# US 2026/0096091 A1 · Memory device having ultra-lightly doped region and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0096091 A1
- Document ID: US20260096091A1
- Status: Published application
- Kind: A1
- Application number: 19/411,437
- Filed: 2025-12-08
- Published: 2026-04-02
- Earliest claimed: 2022-12-09
- Assignees: Nanya Technology Corporation
- Applicants: Nanya Technology Corporation
- Inventors: CHUNG-LIN HUANG
- Web page: https://patentgrep.com/patent/US20260096091A1

## CPC

- H10B 12/34: {the transistor being at least partially in a trench in the substrate}
- H10B 12/053: {the transistor being at least partially in a trench in the substrate (vertical transistor in combination with a capacitor formed in a substrate trench H10B12/0383)}
- H10B 12/488: {Word lines}
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

The present application provides a memory device having an ultra-lightly doped region and a manufacturing method of the memory device. The memory device includes a semiconductor substrate including a word line extending into the semiconductor substrate, wherein the semiconductor substrate is defined with a source region, a drain region and an ultra-lightly doped region under the drain region, the word line is disposed between the source region and the drain region, and the ultra-lightly doped region is disposed at a sidewall of the word line.

## Claims

### Claim 1

A method of manufacturing a memory device, comprising:
providing a semiconductor substrate;
forming a word line extending into the semiconductor substrate;
forming a recess adjacent to the word line; and
implanting dopants into the semiconductor substrate through the recess,
wherein the dopants collide with the semiconductor substrate exposed through the recess and diffuse across the word line to form an ultra-lightly doped region over a sidewall of the word line.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the implantation of the dopants is performed after the formation of the word line.

### Claim 3 (depends on 1)

The method according to claim 1, wherein a depth of the recess is substantially less than a depth of the word line.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the depth of the word line is about 120 nm to about 200 nm.

### Claim 5 (depends on 3)

The method according to claim 3, wherein the depth of the recess is about 10 nm to about 50 nm.

### Claim 6 (depends on 1)

The method according to claim 1, further comprising disposing a hard mask layer over the semiconductor substrate prior to the implantation of the dopants.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the hard mask layer is removed after the implantation of the dopants.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the hard mask layer includes nitride.

### Claim 9 (depends on 1)

The method according to claim 1, wherein a thickness of the hard mask layer is about 30 nm to about 50 nm.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the hard mask layer blocks the dopants from being implanted into the semiconductor substrate.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the dopants are partially blocked by the word line.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the dopants have a kinetic energy in a range of about 1 KeV to about 30 KeV.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the dopants include boron, phosphorous or arsenic.

### Claim 14 (depends on 1)

The method according to claim 1, further comprising forming a plug within the recess after the implantation of the dopants.

### Claim 15 (depends on 1)

The method according to claim 1, wherein a semiconductive material is deposited into the recess after the implantation of the dopants.