# US 2026/0094838 A1 · Aqueous zinc-based battery with a high hardness heterostructure material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0094838 A1
- Document ID: US20260094838A1
- Status: Published application
- Kind: A1
- Application number: 18/901,139
- Filed: 2024-09-30
- Published: 2026-04-02
- Earliest claimed: 2024-09-30
- Assignees: City University of Hong Kong
- Applicants: City University of Hong Kong
- Inventors: Jian LU; Yuhan CHEN; Jianan YIN
- Web page: https://patentgrep.com/patent/US20260094838A1

## CPC

- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/42: Alloys based on zinc
- H01M 10/36: Accumulators not provided for in groups H01M10/05-H01M10/34
- H01M 10/365: {Zinc-halogen accumulators}
- H01M 4/483: {for non-aqueous cells (H01M4/485 takes precedence)}
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0002: Aqueous electrolytes
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

This invention relates to the strategy of synergizing mechanical and chemical regulations to prohibit dendrite growth on metal electrode surfaces. High-hardness materials are selected and modified to present amorphous-crystalline heterostructures. Enhanced interactions between metal ions and modified metal electrodes contribute to uniform nucleation. High hardness mechanically blocks dendrite growth. As such, the present invention further relates to an amorphous-crystalline heterostructural diamond coating modified Zn electrode and a full cell.

## Claims

### Claim 1

An aqueous zinc-based battery with a high hardness heterostructure material, comprising:
a reversible and dendrite-free anode comprising an anode material and a barrier layer with a hardness of at least 60 GPa coated on the anode material, wherein the barrier layer is made from a local graphitization material having a nanoscale three-dimensional amorphous-crystalline heterostructure;
a cathode comprising a cathode material;
a separator between the reversible and dendrite-free anode and the cathode; and
an electrolyte comprising an aqueous solution that is in ionic contact with both the reversible and dendrite-free anode and the cathode through the separator,
wherein an amorphous carbon domain is embedded in a crystalline matrix of the local graphitization material, and
wherein the barrier layer reduces a desolvation energy barrier for Zn2+ ions.

### Claim 2 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the barrier layer exhibits hydrophobicity to prevent water-mediated side reactions at the reversible and dendrite-free anode surface.

### Claim 3 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the local graphitization material comprises diamond-derived materials, activated carbon, carbide, boride, nitride, or a combination thereof.

### Claim 4 (depends on 3)

The aqueous zinc-based battery of claim 3, wherein the local graphitization material is nano dual-phase diamond particles fabricated via a thermal treatment.

### Claim 5 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the anode material comprises zinc foil, zinc powder, zinc plate, or zinc alloy.

### Claim 6 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the cathode material comprises MnO2, ZnMn2O4, V2O5, NH4V4O10, or a combination thereof.

### Claim 7 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the separator comprises glass fiber, polymer membranes comprising polyacrylonitrile, Nafion, polyvinyl alcohol, or cellulose-based materials comprising lignocellulose, g-C3N4 modified cellulose, cotton cellulose.

### Claim 8 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the electrolyte comprises ZnSO4, Zn(CF3SO3)2, Zn(CH3COO)2, ZnCl2, KOH solutions, or a combination thereof.

### Claim 9 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the nanoscale three-dimensional amorphous-crystalline heterostructure is characterized by a broad peak of amorphous structure centered at approximately 2θ equal to 26°.

### Claim 10 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the reversible and dendrite-free anode is configured to exhibit reduced hydrogen evolution reaction and enhanced anti-corrosion performance compared to a bare zinc anode.

### Claim 11 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the local graphitization material has an irregular flake morphology with an average size of approximately 200 nm.

### Claim 12 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the aqueous zinc-based battery exhibits a cycling stability of at least 3000 hours at a current density of 5 mA/cm2 with a capacity of 1 mAh/cm2.

### Claim 13 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the aqueous zinc-based battery maintains a nucleation overpotential of less than 90 mV during cycling.

### Claim 14 (depends on 1)

The aqueous zinc-based battery of claim 1, wherein the aqueous zinc-based battery exhibits a cumulative plating capacity of at least 8000 mAh/cm2 during long-term cycling.

### Claim 15

A method of fabricating a barrier layer with a hardness of at least 60 GPa for use in a reversible and dendrite-free anode, comprising:
mixing one or more synthetic nano diamond particles with an acrylic acid ammonium salt polymer, a monomer, a cross-linking agent, a photoinitiator, and water to form a slurry;
drying the slurry at a temperature of approximately 80° C. for 1-4 hours;
sintering the dried slurry in an argon atmosphere at a temperature ranging from 900° C. to 2000° C. at a ramp rate of 5° C. per minute to obtain a local graphitization material, wherein the local graphitization material is formed with a nanoscale three-dimensional amorphous-crystalline heterostructure; and
spin-coating the local graphitization material onto an anode material to form the barrier layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the sintering process is conducted for a duration of approximately 30 hours.

### Claim 17 (depends on 15)

The method of claim 15, further comprising a cooling step following the sintering process to gradually reduce the temperature of the local graphitization material.

### Claim 18 (depends on 15)

The method of claim 15, wherein the photoinitiator comprises 2-hydroxy-2-methylpropiophenone and diphenyl(2,4,6-trimethylbenzoyl)phosphine oxide, the monomer comprises acrylamide or acrylic acid, and the cross-linking agent comprises N,N′-methylenebisacrylamide or hexamethylene diisocyanate.

### Claim 19 (depends on 15)

The method of claim 15, wherein the slurry comprises
50-70 wt % of one or more synthetic nano diamond particles;
1-5 wt % of acrylic acid ammonium salt polymer;
1-5 wt % of monomer;
1-5 wt % of cross-linking agent;
0.1-5 wt % of photoinitiator;
1-10 wt % of water.