# US 2026/0097987 A1 · Glass tube for pharmaceutical containers and process for the production of a glass tube

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0097987 A1
- Document ID: US20260097987A1
- Status: Published application
- Kind: A1
- Application number: 19/416,007
- Filed: 2025-12-11
- Published: 2026-04-09
- Earliest claimed: 2021-11-29
- Assignees: Schott AG
- Applicants: Schott AG
- Inventors: Stephan Tratzky; André Witzmann; Volker Trinks
- Web page: https://patentgrep.com/patent/US20260097987A1

## CPC

- C03B 17/04: Forming tubes or rods by drawing from stationary or rotating tools or from forming nozzles
- C03C 4/20: for chemical resistant glass
- A61J 1/1468: {Containers characterised by specific material properties}
- C03B 23/09: Reshaping the ends, e.g. as grooves, threads or mouths
- C03C 3/091: containing aluminium
- C03C 23/0075: {Cleaning of glass (specially adapted to plate glass B08B11/00)}
- C03C 2203/50: After-treatment
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- A61J: CONTAINERS SPECIALLY ADAPTED FOR MEDICAL OR PHARMACEUTICAL PURPOSES; DEVICES OR METHODS SPECIALLY ADAPTED FOR BRINGING PHARMACEUTICAL PRODUCTS INTO PARTICULAR PHYSICAL OR ADMINISTERING FORMS; DEVICES FOR ADMINISTERING FOOD OR MEDICINES ORALLY; BABY COMFORTERS; DEVICES FOR RECEIVING SPITTLE

## Abstract

A glass tube for pharmaceutical containers and a process for the production of a glass tube are provided. The glass tubes have low alkali leachability and are devoid of a lamp ring.

## Claims

### Claim 1

A process for producing a glass tube for pharmaceutical containers, comprising:
providing a glass melt comprising volatile components;
forming the glass melt into the glass tube having an inner surface and an outer surface;
cutting the glass tube to define a first end and a second end;
forming the first end into a first closed end; and
reducing condensation of the volatile components at the inner surface.

### Claim 2 (depends on 1)

The process of claim 1, further comprising forming the second end into a second closed end.

### Claim 3 (depends on 1)

The process of claim 1, wherein the step of providing the glass melt comprises melting a batch of raw materials yielding oxides comprised in the glass melt.

### Claim 4 (depends on 1)

The process of claim 1, wherein the volatile components comprise borates.

### Claim 5 (depends on 1)

The process of claim 1, wherein the step of forming the glass melt into the glass tube comprises drawing the glass melt to form the glass tube.

### Claim 6 (depends on 1)

The process of claim 1, wherein the step of reducing condensation of the volatile comprises establishing an excess pressure inside the glass tube with respect to outside of the glass tube.

### Claim 7 (depends on 6)

The process of claim 6, wherein the step of establishing the excess pressure inside the glass tube comprises placing solid carbon dioxide inside the glass tube.

### Claim 8 (depends on 7)

The process of claim 7, wherein the solid carbon dioxide comprises dry ice pellets.

### Claim 9 (depends on 6)

The process of claim 6, wherein the step of establishing the excess pressure inside the glass tube comprises evaporating liquid nitrogen inside the glass tube.

### Claim 10 (depends on 6)

The process of claim 6, wherein the step of establishing the excess pressure inside the glass tube comprises releasing a gas inside the glass tube.

### Claim 11 (depends on 10)

The process of claim 10, wherein the gas is selected from a group consisting of CO2, N2, O2, H2, and combinations thereof.

### Claim 12 (depends on 10)

The process of claim 10, wherein the step of releasing the gas inside the glass tube comprises placing a reaction mixture inside the glass tube and causing the reaction mixture to release the gas.

### Claim 13 (depends on 1)

The process of claim 1, further comprising forming a pressure compensation vent hole in the glass tube that passes from the inner surface to the outer surface.

### Claim 14 (depends on 13)

The process of claim 13, wherein the pressure compensation vent hole is formed at a first vicinity, the first vicinity being between 15 mm from the first end and a first intermediate location offset from the first end by a distance that is between ten times an inner diameter (di) of the glass tube and at most 75 mm.

### Claim 15 (depends on 14)

The process of claim 14, wherein the step of reducing condensation is configured so that the first vicinity is devoid of a first lamp ring.

### Claim 16 (depends on 14)

The process of claim 14, wherein the step of reducing condensation is configured so that a ratio of transmittance for at least one wavelength in a range of 350 to 800 nm for the first vicinity and a middle section is at least 0.97.

### Claim 17 (depends on 14)

The process of claim 14, wherein the step of reducing condensation is configured so that the first vicinity has a first alkali leachability of less than 0.9 μg cm−2, first alkali leachability being determined as relative concentration in an eluate prepared according to ISO 4802-2:2010, except that initial rinsing steps with distilled water at ambient temperature are omitted.

### Claim 18 (depends on 1)

The process of claim 1, wherein the glass melt comprises a glass composition having a fining agent selected from a group consisting of a chloride, a sulfate, and combinations thereof.

### Claim 19 (depends on 1)

The process of claim 1, wherein the glass melt comprises a glass composition selected from a group consisting of soda-lime glass, borosilicate glass, aluminosilicate glass, and glass comprising from 5 mol % to 20 mol % boric oxide based on all oxides present in the glass composition.

### Claim 20 (depends on 1)

The process of claim 1, wherein the glass melt comprises a glass composition comprising 60 to 85 mol % SiO2, 5 to 20 mol % B2O3, 2 to 10 mol % Al2O3, 0 to 2 mol % Fe2O3, 2 to 10 mol % Na2O, 0 to 5 mol % K2O, 0 to 2 mol % BaO, 0 to 2 mol % CaO, and 0 to 10 mol % TiO2, based on all oxides present in the glass composition.