# US 2026/0096357 A1 · Titanium silicon nitride barrier layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0096357 A1
- Document ID: US20260096357A1
- Status: Published application
- Kind: A1
- Application number: 19/315,375
- Filed: 2025-08-29
- Published: 2026-04-02
- Earliest claimed: 2019-10-08
- Assignees: Eugenus, Inc.
- Applicants: Eugenus, Inc.
- Inventors: Jae Seok Heo; Jerry Mack; Somilkumar J. Rathi; Niloy Mukherjee
- Web page: https://patentgrep.com/patent/US20260096357A1

## CPC

- H10N 70/8413: {adapted for resistive heating}
- H10N 70/011: {Manufacture or treatment of multistable switching devices}
- H10N 70/231: {based on solid-state phase change, e.g. between amorphous and crystalline phases, Ovshinsky effect}
- H10N 70/8828: {Tellurides, e.g. GeSbTe}
- H10B 63/24: {of the Ovonic threshold switching type}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

The disclosed technology generally relates to a barrier layer comprising titanium silicon nitride, and more particularly to a barrier layer for nonvolatile memory devices, and methods of forming the same. In one aspect, a method of forming an electrode for a phase change memory device comprises forming over a semiconductor substrate an electrode comprising titanium silicon nitride (TiSiN) on a phase change storage element configured to store a memory state. Forming the electrode comprises exposing a semiconductor substrate to one or more cyclical vapor deposition cycles, wherein a plurality of the cyclical vapor deposition cycles comprises an exposure to a Ti precursor, an exposure to a N precursor and an exposure to a Si precursor.

## Claims

### Claim 1

(canceled)

### Claim 2

A method of forming one or more electrodes for a memory device, the method comprising:
providing a substrate having formed thereover a chalcogenide alloy layer; and
forming an electrode comprising titanium silicon nitride (TiSiN) over the chalcogenide alloy layer by exposing the substrate, without aid of plasma, to one or more vapor deposition cycles comprising alternating and non-overlapping exposures to one or more first deposition phases and one or more second deposition phases,
wherein each of the one or more first deposition phases comprises exposures of the substrate to a titanium (Ti) precursor alternating with a nitrogen (N) precursor,
wherein each of the one or more second deposition phases comprises exposures of the substrate to a silicon (Si) precursor and the N precursor, and
wherein in at least one of the first deposition phases, the exposure to the N precursor follows the exposure to the Ti precursor without an intervening exposure to the Si precursor.

### Claim 3 (depends on 2)

The method of claim 2, wherein the electrode is formed at a first side of the chalcogenide alloy layer, and wherein the method further comprises forming a second electrode comprising TiSiN over the chalcogenide alloy layer at a second side of the chalcogenide alloy layer opposite the first side.

### Claim 4 (depends on 3)

The method of claim 3, wherein the chalcogenide alloy layer comprises an Ovonic threshold switching material.

### Claim 5 (depends on 4)

The method of claim 4, wherein no other chalcogenide alloy layer is present between the electrode and the second electrode.

### Claim 6 (depends on 2)

The method of claim 2, wherein forming the electrode comprises exposing the substrate to the one or more vapor deposition cycles at a temperature lower than 400° C.

### Claim 7 (depends on 2)

The method of claim 2, wherein the electrode is at least partially amorphous.

### Claim 8 (depends on 2)

The method of claim 2, wherein forming the electrode comprises adjusting a silicon concentration such that the electrode has an electrical resistivity between about 500 μΩ-cm and about 30,000 μΩ-cm.

### Claim 9 (depends on 2)

The method of claim 2, wherein the electrode has a silicon concentration exceeding about 5 atomic %.

### Claim 10 (depends on 2)

The method of claim 2, wherein the electrode is interposed between the chalcogenide alloy layer and a metallization line.

### Claim 11 (depends on 10)

The method of claim 10, wherein the metallization line comprises one of a wordline and a bitline, and wherein the memory device further comprises the other of the wordline and the bitline crossing the one of the wordline and the bitline.

### Claim 12

A method of forming one or more electrodes for a memory device, the method comprising:
providing a substrate having formed thereover a chalcogenide alloy layer;
forming an electrode comprising titanium silicon nitride (TiSiN) over the chalcogenide alloy layer by exposing the substrate at a temperature lower than 400° C. to one or more vapor deposition cycles, wherein each of the one or more vapor deposition cycles comprises an exposure to a titanium (Ti) precursor, an exposure to a nitrogen (N) precursor, and an exposure to a silicon (Si) precursor, and
wherein the exposure to the N precursor follows the exposure to the Ti precursor without an intervening exposure to the Si precursor.

### Claim 13 (depends on 12)

The method of claim 12, wherein the chalcogenide alloy layer comprises an Ovonic threshold switching material.

### Claim 14 (depends on 13)

The method of claim 13, wherein the electrode is formed at a first side of the chalcogenide alloy layer, and wherein the method further comprises forming a second electrode comprising TiSiN over the chalcogenide alloy layer at a second side of the chalcogenide alloy layer opposite the first side.

### Claim 15 (depends on 14)

The method of claim 14, wherein no other chalcogenide alloy layer is present between the electrode and the second electrode.

### Claim 16 (depends on 15)

The method of claim 15, wherein the chalcogenide alloy layer, the electrode and the second electrode is formed between a wordline and a bitline crossing each other in orthogonal directions.

### Claim 17 (depends on 12)

The method of claim 12, wherein forming the electrode comprises exposing the substrate to the one or more vapor deposition cycles at the temperature greater than 200° C. and less than 400° C.

### Claim 18 (depends on 12)

The method of claim 12, wherein the electrode is at least partially amorphous.

### Claim 19 (depends on 12)

The method of claim 12, wherein forming the electrode comprises forming by thermal atomic layer deposition.

### Claim 20 (depends on 12)

The method of claim 12, wherein the Si precursor is a precursor selected from the group consisting of SiH4, Si2H6, SiH2Cl2, SiH3Cl1, Si2Cl6 and Si3Cl8.