# US 2026/0094845 A1 · Electrode for fuel cell with prevented ionomer poisoning of catalyst and reduced elution and method of manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0094845 A1
- Document ID: US20260094845A1
- Status: Published application
- Kind: A1
- Application number: 19/174,681
- Filed: 2025-04-09
- Published: 2026-04-02
- Earliest claimed: 2024-10-02
- Assignees: Hyundai Motor Company; Kia Corporation
- Applicants: Hyundai Motor Company; Kia Corporation
- Inventors: Il Seok Chae; Seong Hun Cho; Sang Jin Han
- Web page: https://patentgrep.com/patent/US20260094845A1

## CPC

- H01M 4/8605: {Porous electrodes}
- H01M 4/8663: {Selection of inactive substances as ingredients for catalytic active masses, e.g. binders, fillers}
- H01M 4/8668: {Binders}
- H01M 4/8828: {Coating with slurry or ink}
- H01M 4/926: {on carbon or graphite}
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An electrode for a fuel cell comprises an electrode binder and an electrode catalyst dispersed therein. The electrode catalyst includes a catalyst complex with a catalytic metal supported on a support and a porous polymer coating layer. The porous polymer enhances performance by forming a core-shell structure on the catalytic metal surface. A method of manufacturing the electrode includes involving preparation of the catalyst complex, coating the catalytic metal with the porous polymer to form an electrode catalyst, combining the catalyst with an electrode binder to prepare a slurry, and applying the slurry onto a substrate. The porous polymer is optionally a polymer of intrinsic microporosity (PIM) or a copolymer, with molecular weight, composition, and thickness optimized for conductivity and performance. The electrode is suitable for use in a membrane-electrode assembly for fuel cells.

## Claims

### Claim 1

An electrode for a fuel cell, the electrode comprising:
an electrode binder; and
an electrode catalyst admixed with the electrode binder,
wherein the electrode catalyst comprises:
a catalyst complex including a catalytic metal supported on a support; and
a coating layer of a porous polymer on at least a portion of a surface of the catalytic metal.

### Claim 2 (depends on 1)

The electrode of claim 1, wherein the electrode binder comprises a perfluorinated sulfonic acid polymer.

### Claim 3 (depends on 1)

The electrode of claim 1, wherein the catalytic metal comprises one or more of platinum, palladium, cobalt, gold, ruthenium, tin, molybdenum, rhodium, iridium, bismuth, copper, yttrium, and chromium.

### Claim 4 (depends on 1)

The electrode of claim 1, wherein the support comprises a carbon-based support, and the carbon-based support comprises one or more of carbon black, carbon nanotubes, graphite, and graphene.

### Claim 5 (depends on 1)

The electrode of claim 1, wherein the porous polymer comprises a polymer of intrinsic microporosity (PIM).

### Claim 6 (depends on 1)

The electrode of claim 1, wherein the porous polymer comprises a copolymer of any one of monomers A1 to A18 below and any one of monomers B1 to B19 below:
wherein Ha comprises one or more of F, Cl, Br, and I.

### Claim 7 (depends on 1)

The electrode of claim 1, wherein the porous polymer is represented by Chemical Formula 1 below:
wherein X comprises one or more of
and
n is an integer from 1 to 10.

### Claim 8 (depends on 1)

The electrode of claim 1, wherein the coating layer comprises a porous polymer having a number average molecular weight (Mn) of about 5,000 to 100,000.

### Claim 9 (depends on 1)

The electrode of claim 1, wherein a weight ratio of the catalyst complex to the porous polymer in the coating layer is about 100:3 to 100:20.

### Claim 10 (depends on 1)

The electrode of claim 1, wherein a thickness of the coating layer is about 0.1 nm to 5 nm.

### Claim 11 (depends on 1)

A membrane-electrode assembly comprising:
an electrolyte membrane;
a cathode formed on one side of the electrolyte membrane; and
an anode formed on the other side of the electrolyte membrane,
wherein at least one of the cathode and the anode comprises the electrode of claim 1.

### Claim 12

A method of manufacturing an electrode for a fuel cell, the method comprising:
preparing a catalyst complex comprising a support, a catalytic metal and a porous polymer;
manufacturing an electrode catalyst with a core-shell structure by coating at least a portion of a surface of the catalytic metal with the porous polymer;
preparing a slurry by combining the electrode catalyst with an electrode binder; and
forming an electrode by applying the slurry onto a substrate.

### Claim 13 (depends on 12)

The method of claim 12, wherein manufacturing the electrode catalyst comprises:
adding the catalyst complex and the porous polymer to a solvent followed by mixing;
precipitating and recovering the electrode catalyst by pouring an aqueous solvent into a mixture; and
drying the recovered electrode catalyst.

### Claim 14 (depends on 12)

The method of claim 12, wherein the catalytic metal comprises one or more of platinum, palladium, cobalt, gold, ruthenium, tin, molybdenum, rhodium, iridium, bismuth, copper, yttrium, and chromium, and combinations thereof.

### Claim 15 (depends on 12)

The method of claim 12, wherein the porous polymer comprises a polymer of intrinsic microporosity (PIM).

### Claim 16 (depends on 12)

The method of claim 12, wherein the porous polymer comprises a copolymer of at least one of monomers A1 to A18 below and at least one of monomers B1 to B19 below:
wherein Ha comprises one or more of F, Cl, Br, and I.

### Claim 17 (depends on 12)

The method of claim 12, wherein the porous polymer is represented by Chemical Formula 1 below:
wherein X comprises one or more of
and
n is an integer from 1 to 10.

### Claim 18 (depends on 12)

The method of claim 12, wherein the coating layer comprises a porous polymer having a number average molecular weight (Mn) of about 5,000 to 100,000.

### Claim 19 (depends on 12)

The method of claim 12, wherein a weight ratio of the catalyst complex to the porous polymer is about 100:3 to 100:20.

### Claim 20 (depends on 12)