# US 2026/0094816 A1 · Negative electrode of secondary battery, manufacturing method of negative electrode, and secondary battery with negative electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0094816 A1
- Document ID: US20260094816A1
- Status: Published application
- Kind: A1
- Application number: 19/337,196
- Filed: 2025-09-23
- Published: 2026-04-02
- Earliest claimed: 2024-09-27
- Assignees: Prime Planet Energy & Solutions, Inc.
- Applicants: Prime Planet Energy & Solutions, Inc.
- Inventors: SURIM KANG
- Web page: https://patentgrep.com/patent/US20260094816A1

## CPC

- H01M 4/366: {as layered products}
- C01B 32/05: Preparation or purification of carbon not covered by groups C01B32/15, C01B32/20, C01B32/25, C01B32/30
- C01B 33/02: Silicon (forming single crystals or homogeneous polycrystalline material with defined structure C30B)
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/364: {as mixtures}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/582: {Halogenides}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/625: {Carbon or graphite}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is a technique to suppress a swell of the negative electrode. In the negative electrode disclosed herein, a negative electrode active material layer includes a first layer at a negative electrode current collector side and a second layer at a surface layer side. The first layer contains first Si-containing particles. The second layer contains second Si-containing particles. A Si content rate of the second Si-containing particles is smaller than a Si content rate of the first Si-containing particles. Each of the first Si-containing particles and the second Si-containing particles include a LiF coating layer. A second peak intensity ratio relating to a LiF of the second Si-containing particles is smaller than a first peak intensity ratio relating to the LiF of the first Si-containing particles. A difference between the first peak intensity ratio and the second peak intensity ratio is 0.050 to 1.00.

## Claims

### Claim 1

A negative electrode of a secondary battery, comprising:
a negative electrode current collector; and
a negative electrode active material layer that is supported by the negative electrode current collector, wherein
the negative electrode active material layer comprises a first layer positioned at a side of the negative electrode current collector and a second layer positioned at a surface layer side,
the first layer comprises first Si-containing particles as a negative electrode active material,
the second layer comprises second Si-containing particles as the negative electrode active material,
a Si content rate of the second Si-containing particles is smaller than a Si content rate of the first Si-containing particles,
each of the first Si-containing particles and the second Si-containing particles comprise a LiF coating layer, and
when, on an XPS spectrum of the first Si-containing particles measured by a X-ray photoelectron spectroscopy, a ratio of a peak intensity of an F of a LiF with respect to the peak intensity of the F of one being other than the LiF is defined as a first peak intensity ratio, and on an XPS spectrum of the second Si-containing particles, the ratio of the peak intensity of the F of the LiF with respect to the peak intensity of the F of one being other than the LiF is defined as a second peak intensity ratio, the second peak intensity ratio is smaller than the first peak intensity ratio, and a difference between the first peak intensity ratio and the second peak intensity ratio is equal to or more than 0.050 and not more than 1.00.

### Claim 2 (depends on 1)

The negative electrode according to claim 1, wherein
the Si content rate of the second Si-containing particles with respect to the Si content rate of the first Si-containing particles is equal to or more than 0.3 and not more than 0.9.

### Claim 3 (depends on 1)

The negative electrode according to claim 1, wherein
the Si content rate of the first Si-containing particles is equal to or more than 30 mass % and not more than 80 mass %, and
the Si content rate of the second Si-containing particles is equal to or more than 20 mass % and not more than 70 mass %.

### Claim 4 (depends on 1)

The negative electrode according to claim 1, wherein
the first peak intensity ratio is equal to or more than 0.450 and not more than 1.00.

### Claim 5 (depends on 1)

The negative electrode according to claim 1, wherein
the second peak intensity ratio is equal to or more than 0.200 and less than 0.450.

### Claim 6 (depends on 1)

The negative electrode according to claim 1, wherein
the first Si-containing particles and the second Si-containing particles comprise Si—C composite particles comprising a carbon base material and comprising Si contained at inside of the carbon base material and comprise the LiF coating layer arranged at least on a part of a surface of the Si—C composite particles.

### Claim 7 (depends on 1)

The negative electrode according to claim 1, wherein
the first layer and the second layer further comprise graphite particles, as the negative electrode active material, that substantially do not comprise a Si.

### Claim 8

A manufacturing method of a negative electrode of a secondary battery, comprising:
preparing a first paste that comprises first Si-containing particles as a negative electrode active material and comprises a dispersion medium;
preparing a second paste that comprises second Si-containing particles as the negative electrode active material and comprises the dispersion medium;
applying the first paste to coat a negative electrode current collector and to dry so as to form a dry layer of the first paste;
applying the second paste to coat the dry layer of the first paste and to dry so as to form a dry layer of the second paste; and
pressing the dry layer of the first paste and the dry layer of the second paste, wherein
a Si content rate of the second Si-containing particles is smaller than a Si content rate of the first Si-containing particles,
each of the first Si-containing particles and the second Si-containing particles comprises a LiF coating layer, and
when, on an XPS spectrum of the first Si-containing particles measured by a X-ray photoelectron spectroscopy, a ratio of a peak intensity of an F of a LiF with respect to the peak intensity of the F of one being other than the LiF is defined as a first peak intensity ratio, and on an XPS spectrum of the second Si-containing particles, the ratio of the peak intensity of the F of the LiF with respect to the peak intensity of the F of one being other than the LiF is defined as a second peak intensity ratio, the second peak intensity ratio is smaller than the first peak intensity ratio, and a difference between the first peak intensity ratio and the second peak intensity ratio is equal to or more than 0.050 and not more than 1.00.

### Claim 9 (depends on 8)

The manufacturing method according to claim 8, wherein
the preparing the first paste comprises preparing the first Si-containing particles,
the preparing the second paste comprises preparing the second Si-containing particles,
at the preparing the first Si-containing particles and the preparing the second Si-containing particles,
Si—C composite particles, comprising a carbon base material and comprising Si comprised at inside of the carbon base material, is prepared, and
by making the Si—C composite particles react with a water-soluble lithium salt and a fluorinated agent in a state where the Si—C composite particles is dispersed into a water or a water-soluble organic solvent so as to generate a LiF, the first Si-containing particles and the second Si-containing particles are prepared.

### Claim 10 (depends on 1)

A secondary battery, comprising:
a positive electrode;
a negative electrode; and
an electrolyte, wherein
the negative electrode is the negative electrode according to claim 1.