# US 2026/0092400 A1 · SiC CRYSTAL AND METHOD FOR MANUFACTURING SiC CRYSTAL

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0092400 A1
- Document ID: US20260092400A1
- Status: Published application
- Kind: A1
- Application number: 19/344,905
- Filed: 2025-09-30
- Published: 2026-04-02
- Earliest claimed: 2024-09-30
- Assignees: Resonac Corporation
- Applicants: Resonac Corporation
- Inventors: Shota OTOGAWA
- Web page: https://patentgrep.com/patent/US20260092400A1

## CPC

- C30B 29/36: Carbides
- C30B 33/00: After-treatment of single crystals or homogeneous polycrystalline material with defined structure (C30B31/00 takes precedence)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A SiC crystal according to the present embodiment has a first surface which is one surface in a stacking direction, wherein in a case where a waviness curve of the first surface is measured along a first measurement line that passes through a center of the first surface and extends in a <1-100> direction, a lowest point of the waviness curve on the first measurement line is dislocated from the center.

## Claims

### Claim 1

A SiC crystal comprising a first surface which is one surface in a stacking direction,
wherein in a case where a waviness curve of the first surface is measured along a first measurement line that passes through a center of the first surface and extends in a <1-100> direction, a lowest point of the waviness curve on the first measurement line is dislocated from the center.

### Claim 2 (depends on 1)

The SiC crystal according to claim 1, wherein in a case where a waviness curve of the first surface is measured along a second measurement line that passes through a center of the first surface and extends in an <11-20> direction, a lowest point of the waviness curve on the second measurement line is dislocated from the center.

### Claim 3 (depends on 1)

The SiC crystal according to claim 1, wherein a surface roughness Ra of the first surface which is measured along the first measurement line is 20 nm or less.

### Claim 4 (depends on 1)

The SiC crystal according to claim 1, wherein a surface roughness Ra of the first surface which is measured along a second measurement line that passes through a center of the first surface and extends in an <11-20> direction is 30 nm or less.

### Claim 5 (depends on 1)

The SiC crystal according to claim 1,
wherein the first surface has abrasive grain trajectories, and
wherein an intersection point at which the abrasive grain trajectories overlap with each other most is dislocated from the center.

### Claim 6 (depends on 1)

The SiC crystal according to claim 1, wherein a difference between a highest point and a lowest point of the waviness curve on the first measurement line is 3.5 μm or less.

### Claim 7 (depends on 2)

The SiC crystal according to claim 2, wherein a difference between a highest point and a lowest point of the waviness curve on the second measurement line is 3.5 μm or less.

### Claim 8

A SiC crystal comprising a first surface which is one surface in a stacking direction,
wherein in a case where a waviness curve of the first surface is measured along a first measurement line that passes through a center of the first surface and extends in a <1-100> direction, a difference between a highest point and a lowest point of the waviness curve on the first measurement line is 3.5 μm or less.

### Claim 9 (depends on 8)

The SiC crystal according to claim 8, wherein in a case where a waviness curve of the first surface is measured along a second measurement line that passes through a center of the first surface and extends in an <11-20> direction, a difference between a highest point and a lowest point of the waviness curve on the second measurement line is 3.5 μm or less.

### Claim 10 (depends on 8)

The SiC crystal according to claim 8, wherein a surface roughness Ra of the first surface which is measured along the first measurement line is 20 nm or less.

### Claim 11 (depends on 8)

The SiC crystal according to claim 8, wherein a surface roughness Ra of the first surface which is measured along a second measurement line that passes through a center of the first surface and extends in an <11-20> direction is 30 nm or less.

### Claim 12 (depends on 8)

The SiC crystal according to claim 8,
wherein the first surface has abrasive grain trajectories, and
wherein an intersection point at which the abrasive grain trajectories overlap with each other most is dislocated from the center.

### Claim 13 (depends on 8)

The SiC crystal according to claim 8, wherein the lowest point of the waviness curve on the first measurement line is dislocated from the center.

### Claim 14 (depends on 9)

The SiC crystal according to claim 9, wherein the lowest point of the waviness curve on the second measurement line is dislocated from the center.

### Claim 15 (depends on 1)

The SiC crystal according to claim 1, wherein the SiC crystal has a diameter of 145 mm or greater.

### Claim 16

A method for manufacturing a SiC crystal, comprising:
a step of placing a workpiece made of a SiC crystal on a support table; and
a step of grinding a first surface of the workpiece by bringing the workpiece placed on the support table rotating in a first direction into contact with a grinding disk rotating in a second direction opposite to the first direction,
wherein the grinding disk is disposed at a position facing the support table such that a center of the grinding disk does not coincide with a center of the support table, and
wherein a center of the workpiece is dislocated from the center of the support table.

### Claim 17 (depends on 16)

The method for manufacturing a SiC crystal according to claim 16, wherein a distance between the center of the workpiece and the center of the support table is greater than or equal to a radius of the workpiece.

### Claim 18 (depends on 16)

The method for manufacturing a SiC crystal according to claim 16, wherein a distance between the center of the workpiece and the center of the support table is equal to a radius of the workpiece.

### Claim 19 (depends on 16)

The method for manufacturing a SiC crystal according to claim 16, wherein the workpiece has a diameter of 149 mm or greater.

### Claim 20 (depends on 16)

The method for manufacturing a SiC crystal according to claim 16,
wherein in a case where a distance between the center of the workpiece and the center of the support table is defined as x and a rotation speed of the support table is defined as n, a peripheral speed of the support table at a placement position of the workpiece is 2πxn, and
wherein in a case where a speed at which the grinding disk approaches the workpiece is defined as f, 2πxn/f, which is a ratio of a cutting speed to the peripheral speed, satisfies 2πxn/f ≤ 1.03×106.