methacrylate, and methyl methacrylate; and
wherein the itaconate derivative is prepared by esterification of itaconic acid with a saturated monohydric alcohol containing 4-7 carbon atoms.

### Claim 9 (depends on 8)

The method according to claim 8, wherein, a mass ratio of an itaconate to methyl methacrylate is 1:(1.3-6.1); and
wherein a mass ratio of the itaconate to glycidyl methacrylate is 1:(0.025-0.4).

### Claim 10

(canceled)

### Claim 11 (depends on 1)

The method according to claim 1, wherein, during a polymerizing process, an initiator is added, the initiator is selected from at least one of azobisisobutyronitrile and azobisisoheptonitrile; and
, wherein an amount of the initiator is 0.05-0.2 wt % of a total mass of the three monomers.

### Claim 12

A PC masterbatch loaded with an interfacial conditioning aid, being prepared by a method including:
S1, preparing an interfacial conditioning aid by polymerizing by an itaconate derivative or methyl acrylate, glycidyl methacrylate and methyl methacrylate as raw material;
S2, mixing the interfacial conditioning aid with a polycarbonate solution, and performing co-precipitation to prepare PC masterbatch loaded with the interfacial conditioning aid; and
wherein a mass of the interfacial conditioning aid is 10-250 wt % of a mass of the polycarbonate.

### Claim 13 (depends on 12)

The PC masterbatch loaded with an interfacial conditioning aid according to claim 12, wherein, the polycarbonate is first dissolved in the first solvent to obtain a first solution; the interfacial conditioning aid is added into the first solution for mixing to obtain a second mixed solution; and the second mixed solution is added into a second solvent to separate out a precipitate of PC loaded with the interfacial conditioning aid, wherein a performance of the second solvent in dissolving PC and the interfacial conditioning aid is lower than that of the first solvent; and
, wherein the second solvent comprises an alcohol.

### Claim 14

A method for preparing a PC composite, including:
mixing the PC masterbatch loaded with an interfacial conditioning aid
with a polycarbonate and a polyester to form a mixed system, and performing a blend extrusion on the mixed system to obtain the PC composite; or,
mixing the PC masterbatch loaded with an interfacial conditioning aid with a polyester component to form a mixed system, and performing the blend extrusion on the mixed system to obtain the PC composite;
wherein, the polyester is an aromatic acid saturated polyester; and
wherein, the PC masterbatch loaded with an interfacial conditioning aid is prepared by a method including:
S1, preparing an interfacial conditioning aid by polymerizing by an itaconate derivative or methyl acrylate, glycidyl methacrylate and methyl methacrylate as raw material;
S2, mixing the interfacial conditioning aid with a polycarbonate solution, and performing co-precipitation to prepare PC masterbatch loaded with the interfacial conditioning aid; and
wherein a mass of the interfacial conditioning aid is 10-250 wt % of a mass of the polycarbonate.

### Claim 15 (depends on 14)

The method according to claim 14, wherein, a content of the PC masterbatch loaded with the interfacial conditioning aid in the mixed system is 0.5-60 wt %; and
, wherein a content of the PC in the mixed system is 1-99 wt %.

### Claim 16 (depends on 14)

The method according to claim 14, wherein, a content of the interfacial conditioning aid in the mixed system is 0.3-6 wt %; and
wherein the content of the polyester in the mixed system is 0.5-40 wt %.

### Claim 17

(canceled)

### Claim 18

(canceled)

### Claim 19 (depends on 8)

The method according to claim 8, wherein, the itaconate derivative comprises one or a mixture of more than one of dibutyl itaconate, diisobutyl itaconate, diamyl itaconate, diisoamyl itaconate, dihexyl itaconate, and diheptyl itaconate.

### Claim 20 (depends on 8)

The method according to claim 8, wherein, the polymerizing is performed at a temperature in a range of 60-80° C.

### Claim 21 (depends on 12)

The PC masterbatch loaded with an interfacial conditioning aid according to claim 12, wherein, the first solvent is selected from chloroalkanes.

### Claim 22 (depends on 13)

The PC masterbatch loaded with an interfacial conditioning aid according to claim 13, wherein, a PC component is mixed with the interfacial conditioning aid at a temperature of 20-40° C.

### Claim 23 (depends on 15)

The method according to claim 15, wherein, a content of the polyester in the mixed system is 0.5-40 wt %.