# US 2026/0094743 A1 · NdFeB MAGNET

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0094743 A1
- Document ID: US20260094743A1
- Status: Published application
- Kind: A1
- Application number: 19/295,983
- Filed: 2025-08-11
- Published: 2026-04-02
- Earliest claimed: 2024-09-29
- Assignees: Ningbo Konit Industries Inc.; Ningbo Konit HEFENG NEW Material Co.,Ltd.; Ningbo Konit Xinfeng Precision Manufacturing Co., Ltd; Ningbo Konit & Nihon Magnetic Material Inc.; Beijing Zhong Ke San Huan Hi-Tech Co., Ltd.
- Applicants: Ningbo Konit Industries Inc.; Ningbo Konit HEFENG NEW Material Co.,Ltd.; Ningbo Konit Xinfeng Precision Manufacturing Co., Ltd.; Ningbo Konit & Nihon Magnetic Material Inc.; Beijing Zhong Ke San Huan Hi-Tech Co., Ltd.
- Inventors: Chao CHEN; Lijun DING; Chenghong GU; Wei ZHU; E NIU; Die HU
- Web page: https://patentgrep.com/patent/US20260094743A1

## CPC

- H01F 1/0577: {sintered}
- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- C22C 33/02: by powder metallurgy
- C22C 33/0278: {with at least one alloying element having a minimum content above 5%}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/06: containing aluminium
- C22C 38/10: containing cobalt
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- H01F 41/0266: {Moulding; Pressing (H01F41/0273 takes precedence; hard magnetic particles H01F1/06, H01F1/11)}
- H01F 41/0293: {diffusion of rare earth elements, e.g. Tb, Dy or Ho, into permanent magnets}
- B22F 2003/248: {Thermal after-treatment}
- C22C 2202/02: Magnetic
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A NdFeB magnet includes main phase grains, thin-layer grain boundary phases, and triangular region grain boundary phases. The distribution of the triangular region grain boundary phase within the NdFeB magnet satisfies 0.057≤S1/S≤0.073. The NdFeB magnet includes R, M, M1, Co, B, and T. R represents one or more selected from Nd, Pr, Ho, Ce, Gd, Dy, and Tb. M represents one or more selected from Al, Cu, and Ga. M1 represents one or more selected from Ti, Zr, Nb, W, and V. T is selected from Fe and other impurity elements. The content of R in the NdFeB magnet is in a range of 28 to 32 wt %, and the content of M1 is in a range of 0.4 to 1.0 wt %. The triangular grain boundary phase includes the R-T-M-Co phase. The content of Co in the R-T-M-Co phase is in a range of 6.2 to 10.4 at %.

## Claims

### Claim 1

A NdFeB magnet comprising main phase grains, thin-layer grain boundary phases, and triangular region grain boundary phases;
wherein:
a distribution of the triangular region grain boundary phases within the NdFeB magnet satisfies 0.057≤S1/S≤0.073, where S1 represents an area of all of the triangular region grain boundary phases in a cross-section of the NdFeB magnet, and S represents a total area of the cross-section;
the NdFeB magnet includes R, M, M1, Co, B, and T, where:
R represents one or more selected from Nd, Pr, Ho, Ce, Gd, Dy, and Tb;
M represents one or more selected from Al, Cu, and Ga;
M1 represents one or more selected from Ti, Zr, Nb, W, and V;
T represents one or more selected from Fe and other impurity elements; and
a content of R in the NdFeB magnet is in a range of 28 to 32 wt %, and a content of M1 in the NdFeB magnet is in a range of 0.4 to 1.0 wt %; and
the triangular grain boundary phases include R-T-M-Co phases, and a content of Co in the R-T-M-Co phases is in a range of 6.2 to 10.4 at %.

### Claim 2 (depends on 1)

The NdFeB magnet according to claim 1, wherein in the NdFeB magnet, a content of M1 is in a range of 0.4 to 1 wt %, a content of Co is in a range of 0.4 to 2 wt %, a content of Cu is in a range of 0.1 to 0.25 wt %, a content of Ga is in a range of 0.1 to 0.25 wt %, a content of Al is in a range of 0.05 to 1.2 wt %, a content of B is in a range of 0.85 to 1.05 wt %, with the remainder being Fe and other impurity elements.

### Claim 3 (depends on 1)

The NdFeB magnet according to claim 1, wherein R does not contain Ce and Gd.

### Claim 4 (depends on 1)

The NdFeB magnet according to claim 1, wherein a content of Ti in M1 is in a range of 0 to 0.4 wt %, and a content of Zr is in a range of 0.25 to 0.7 wt %.

### Claim 5 (depends on 1)

The NdFeB magnet according to claim 1, wherein M1 includes at least one of Ti or Zr.

### Claim 6 (depends on 1)

The NdFeB magnet according to claim 1, wherein a content of R in the R-T-M-Co phases is in a range of 38 to 90 at %.

### Claim 7 (depends on 1)

The NdFeB magnet according to claim 1, wherein:
a content of Cu in the R-T-M-Co phases is in a range of 4 to 9.7 at %; and
a content of Ga in the R-T-M-Co phases is in a range of 2.9 to 6 at %.

### Claim 8 (depends on 1)

The NdFeB magnet according to claim 1, wherein a distribution of the R-T-M-Co phases within the triangular region grain boundary satisfies 0.162≤S2/S1≤0.18, where S2 represents an area of all of the R-T-M-Co phases within the triangular region grain boundary phases in the cross-section of the NdFeB magnet.

### Claim 9 (depends on 1)

The NdFeB magnet according to claim 1, wherein:
the triangular grain boundary phases further include R6T13M1 phases; and
a distribution of the R6T13M1 phases within the triangular grain boundary phases satisfies 0.8≤S3/S1≤0.815, where S3 represents an area of all of the R6T13M1 phases in the cross-section of the NdFeB magnet.

### Claim 10 (depends on 1)

The NdFeB magnet according to claim 1, wherein:
a roundness of the main phase grains is in a range of 0.6 to 0.9; and
an average grain size of the main phase grains is in a range of 3.5 to 4.5 μm.

### Claim 11 (depends on 1)

A method for preparing the NdFeB magnet according to claim 1, comprising:
forming raw alloy powder into a compact; and
performing sintering process and aging process on the compact;
wherein
the aging process includes:
a first aging treatment performed at a temperature in a range of 870 to 940° C. with a holding time of 0.5 to 4 h;
a second aging treatment performed at a temperature in a range of 420 to 670° C. with a holding time of 1 to 10 h; and
a third aging treatment performed at a temperature in a range of 620 to 670° C. with a holding time of 1 to 10 h; and
the raw alloy powder includes R, M, M1, Co, B, and T.

### Claim 12 (depends on 11)

The method according to claim 11, wherein:
the temperature for the second aging treatment is in a range of 450 to 660° C.; and
the temperature for the third aging treatment is in a range of 630 to 670° C.

### Claim 13 (depends on 11)

The method according to claim 11, wherein in the raw alloy powder:
a content of R is in a range of 28 to 32 wt %;
a content of M1 is in a range of 0.4 to 1.0 wt %;
a content of Co is in a range of 0.4 to 2 wt %;
a content of Cu is in a range of 0.1 to 0.25 wt %;
a content of Ga is in a range of 0.1 to 0.25 wt %;
a content of Al is in a range of 0.05 to 1.2 wt %;
a content of B is in a range of 0.85 to 1.05 wt %; and
the remainder includes Fe and other impurity elements.

### Claim 14 (depends on 11)

The method according to claim 11, wherein R does not contain Ce and Gd.