# US 2026/0098051 A1 · Organoamino-functionalized cyclic oligosiloxanes for deposition of silicon-containing films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0098051 A1
- Document ID: US20260098051A1
- Status: Published application
- Kind: A1
- Application number: 19/415,459
- Filed: 2025-12-10
- Published: 2026-04-09
- Earliest claimed: 2019-04-05
- Assignees: Versum Materials US, LLC
- Applicants: Versum Materials US, LLC
- Inventors: MATTHEW R. MACDONALD; JOHN F. LEHMANN
- Web page: https://patentgrep.com/patent/US20260098051A1

## CPC

- C07F 7/0816: {said ring comprising Si as a ring atom}
- C23C 16/401: {containing silicon}
- C07F 7/21: Cyclic compounds having at least one ring containing silicon, but no carbon in the ring
- C23C 16/402: {Silicon dioxide}
- C23C 16/45542: {Plasma being used non-continuously during the ALD reactions}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- C23C 16/45504: {Laminar flow}
- C07F: ACYCLIC, CARBOCYCLIC OR HETEROCYCLIC COMPOUNDS CONTAINING ELEMENTS OTHER THAN CARBON, HYDROGEN, HALOGEN, OXYGEN, NITROGEN, SULFUR, SELENIUM OR TELLURIUM (metal-containing porphyrins C07D487/22)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Amino-functionalized cyclic oligosiloxanes, which have at least three silicon and three oxygen atoms as well as at least one organoamino group and methods for making the oligosiloxanes are disclosed. Methods for depositing silicon and oxygen containing films using the organoamino-functionalized cyclic oligosiloxanes are also disclosed.

## Claims

### Claim 1

A method for depositing a film comprising silicon and oxygen onto a substrate, the method comprising the steps of:
a) providing a substrate in a reactor;
b) introducing into the reactor at least one silicon precursor compound selected from the group consisting of Formulae A-D
wherein R1 is selected from the group consisting of a linear C1 to C10 alkyl group, a branched C3 to C10 alkyl group, a C3 to C10 cyclic alkyl group, a C3 to C10 heterocyclic group, a C3 to C10 alkenyl group, a C3 to C10 alkynyl group, and a C4 to C10 aryl group; R2 is selected from the group consisting of hydrogen, a C1 to C10 linear alkyl group, a branched C3 to C10 alkyl group, a C3 to C10 cyclic alkyl group, a C3 to C10 heterocyclic group, a C3 to C10 alkenyl group, a C3 to C10 alkynyl group, and a C4 to C10 aryl group, wherein R1 and R2 are either linked to form a cyclic ring structure or are not linked to form a cyclic ring structure; R3-11 are each independently selected from the group consisting of hydrogen, a linear C1 to C10 alkyl group, a branched C3 to C10 alkyl group, a C3 to C10 cyclic alkyl group, a C2 to C10 alkenyl group, a C2 to C10 alkynyl group, a C4 to C10 aryl group, and an organoamino group, NR1R2, wherein R1 and R2 are defined above; n=1, 2, or 3, and m=2 or 3;
c) purging the reactor with a purge gas;
d) introducing at least one of an oxygen-containing source and a nitrogen-containing source into the reactor; and
e) purging the reactor with the purge gas,
wherein the steps b through e are repeated until a desired thickness of film is deposited; and wherein the method is conducted at one or more temperatures ranging from about 25° C. to 700° C.

### Claim 2

A silicon and oxygen containing film comprising at least one of the following characteristics: a density of at least about 2.1 g/cc; a wet etch rate that is less than about 2.5 Å/s as measured in a solution of 1:100 of HF to water dilute HF (0.5 wt % dHF) acid; an electrical leakage of less than about 1 e-8 A/cm2 up to 6 MV/cm; and a hydrogen impurity of less than about 5 e20 at/cc as measured by Secondary Ion Mass Spectrometry (SIMS).

### Claim 3 (depends on 1)

The method of claim 1 wherein the silicon precursor compound further comprising at least one selected from the group consisting of a solvent and an inert gas.