# US 2026/0094829 A1 · Negative electrode of secondary battery, method for manufacturing the negative electrode, and secondary battery using the negative electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0094829 A1
- Document ID: US20260094829A1
- Status: Published application
- Kind: A1
- Application number: 19/337,267
- Filed: 2025-09-23
- Published: 2026-04-02
- Earliest claimed: 2024-09-27
- Assignees: Prime Planet Energy & Solutions, Inc.
- Applicants: Prime Planet Energy & Solutions, Inc.
- Inventors: Naoto ONODERA
- Web page: https://patentgrep.com/patent/US20260094829A1

## CPC

- H01M 4/587: for inserting or intercalating light metals
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/364: {as mixtures}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The negative electrode of a secondary battery of the present disclosure includes a negative electrode current collector, and a negative electrode active material layer supported by the negative electrode current collector. The negative electrode active material layer contains graphite particles, first Si-containing particles, and second Si-containing particles. The content rate of Si in the first Si-containing particles is smaller than the content rate of Si in the second Si-containing particles. When a density of a molded body obtained by uniaxially pressurizing and molding 1 g of particles at 25° C. and at 60 MPa into a tablet having a diameter of 20 mm is defined as a consolidation density, the consolidation density of the first Si-containing particles is 0.9 g/cm3 or more, and the consolidation density of the second Si-containing particles is less than 0.9 g/cm3

## Claims

### Claim 1

A negative electrode of a secondary battery, comprising:
a negative electrode current collector; and
a negative electrode active material layer supported by the negative electrode current collector; wherein
the negative electrode active material layer contains graphite particles, first Si-containing particles, and second Si-containing particles,
a content rate of Si in the first Si-containing particles is smaller than a content rate of Si in the second Si-containing particles, and
a consolidation density of the first Si-containing particles is 0.9 g/cm3 or more and a consolidation density of the second Si-containing particles is less than 0.9 g/cm3 when a density of a molded body obtained by uniaxially pressurizing and molding 1 g of particles at 25° C. and at 60 MPa into a tablet having a diameter of 20 mm is defined as a consolidation density.

### Claim 2 (depends on 1)

The negative electrode according to claim 1, wherein the consolidation density of the first Si-containing particles is 0.95 g/cm3 or more and 1.8 g/cm3 or less.

### Claim 3 (depends on 1)

The negative electrode according to claim 1, wherein the consolidation density of the second Si-containing particles is 0.65 g/cm3 or more and 0.85 g/cm3 or less.

### Claim 4 (depends on 1)

The negative electrode according to claim 1, wherein a mass ratio between the first Si-containing particles and the second Si-containing particles is 20:80 to 80:20.

### Claim 5 (depends on 1)

The negative electrode according to claim 1, wherein a ratio of the content rate of Si in the first Si-containing particles with respect to the content rate of Si in the second Si-containing particles is 0.10 to 0.90.

### Claim 6 (depends on 1)

The negative electrode according to claim 1, wherein the content rate of Si in the first Si-containing particles is 20% by mass to 55% by mass, and the content rate of Si in the second Si-containing particles is 45% by mass to 80% by mass.

### Claim 7 (depends on 1)

The negative electrode according to claim 1, wherein a content rate of the graphite particles with respect to a total of the graphite particles, the first Si-containing particles, and the second Si-containing particles is 40% by mass to 90% by mass.

### Claim 8 (depends on 1)

The negative electrode according to claim 1, wherein
a ratio of an average particle diameter (D50) of the graphite particles with respect to an average particle diameter (D50) of the first Si-containing particles is 1.0 to 8.0, and
a ratio of an average particle diameter (D50) of the graphite particles with respect to an average particle diameter (D50) of the second Si-containing particles is 1.0 to 8.0.

### Claim 9

A method for producing a negative electrode of a secondary battery, the method comprising steps of:
preparing a negative electrode paste containing graphite particles, first Si-containing particles, second Si-containing particles, and a dispersion medium;
applying the negative electrode paste to a negative electrode current collector;
drying the applied negative electrode paste to form a negative electrode active material layer; and
pressing the negative electrode active material layer, wherein
a content rate of Si in the first Si-containing particles is smaller than a content rate of Si in the second Si-containing particles,
a consolidation density of the first Si-containing particles is 0.9 g/cm3 or more and a consolidation density of the second Si-containing particles is less than 0.9 g/cm3 when a density of a molded body obtained by uniaxially pressurizing and molding 1 g of particles at 25° C. and at 60 MPa into a tablet having a diameter of 20 mm is defined as a consolidation density of particles.

### Claim 10 (depends on 1)

A secondary battery comprising
a positive electrode;
a negative electrode; and
an electrolyte,
wherein the negative electrode is the negative electrode according to claim 1.