# US 2026/0094852 A1 · Solid-state electrolyte sheet, solid oxide fuel cell, solid oxide electrolyzer cell, and methods of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0094852 A1
- Document ID: US20260094852A1
- Status: Published application
- Kind: A1
- Application number: 19/338,303
- Filed: 2025-09-24
- Published: 2026-04-02
- Earliest claimed: 2024-10-01
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Shyam Lekhraj Chatlani; Rahul Suryakant Kadam; Timothy Joseph Markel; Nathan Michael Zink
- Web page: https://patentgrep.com/patent/US20260094852A1

## CPC

- H01M 8/1253: the electrolyte containing zirconium oxide
- H01M 8/126: the electrolyte containing cerium oxide
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A solid-state electrolyte sheet includes stabilized zirconia grains having from 3 mol % to 12 mol % of a dopant selected from alumina, cerium oxide, gadolinium oxide, scandia, yttria, ytterbia, and combinations thereof. In aspects, the solid-state electrolyte sheet exhibits an ionic conductivity of 6.79 S/m or more at 800° C. or 8.8 S/m or more at 835° C. In aspects, the stabilized zirconia grains can exhibit a ratio of a cubic phase to a tetragonal phase (C/T ratio) of 0.12 or more. In aspects, the solid-state electrolyte sheet can be part of a solid oxide fuel cell and/or a solid oxide electrolyzer cell. Methods include casting a green tape comprising stabilized zirconia and firing the green tape by heating to form a sintered tape and then quenching the sintered tape from a starting temperature of 600° C. or more to a final temperature of less than 100° C.

## Claims

### Claim 1

A solid-state electrolyte sheet comprising:
stabilized zirconia grains comprising from 3 mol % to 12 mol % of a dopant selected from a group consisting of alumina, cerium oxide, gadolinium oxide, scandia, yttria, ytterbia, and combinations thereof;
a thickness in a range from 10 micrometers to 300 micrometers; and
an ionic conductivity at 800° C. of 6.79 S/m or more.

### Claim 2 (depends on 1)

The solid-state electrolyte sheet of claim 1, wherein the ionic conductivity at 835° C. of 8.8 S/m or more.

### Claim 3 (depends on 1)

The solid-state electrolyte sheet of claim 1, wherein the stabilized zirconia grains comprise a mixture of a cubic phase and a tetragonal phase.

### Claim 4 (depends on 1)

The solid-state electrolyte sheet of claim 1, wherein the stabilized zirconia grains exhibit a ratio of a cubic phase to a tetragonal phase (C/T ratio) of 0.12 or more.

### Claim 5 (depends on 4)

The solid-state electrolyte sheet of claim 4, wherein the C/T ratio is from 0.27 to 0.50.

### Claim 6 (depends on 1)

The solid-state electrolyte sheet of claim 1, wherein the ionic conductivity at 800° C. is 7.00 S/m or more, or the ionic conductivity at 835° C. is 9.0 S/m or more.

### Claim 7 (depends on 1)

The solid-state electrolyte sheet of claim 1, wherein a majority of pores in the solid-state electrolyte sheet is a closed porosity, and the solid-state electrolyte sheet comprises a porosity of 1.0% or less.

### Claim 8 (depends on 1)

The solid-state electrolyte sheet of claim 1, wherein the stabilized zirconia grains comprise from 3 mol % to about 6 mol % of the dopant, and the dopant comprises scandia.

### Claim 9 (depends on 1)

The solid-state electrolyte sheet of claim 1, wherein an average grain size of the stabilized zirconia grains is from 0.3 μm to 2.5 μm.

### Claim 10 (depends on 1)

The solid-state electrolyte sheet of claim 1, wherein an average grain size of the stabilized zirconia grains is from 1.01 μm to 2.5 μm.

### Claim 11 (depends on 1)

A solid oxide fuel cell comprising:
the solid-state electrolyte sheet of claim 1 comprising a first major surface and a second major surface with the thickness defined therebetween;
an oxygen electrode disposed on the first major surface; and
a fuel electrode disposed on the second major surface.

### Claim 12

A solid-state electrolyte sheet comprising:
stabilized zirconia grains comprising from about 3 mol % to about 12 mol % of a dopant selected from a group consisting of alumina, cerium oxide, gadolinium oxide, scandia, yttria, ytterbia, and combinations thereof;
a thickness in a range from about 10 micrometers to about 300 micrometers;
an ionic conductivity at 800° C. of 6.79 S/m or more; and
an ionic conductivity at 835° C. of 8.8 S/m or more,
wherein the stabilized zirconia grains exhibit a ratio of a cubic phase to a tetragonal phase (C/T ratio) from 0.15 to 0.50.

### Claim 13 (depends on 12)

The solid-state electrolyte sheet of claim 12, wherein the C/T ratio is from 0.27 to 0.50.

### Claim 14 (depends on 12)

The solid-state electrolyte sheet of claim 12, wherein:
the ionic conductivity at 800° C. is 7.00 S/m or more; or
the ionic conductivity at 835° C. is 9.0 S/m or more.

### Claim 15

A method of making a solid-state electrolyte sheet comprising:
casting a green tape comprising stabilized zirconia comprising from 3 mol % to 12 mol % of a dopant selected from a group consisting of alumina, cerium oxide, gadolinium oxide, scandia, yttria, ytterbia, and combinations thereof;
firing the green tape to form the solid-state electrolyte sheet, wherein the firing comprises:
heating the green tape at temperatures of 600° C. or more for 90 minutes or less with a maximum temperature of 1650° C. or less to form a sintered tape; and
quenching the sintered tape from a temperature of from a starting temperature of 500° C. or more to final temperature of less than 100° C.

### Claim 16 (depends on 15)

The method of claim 15, wherein the starting temperature for the quenching is from 600° C. to 1000° C., and the solid-state electrolyte sheet comprises stabilized zirconia grains comprise a mixture of a cubic phase and a tetragonal phase.

### Claim 17 (depends on 15)

The method of claim 15, wherein the stabilized zirconia grains in the solid-state electrolyte sheet exhibit a ratio of a cubic phase to a tetragonal phase (C/T ratio) is 0.12 or more, and an average grain size of the stabilized zirconia grains is from 0.3 μm to 2.5 μm.

### Claim 18 (depends on 15)

The method of claim 15, wherein a thickness of the solid-state electrolyte sheet is in a range from 10 micrometers to 300 micrometers, and a cubic phase is the predominant crystal phase in the stabilized zirconia grains, and a majority of pores in the solid-state electrolyte sheet is a closed porosity, and the solid-state electrolyte sheet comprises a porosity of 1% or less.

### Claim 19 (depends on 15)

The method of claim 15, wherein the dopant comprises scandia, the stabilized zirconia grains comprise from 3 mol % to about 6 mol % of the dopant, and the stabilized zirconia grains are free of at least one of alumina, yttria, a lanthanoid oxide, or combinations thereof.

### Claim 20 (depends on 15)

The method of claim 15, wherein the green tape, as a wt % of the green tape, comprises:
from 55 wt % to 70 wt % of the stabilized zirconia;
from 15 wt % to 25 wt % of a solvent;
from 10 wt % to 15 wt % of a polymeric binder;
from 0.1 wt % to 5 wt % of a dispersant; and
from 0.1 wt % to 2 wt % of a protic base.