# US 2026/0097958 A1 · Benchtop method for making thermoelectric silver selenide-based materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0097958 A1
- Document ID: US20260097958A1
- Status: Published application
- Kind: A1
- Application number: 19/339,536
- Filed: 2025-09-25
- Published: 2026-04-09
- Earliest claimed: 2024-10-04
- Assignees: Iowa State University Research Foundation, Inc.
- Applicants: Iowa State University Research Foundation, Inc.
- Inventors: Kirill Kovnir; Yao Abusa
- Web page: https://patentgrep.com/patent/US20260097958A1

## CPC

- C01B 19/007: {Tellurides or selenides of metals (C01B19/002 takes precedence)}
- C01P 2002/54: one element only
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/82: by IR- or Raman-data
- C01P 2002/85: by XPS, EDX or EDAX data
- C01P 2002/88: by thermal analysis data, e.g. TGA, DTA, DSC
- C01P 2004/03: obtained by SEM
- C01P 2004/04: obtained by TEM, STEM, STM or AFM
- C01P 2006/40: Electric properties
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Disclosed are embodiments of a near-room temperature thermoelectric material β-Ag2Se. Interstitial, vacancy, and substitutional doping has been used to tune the charge and heat transport properties of the parent β-Ag2Se structure to enhance thermoelectric performance. The transformation of β-Ag2Se into α-Ag2Se at ˜134° C. and the low solubility of dopants are obstacles to this doping approach. Embodiments of the present disclosure relate to a facile, safe, scalable, and cost-effective benchtop approach to successfully produce doped β-Ag2Se. The doped materials provide enhancement of thermoelectric performance with a high peak zT of 1.30 at 117° C. and an average zT of about 1.15 in the 25-120° C. range for 0.2 at. % Zn-doped Ag2Se. Zn doping into Ag vacancies/interstitials creates point defects, enhancing the scattering of phonons and tuning the charge carrier properties—leading to the significant suppression of thermal conductivity.

## Claims

### Claim 1

A method of preparing a thermoelectric compound, comprising:
heating a solution comprising Se to a temperature below 130° C.;
adding a first compound comprising Ag to the solution to form a mixture; and
reacting the mixture to produce a β-Ag2Se compound.

### Claim 2 (depends on 1)

The method of claim 1, wherein the solution comprises a monoamine, a polyamine, or an alkanol amine.

### Claim 3 (depends on 1)

The method of claim 1, wherein the solution comprises ethylenediamine, diaminopropane, diethylenetriamine, alkylamine, ethanolamine, or propanolamine.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first compound is a salt of Ag.

### Claim 5 (depends on 4)

The method of claim 4, wherein the salt of Ag is a halide, AgNO3 and Ag2CO3.

### Claim 6 (depends on 1)

The method of claim 1, wherein the adding further comprises adding a second compound comprising an element other than Ag.

### Claim 7 (depends on 6)

The method of claim 6, wherein the element is Zn, Mg, Al, P, Si, Mn, Ni, Pb, Cd, Sn, Bi, S, or Te.

### Claim 8 (depends on 6)

The method of claim 6, wherein the β-Ag2Se compound comprises up to 1.0 at % of the element.

### Claim 9 (depends on 1)

The method of claim 1, wherein the β-Ag2Se compound comprises a figure of merit zT of at least 0.7 at 120° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the β-Ag2Se compound comprises an average figure of merit zT of at least 0.98 across a whole temperature range of 25° C. to 120° C.

### Claim 11

A method of preparing a thermoelectric compound, comprising:
adding one or more solid reactants comprising Se and Ag to a solvent to form a mixture, the solvent being heated to a temperature below 130° C.; and
reacting the mixture to produce a β-Ag2Se compound.

### Claim 12 (depends on 11)

The method of claim 11, wherein the solvent comprises a monoamine, a polyamine, or an alkanol amine.

### Claim 13 (depends on 11)

The method of claim 11, wherein the solvent comprises ethylenediamine, diaminopropane, diethylenetriamine, alkyl amine, ethanolamine, or propanol amine.

### Claim 14 (depends on 11)

The method of claim 11, wherein a first solid reactant of the one or more solid reactants is a salt of Ag.

### Claim 15 (depends on 14)

The method of claim 14, wherein the salt of Ag is a halide, AgNO3 and Ag2CO3.

### Claim 16 (depends on 14)

The method of claim 14, wherein a second solid reactant of the one or more solid reactants is elemental selenium.

### Claim 17 (depends on 16)

The method of claim 16, wherein the one or more solid reactants further comprises a third solid reactant comprising an element other than Ag.

### Claim 18 (depends on 17)

The method of claim 17, wherein the element is Zn, Mg, Al, P, Si, Mn, Ni, Pb, Cd, Sn, Bi, S, or Te.

### Claim 19 (depends on 17)

The method of claim 17, wherein the β-Ag2Se compound comprises up to 1.0 at % of the element.

### Claim 20 (depends on 11)

The method of claim 11, wherein the β-Ag2Se compound comprises a figure of merit zT of at least 0.7 at 120° C.

### Claim 21 (depends on 11)

The method of claim 11, wherein the β-Ag2Se compound comprises an average figure of merit zT of at least 0.98 across a whole temperature range of 25° C. to 120° C.

### Claim 22

A thermoelectric compound, comprising:
β-Ag2Se; and
a dopant;
wherein the thermoelectric compound comprises a figure of merit zT of at least 0.7 at 120° C.

### Claim 23 (depends on 22)

The thermoelectric compound of claim 22, wherein the dopant is Zn, Mg, Al, P, Si, Mn, Ni, Pb, Cd, Sn, Bi, S, or Te.

### Claim 24 (depends on 22)

The thermoelectric compound of claim 22, wherein the thermoelectric comopund comprises up to 1.0 at % of the dopant.

### Claim 25 (depends on 22)

The thermoelectric compound of claim 22, wherein the thermoelectric compound comprises an average figure of merit zT of at least 0.98 across a whole temperature range of 25° C. to 120° C.