# US 2026/0096135 A1 · Semiconductor structure and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0096135 A1
- Document ID: US20260096135A1
- Status: Published application
- Kind: A1
- Application number: 18/938,230
- Filed: 2024-11-05
- Published: 2026-04-02
- Earliest claimed: 2024-10-01
- Assignees: United Microelectronics Corp.
- Applicants: United Microelectronics Corp.
- Inventors: Huang-I Chen; Cheng-Hsin Lee; Cheng-Hua Chou
- Web page: https://patentgrep.com/patent/US20260096135A1

## CPC

- H10D 30/6215: {having multiple independently-addressable gate electrodes}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 62/10: Shapes, relative sizes or dispositions of the regions of the semiconductor bodies; Shapes of the semiconductor bodies
- H10D 62/126: {Top-view geometrical layouts of the regions or the junctions}
- H10P 14/68: Organic materials, e.g. photoresists
- H10P 32/20: Diffusion for doping of insulating layers
- H10P 50/283: {by chemical means}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The invention provides a method for manufacturing a semiconductor structure, which comprises the following steps: providing a substrate with a shallow trench isolation structure and a first active area, wherein a top surface of the shallow trench isolation structure is higher than a top surface of the substrate in the first active area, performing an etching step to remove part of the shallow trench isolation structure so that the top surface of the shallow trench isolation structure is lower than that of the substrate in the first active area, and after the etching step, a doping step is performed on the first active area.

## Claims

### Claim 1

A manufacturing method of a semiconductor structure, comprising:
providing a substrate, wherein a shallow trench isolation structure and a first active area are formed on the substrate, wherein a top surface of the shallow trench isolation structure is higher than a top surface of the substrate in the first active area;
performing an etching step to remove part of the shallow trench isolation structure so that the top surface of the shallow trench isolation structure is lower than the top surface of the substrate of the first active area; and
performing a doping step on the first active area after the etching step.

### Claim 2 (depends on 1)

The method for manufacturing a semiconductor structure according to claim 1, wherein after the etching step, a height difference between the top surface of the shallow trench isolation structure and the top surface of the first active area is defined as H1, where H1 is between 2 nm and 10 nm.

### Claim 3 (depends on 2)

The method for manufacturing a semiconductor structure according to claim 2, wherein after the etching step, a depth of the shallow trench isolation structure is defined as D1, wherein the ratio of H1 to D1 is less than 0.05.

### Claim 4 (depends on 1)

The method for manufacturing a semiconductor structure according to claim 1, wherein, from a top view, a length of the first active area is defined as L1 and a width is defined as W1, wherein the width W1 is less than 250 nm.

### Claim 5 (depends on 4)

The method for manufacturing a semiconductor structure according to claim 4, wherein the ratio of the length L1 to the width W1 is greater than 0.1.

### Claim 6 (depends on 1)

The method for manufacturing a semiconductor structure according to claim 1, further comprising forming an oxide layer and a nitride layer on the first active area, wherein the nitride layer is stacked on the oxide layer.

### Claim 7 (depends on 6)

The method for manufacturing a semiconductor structure according to claim 6, wherein a part of the oxide layer is removed during the etching step, so that a width of the oxide layer is smaller than a width of the nitride layer.

### Claim 8 (depends on 6)

The method for manufacturing a semiconductor structure according to claim 6, wherein after the etching step, the oxide layer and the nitride layer are completely removed, and then the doping step is then performed.

### Claim 9 (depends on 6)

The method for manufacturing a semiconductor structure according to claim 6, wherein before the etching step, the top surface of the shallow trench isolation structure is aligned with a top surface of the nitride layer in the horizontal direction.

### Claim 10 (depends on 1)

The method for manufacturing a semiconductor structure according to claim 1, wherein the interface of the first active area and the shallow trench isolation structure comprises a rounded corner.

### Claim 11 (depends on 1)

The method for manufacturing a semiconductor structure according to claim 1, wherein after the doping step, further comprising forming a first gate structure on the first active area and part of the shallow trench isolation structure, wherein a bottom surface of the first gate structure contacting the first active area is defined as a first bottom surface, and a bottom surface of the first gate structure contacting the shallow trench isolation structure is defined as a second bottom surface, wherein the height difference between the first bottom surface and the second bottom surface in a vertical direction is within 10 nanometers.

### Claim 12 (depends on 1)

The method for manufacturing a semiconductor structure according to claim 1, wherein the etching step comprises a wet etching step, and the wet etching step comprises a buffered oxide etch (BOE) etching step.

### Claim 13 (depends on 1)

The method for manufacturing a semiconductor structure according to claim 1, further comprising forming a second active area in the substrate, wherein the shallow trench isolation structure is located between the first active area and the second active area.

### Claim 14 (depends on 13)

The method for manufacturing a semiconductor structure according to claim 13, wherein the doping step further comprises doping the first active area and the second active area respectively, so as to dope the first active area and the second active area with ions of different conductivity types.

### Claim 15

A semiconductor structure, comprising:
a substrate including a first active area;
a shallow trench isolation structure located on the substrate and around the first active area, wherein a top surface of the shallow trench isolation structure is lower than a top surface of the substrate of the first active area, and a height difference between the top surface of the shallow trench isolation structure and the top surface of the first active area is defined as H1, where H1 is between 2 nm and 10 nm.

### Claim 16 (depends on 15)

The semiconductor structure according to claim 15, wherein a depth of the shallow trench isolation structure is defined as D1, and the ratio of H1 to D1 is less than 0.1.

### Claim 17 (depends on 15)

The semiconductor structure according to claim 15, wherein when viewed from a top view, a length of the first active area is defined as L1 and a width is defined as W1, wherein the width W1 is less than 250 nm, and the ratio of the length L1 to the width W1 is greater than 0.1.

### Claim 18 (depends on 15)

The semiconductor structure according to claim 15, wherein the interface of the first active area and the shallow trench isolation structure comprises a rounded corner.

### Claim 19 (depends on 15)

The semiconductor structure according to claim 15, further comprising a first gate structure on the first active area and part of the shallow trench isolation structure, wherein a bottom surface of the first gate structure contacting the first active area is defined as a first bottom surface, and a bottom surface of the first gate structure contacting the shallow trench isolation structure is defined as a second bottom surface, wherein the height difference between the first bottom surface and the second bottom surface in a vertical direction is within 10 nanometers.

### Claim 20 (depends on 15)

The semiconductor structure according to claim 15, further comprising a second active area, wherein the shallow trench isolation structure is located between the first active area and the second active area, and the first active area and the second active area are respectively doped with ions of different conductivity types.