- Number: US 2026/0093177 A1
- Document ID: US20260093177A1
- Status: Published application
- Kind: A1
- Application number: 19/338,782
- Filed: 2025-09-24
- Published: 2026-04-02
- Earliest claimed: 2024-10-02
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Applicants: Shin-Etsu Chemical Co., Ltd.
- Inventors: Hidenori YAMAGUCHI; Yuki SUDA; Kazunori MAEDA; Seiichiro TACHIBANA
- Web page: https://patentgrep.com/patent/US20260093177A1

## CPC

- G03F 7/0392: {the macromolecular compound being present in a chemically amplified positive photoresist composition}
- G03F 7/0397: {the macromolecular compound having an alicyclic moiety in a side chain}
- G03F 7/094: {Multilayer resist systems, e.g. planarising layers}
- G03F 7/11: having cover layers or intermediate layers, e.g. subbing layers {(G03F7/091 - G03F7/093, B41N3/03 take precedence)}
- G03F 7/40: Treatment after imagewise removal, e.g. baking
- G03F 7/70025: {by lasers}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A patterning process including: forming a multilayer on a substrate for processing; forming a resist upper layer film using a positive chemically-amplified resist composition for ArF excimer; removing the acid-labile group in an exposed portion of the resist upper layer film by exposure and post-exposure bake; performing a higher temperature hard bake for a shorter time than post-exposure bake allowing the removed acid-labile group to volatilize out of the resist upper layer film and a number difference of carbon atoms between an unexposed and exposed portion; removing the resist upper layer film in the exposed portion with a gas plasma containing oxygen by dry development pattern separation; and transferring the resist upper layer film pattern to the multilayer underneath by etching. The patterning process obtains a fine pattern having a narrow pitch by dry development using a (meth)acrylic polymer usable for ArF patterning as the main skeleton and without silylation.

## Claims

### Claim 1

A patterning process comprising the steps of:
forming a multilayer on a substrate to be processed;
forming a resist upper layer film by using a positive chemically-amplified resist composition for ArF excimer containing, at least, a base polymer having a (meth)acrylic structure substituted with an acid-labile group, a photo-acid generator, a quencher having a function of controlling acid diffusion, and an organic solvent;
removing the acid-labile group in an exposed portion of the resist upper layer film by exposure and a post-exposure bake;
performing a hard bake at a higher temperature and for a shorter time than the post-exposure bake to allow the removed acid-labile group to volatilize out of the resist upper layer film and cause a difference in a number of carbon atoms between an unexposed portion and the exposed portion;
removing the resist upper layer film in the exposed portion with a gas plasma containing oxygen by dry development to separate a pattern; and
transferring the pattern of the resist upper layer film to the multilayer underneath by etching.

### Claim 2 (depends on 1)

The patterning process according to claim 1, wherein the base polymer has a (meth)acrylic structure in which a rate of substitution with the acid-labile group is 80% to 100% and the acid-labile group has 4 to 9 carbon atoms.

### Claim 3 (depends on 1)

The patterning process according to claim 1, wherein the base polymer does not have a lactone structure.

### Claim 4 (depends on 2)

The patterning process according to claim 2, wherein the base polymer does not have a lactone structure.

### Claim 5 (depends on 1)

The patterning process according to claim 1, wherein the post-exposure bake is performed at 80° C. to 120° C. for 40 seconds to 120 seconds, and the hard bake is performed at 130° C. or higher for less than 40 seconds.

### Claim 6 (depends on 2)

The patterning process according to claim 2, wherein the post-exposure bake is performed at 80° C. to 120° C. for 40 seconds to 120 seconds, and the hard bake is performed at 130° C. or higher for less than 40 seconds.

### Claim 7 (depends on 3)

The patterning process according to claim 3, wherein the post-exposure bake is performed at 80° C. to 120° C. for 40 seconds to 120 seconds, and the hard bake is performed at 130° C. or higher for less than 40 seconds.

### Claim 8 (depends on 4)

The patterning process according to claim 4, wherein the post-exposure bake is performed at 80° C. to 120° C. for 40 seconds to 120 seconds, and the hard bake is performed at 130° C. or higher for less than 40 seconds.

### Claim 9 (depends on 1)

The patterning process according to claim 1, wherein the resist composition further contains a surfactant that functions as a top coat for ArF immersion exposure, or the patterning process further comprises a step of applying and forming a top coat before the exposure.

### Claim 10 (depends on 2)

The patterning process according to claim 2, wherein the resist composition further contains a surfactant that functions as a top coat for ArF immersion exposure, or the patterning process further comprises a step of applying and forming a top coat before the exposure.

### Claim 11 (depends on 3)

The patterning process according to claim 3, wherein the resist composition further contains a surfactant that functions as a top coat for ArF immersion exposure, or the patterning process further comprises a step of applying and forming a top coat before the exposure.

### Claim 12 (depends on 4)

The patterning process according to claim 4, wherein the resist composition further contains a surfactant that functions as a top coat for ArF immersion exposure, or the patterning process further comprises a step of applying and forming a top coat before the exposure.

### Claim 13 (depends on 5)

The patterning process according to claim 5, wherein the resist composition further contains a surfactant that functions as a top coat for ArF immersion exposure, or the patterning process further comprises a step of applying and forming a top coat before the exposure.

### Claim 14 (depends on 6)

The patterning process according to claim 6, wherein the resist composition further contains a surfactant that functions as a top coat for ArF immersion exposure, or the patterning process further comprises a step of applying and forming a top coat before the exposure.

### Claim 15 (depends on 7)

The patterning process according to claim 7, wherein the resist composition further contains a surfactant that functions as a top coat for ArF immersion exposure, or the patterning process further comprises a step of applying and forming a top coat before the exposure.

### Claim 16 (depends on 8)

The patterning process according to claim 8, wherein the resist composition further contains a surfactant that functions as a top coat for ArF immersion exposure, or the patterning process further comprises a step of applying and forming a top coat before the exposure.