- Number: US 2026/0096555 A1
- Document ID: US20260096555A1
- Status: Published application
- Kind: A1
- Application number: 18/907,511
- Filed: 2024-10-05
- Published: 2026-04-09
- Earliest claimed: 2024-03-20
- Inventors: Marion L. Chiattello; Mark Oman
- Web page: https://patentgrep.com/patent/US20260096555A1

## CPC

- A01N 33/08: containing oxygen or sulfur
- A01N 25/10: Macromolecular compounds
- A01N 25/34: Shaped forms, e.g. sheets, not provided for in any other sub-group of this main group
- A01N 33/04: Nitrogen directly attached to aliphatic or cycloaliphatic carbon atoms
- A01N 33/12: Quaternary ammonium compounds
- A01N 43/36: five-membered rings
- A01P 1/00: Disinfectants; Antimicrobial compounds or mixtures thereof
- A01P 3/00: Fungicides
- A01N: PRESERVATION OF BODIES OF HUMANS OR ANIMALS OR PLANTS OR PARTS THEREOF (preservation of food or foodstuff A23); BIOCIDES, e.g. AS DISINFECTANTS, AS PESTICIDES OR AS HERBICIDES (preparations for medical, dental or toiletry purposes which kill or prevent the growth or proliferation of unwanted organisms A61K); PEST REPELLANTS OR ATTRACTANTS; PLANT GROWTH REGULATORS
- A01P: BIOCIDAL, PEST REPELLANT, PEST ATTRACTANT OR PLANT GROWTH REGULATORY ACTIVITY OF CHEMICAL COMPOUNDS OR PREPARATIONS

## Abstract

A method for treating a fungus, comprising the steps of: providing, in a formulation, a polyethylenimine at a pH of less than two, a majority of protonated sites on the polyethylenimine associated with chloride counterions; exchanging at least ten percent of the chloride counterions for hydroxide anions bound to an anion exchange material resultant in bound chloride ions on the anion exchange material; separating the anion exchange material from the solution, the step of separating resultant in at least a ten percent reduction of the chloride counterions associated with the polyethylenimine; and inactivating at least fifty percent of the fungus within ten hours through treatment of the fungus with the formulation.

## Claims

### Claim 1

A method for treating a fungus, comprising the steps of:
providing, in a solution, a polyethylenimine at a pH of less than two, a majority of protonated sites on said polyethylenimine associated with chloride counterions;
exchanging at least ten percent of said chloride counterions for hydroxide anions bound to an anion exchange material resultant in bound chloride ions on said anion exchange material;
separating said anion exchange material from said solution, said step of separating resultant in at least a ten percent reduction of said chloride counterions associated with said polyethylenimine; and
inactivating at least fifty percent of the fungus within ten hours through treatment of the fungus with said solution.

### Claim 2 (depends on 1)

The method of claim 1, further comprising the step of:
preparing a formulation of said polyethylenimine through addition of an organic solvent to said solution.

### Claim 3 (depends on 2)

The method of claim 2, further comprising the steps of:
applying said formulation to a textile; and
said step of inactivating further comprising the step of: killing, with a contact time of the fungus with the solution of less than ten minutes, greater than sixty percent of the fungus.

### Claim 4 (depends on 2)

The method of claim 2, further comprising the step of:
controlling anions in said formulation to yield an activity coefficient (Y) in a range of 0.93 to 0.999 for at least one protonated secondary amine of said polyethylenimine.

### Claim 5 (depends on 2)

The method of claim 2, further comprising the step of:
adding a conjugate base of an organic acid to said formulation, wherein a ratio of said conjugate base to said chloride counterions comprises a ratio of greater than 1-to-20.

### Claim 6 (depends on 1)

The method of claim 1, said step of exchanging further comprising the step of:
releasing free hydroxide ions from said anion exchange material; and
increasing a pH of said solution, by at least one pH unit, as a result of said free hydroxide ions reacting with protons in said solution.

### Claim 7 (depends on 6)

The method of claim 6, further comprising the step of:
forming from said solution an antifungal film, said antifungal film comprising: (1) a mean thickness of less than 5 μm and (2) a total cationic charge of said protonated sites in a range of 0.1 to 1.8 C/in2.

### Claim 8 (depends on 7)

The method of claim 7, further comprising the step of:
exchanging at least 0.01 percent of said chloride counterions associated with said protonated sites for formate.

### Claim 9 (depends on 8)

The method of claim 8, further comprising the step of:
adding to said solution at least 400 ppm formic acid.

### Claim 10 (depends on 6)

The method of claim 6, further comprising the step of:
forming a film from said solution with a total cationic charge in a range of 0.001 to 10.0 coulombs per square inch, said total cationic charge offset by anions.

### Claim 11 (depends on 10)

The method of claim 10, further comprising the step of:
inactivating greater than fifty percent of non-enveloped viruses contacting said film in less than ten minutes.

### Claim 12 (depends on 6)

The method of claim 6, further comprising the step of:
partially drying said solution into a tacky film comprising a static coefficient of friction, μs, of greater than 1.1; and
said step of inactivating, killing at least 95% of the fungus within 10 minutes of the fungus contacting said tacky film.

### Claim 13 (depends on 1)

The method of claim 1, further comprising the steps of:
adding at least one organic solvent to said solution for form a formulation; and
packaging said formulation in a container, said formulation comprising a total cationic charge density, from said polyethylenimine, in a range of 0.001 to 0.95 meq/g, wherein anions electrostatically offset at least 95% of said total cationic charge density.

### Claim 14 (depends on 13)

The method of claim 13, further comprising the steps of:
adding a salt of a polydiallyldimethylammonium to said formulation; and
inactivating greater than 99.9% of Candida Auris with said formulation with a contact time of 2 minutes according to a JIS 1902 test protocol.

### Claim 15 (depends on 2)

The method of claim 2, further comprising the steps of:
applying said formulation to a substrate to form a film;
rubbing said film with a pressure exceeding four pounds of pressure; and
killing, after said step of rubbing and with a contact time of the fungus with the film of less than thirty minutes, greater than 50% of the fungus.

### Claim 16 (depends on 1)

The method of claim 1 further comprising the steps of:
combining in a formulation of said solution: a salt of a polydiallyldimethylammonium, an organic solvent, and water, said formulation comprising a pH of 4.5±2.0, said step of combining further comprising the step of:
controlling a concentration of said polydiallyldimethylammonium to greater than 50 mg per liter in said formulation to yield a self-spreading surface tension, of said formulation, of less than 50 mN/m; and
spreading the formulation on a substrate to yield an antifungal film, said antifungal film comprising: (1) 5 to 1500 μg per square inch of said polydiallyldimethylammonium; and
killing at least ninety percent of the fungus within ten hours through treatment of the fungus with said formulation.