# US 2026/0094851 A1 · Electrolyte membrane for patterned membrane-electrode assembly and method for preparing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0094851 A1
- Document ID: US20260094851A1
- Status: Published application
- Kind: A1
- Application number: 19/293,582
- Filed: 2025-08-07
- Published: 2026-04-02
- Earliest claimed: 2024-09-10
- Assignees: Hyundai Motor Company; Kia Corporation; Kookmin University Industry Academic Cooperation
- Applicants: Hyundai Motor Company; Kia Corporation; Kookmin University Industry Academic Cooperation
- Inventors: Songi Oh; Won Jae Choi; So Hwa Kim; Da Hee Kwak; Ah Hyeon Park; Jee Youn Hwang; Sung Hee Shin; Se Geun Jang; Sang Hyeok Lee; Yeon Jae Lee
- Web page: https://patentgrep.com/patent/US20260094851A1

## CPC

- H01M 8/1023: having only carbon, e.g. polyarylenes, polystyrenes or polybutadiene-styrenes
- C25B 13/08: based on organic materials
- H01M 8/1004: characterised by membrane-electrode assemblies [MEA] (H01M8/12 takes precedence)
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- H01M 2300/0082: Organic polymers
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A hydrocarbon-based ion exchange membrane is hydrated, then compressed with a mesh template to form an embedded pattern on its surface. After dehydration, the template is removed, yielding an electrolyte membrane featuring improved water uptake, ion conductivity, and mechanical properties. The method supports large-area production at about 70° C. to 90° C. under pressures of about 5 MPa to 15 MPa. A catalyst slurry can be applied to the patterned membrane to create a membrane-electrode assembly, enhancing bonding strength and catalyst utilization in electrochemical devices such as fuel cells and water electrolyzers. The resulting membrane has a moisture content of about 60% by weight or more, a Young's modulus of about 100 MPa or less, and a pattern depth of about 40% or greater relative to the template wires.

## Claims

### Claim 1

A method for preparing an electrolyte membrane for a membrane-electrode assembly, the method comprising:
obtaining a first intermediate by hydrating a hydrocarbon-based ion exchange membrane ;
obtaining a second intermediate by stacking a template on at least one surface of the first intermediate and applying pressure in the stacking direction; and
obtaining the electrolyte membrane by dehydrating the second intermediate and removing the template from the second intermediate,
wherein the electrolyte membrane comprises a pattern having a shape corresponding to the template.

### Claim 2 (depends on 1)

The method of claim 1, wherein the step of obtaining the first intermediate is immersing the hydrocarbon-based ion exchange membrane in a solvent at about 70° C. to 90° C. for about 4 to 6 hours.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first intermediate obtained by immersing the hydrocarbon-based ion exchange membrane in a solvent at about 80° C. for about 4 hours has a moisture content of about 60% by weight or more.

### Claim 4 (depends on 1)

The method of claim 1, wherein when the hydrocarbon-based ion exchange membrane is immersed in a solvent at about 80° C. for about 4 hours, the hydrocarbon-based ion exchange membrane has a length change rate of about 10% or more.

### Claim 5 (depends on 1)

The method of claim 1, wherein when the hydrocarbon-based ion exchange membrane is immersed in a solvent at about 80° C. for about 4 hours, the hydrocarbon-based ion exchange membrane has a thickness change rate of about 30% or more.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first intermediate obtained by immersing the hydrocarbon-based ion exchange membrane in a solvent at about 80° C. for about 4 hours has a Young's modulus of about 100 MPa or less.

### Claim 7 (depends on 1)

The method of claim 1, wherein the template has a mesh-shape in which wires are intertwined in a net-like shape.

### Claim 8 (depends on 1)

The method of claim 1, wherein the template has a stiffness higher than a stiffness of the first intermediate.

### Claim 9 (depends on 1)

The method of claim 1, wherein the template comprises stainless steel.

### Claim 10 (depends on 1)

The method of claim 1, wherein the template has a width of about 300 mm or more and a length of about 500 mm or more, and the first intermediate has a size equal to or larger than a size of the template.

### Claim 11 (depends on 1)

The method of claim 1, wherein the template has a width of about 300 mm or more and a length of about 500 mm or more, and the first intermediate has a size equal to or smaller than a size of the template.

### Claim 12 (depends on 1)

The method of claim 1, wherein the step of obtaining the second intermediate is stacking the template on at least one surface of the first intermediate, and applying a pressure of about 5 MPa to 15 MPa in the stacking direction at about 70° C. to 90° C.

### Claim 13 (depends on 1)

The method of claim 1, wherein the step of obtaining the electrolyte membrane is dehydrating the second intermediate by compressing the second intermediate at about 70° C. to 90° C. for about 1 hour to 2 hours and removing the template.

### Claim 14 (depends on 1)

A method for manufacturing a membrane-electrode assembly, the method comprising a step of applying a catalyst slurry to both surfaces of the electrolyte membrane prepared according to claim 1 to manufacture a pair of electrodes, wherein the electrodes are filled in spaces of the electrolyte membrane formed to be embedded.

### Claim 15

An electrolyte membrane for a membrane-electrode assembly, the electrolyte membrane comprising a hydrocarbon-based ion exchange membrane,
wherein the hydrocarbon-based ion exchange membrane has a pattern with a shape corresponding to a pattern of a template, the pattern being formed to be embedded in at least one surface of the hydrocarbon-based ion exchange membrane, and the template has a mesh-shape in which wires are intertwined in a net-like shape.

### Claim 16 (depends on 15)

The electrolyte membrane of claim 15, wherein the hydrocarbon-based ion exchange membrane has a moisture content of about 60% by weight or more.

### Claim 17 (depends on 15)

The electrolyte membrane of claim 15, wherein the hydrocarbon-based ion exchange membrane has a longitudinal change rate of about 10% or more.

### Claim 18 (depends on 15)

The electrolyte membrane of claim 15, wherein the hydrocarbon-based ion exchange membrane has a width directional change rate of about 30% or more.

### Claim 19 (depends on 15)

The electrolyte membrane of claim 15, the hydrocarbon-based ion exchange membrane has a Young's modulus of about 100 MPa or less.

### Claim 20 (depends on 15)

The electrolyte membrane of claim 15, wherein the pattern formed to be embedded in the hydrocarbon-based ion exchange membrane has a depth of about 40% or more of the diameter of the cross section of the wires of the template.