# US 2026/0096347 A1 · Piezoelectric element and liquid ejection head

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0096347 A1
- Document ID: US20260096347A1
- Status: Published application
- Kind: A1
- Application number: 19/342,946
- Filed: 2025-09-29
- Published: 2026-04-02
- Earliest claimed: 2024-09-30
- Assignees: Seiko Epson Corporation
- Applicants: Seiko Epson Corporation
- Inventors: Nobuo OZAWA; Takatoshi YAMAZAKI; Toshihiro SHIMIZU; Shunsuke YOSHIDA
- Web page: https://patentgrep.com/patent/US20260096347A1

## CPC

- H10N 30/708: {Intermediate layers, e.g. barrier, adhesion or growth control buffer layers}
- B41J 2/14233: {of film type, deformed by bending and disposed on a diaphragm}
- B41J 2/161: {of film type, deformed by bending and disposed on a diaphragm}
- H10N 30/2047: {Membrane type}
- H10N 30/501: {having a non-rectangular cross-section in a plane parallel to the stacking direction, e.g. polygonal or trapezoidal in side view}
- H10N 30/8554: {Lead-zirconium titanate [PZT] based}
- H10N 30/872: {Interconnections, e.g. connection electrodes of multilayer piezoelectric or electrostrictive devices}
- H10N 30/883: {Additional insulation means preventing electrical, physical or chemical damage, e.g. protective coatings}
- B41J 2002/14241: {having a cover around the piezoelectric thin film element}
- B41J 2002/14258: {Multi layer thin film type piezoelectric element}
- B41J 2002/14419: {Manifold}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- B41J: TYPEWRITERS; SELECTIVE PRINTING MECHANISMS, i.e. MECHANISMS PRINTING OTHERWISE THAN FROM A FORME; CORRECTION OF TYPOGRAPHICAL ERRORS

## Abstract

In a piezoelectric element in which a lower electrode, a piezoelectric layer formed of a perovskite-type complex oxide, and an upper electrode are laminated in a laminating direction, the upper electrode has a first hydrogen absorbing layer that absorbs hydrogen. The upper electrode of the piezoelectric element preferably has a second hydrogen absorbing layer different from the first hydrogen absorbing layer. In the piezoelectric element, the film thickness of the first hydrogen absorbing layer is preferably thicker than the film thickness of the second hydrogen absorbing layer in the laminating direction.

## Claims

### Claim 1

A piezoelectric element comprising:
a lower electrode;
a piezoelectric layer formed of a perovskite-type complex oxide; and
an upper electrode having a first hydrogen absorbing layer, wherein
the lower electrode, the piezoelectric layer, and the upper electrode are laminated in a laminating direction, and
the upper electrode has a first hydrogen absorbing layer that absorbs hydrogen.

### Claim 2 (depends on 1)

The piezoelectric element according to claim 1, wherein
the upper electrode has a second hydrogen absorbing layer different from the first hydrogen absorbing layer.

### Claim 3 (depends on 2)

The piezoelectric element according to claim 2, wherein
a film thickness of the first hydrogen absorbing layer is thicker than a film thickness of the second hydrogen absorbing layer in the laminating direction.

### Claim 4 (depends on 2)

The piezoelectric element according to claim 2, wherein
a hydrogen content of the first hydrogen absorbing layer is greater than a hydrogen content of the second hydrogen absorbing layer.

### Claim 5 (depends on 2)

The piezoelectric element according to claim 2, wherein
the upper electrode has an electrode layer formed of a conductive material, and
the electrode layer is provided between the second hydrogen absorbing layer and the first hydrogen absorbing layer in the laminating direction.

### Claim 6 (depends on 2)

The piezoelectric element according to claim 2, wherein
the upper electrode has an electrode layer formed of a conductive material, and
a hydrogen content of the electrode layer is smaller than the hydrogen content of the first hydrogen absorbing layer.

### Claim 7 (depends on 1)

The piezoelectric element according to claim 1, wherein
the film thickness of the first hydrogen absorbing layer is 10 nm or more and 25 nm or less.

### Claim 8 (depends on 1)

The piezoelectric element according to claim 1, wherein
the piezoelectric layer is formed of a plurality of layers, and
variation in a hydrogen content at a central section of the piezoelectric layer is 24% or less with respect to an average value.

### Claim 9 (depends on 1)

The piezoelectric element according to claim 1, further comprising:
a protective film provided on the piezoelectric layer to protect the piezoelectric layer, wherein the first hydrogen absorbing layer is provided on the protective film.

### Claim 10 (depends on 1)

The piezoelectric element according to claim 1, further comprising:
a third hydrogen absorbing layer that absorbs hydrogen provided between the piezoelectric layer and the lower electrode, or on the lower electrode.

### Claim 11 (depends on 1)

The piezoelectric element according to claim 1, further comprising:
a hydrogen barrier layer that suppresses hydrogen from entering into an uppermost layer in the laminating direction.

### Claim 12 (depends on 1)

A liquid ejection head comprising:
the piezoelectric element according to claim 1.