# US 2026/0092398 A1 · SiC EPITAXIAL WAFER, METHOD FOR MANUFACTURING SiC EPITAXIAL WAFER, AND SiC DEVICE

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0092398 A1
- Document ID: US20260092398A1
- Status: Published application
- Kind: A1
- Application number: 19/340,965
- Filed: 2025-09-26
- Published: 2026-04-02
- Earliest claimed: 2024-09-30
- Assignees: Resonac Corporation
- Applicants: Resonac Corporation
- Inventors: Akira MIYASAKA
- Web page: https://patentgrep.com/patent/US20260092398A1

## CPC

- C30B 25/20: the substrate being of the same materials as the epitaxial layer
- C30B 25/165: {the flow of the reactive gases}
- C30B 29/36: Carbides
- H10D 62/8325: {Silicon carbide}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

What is provided is a SiC epitaxial wafer and a SiC device having a SiC epitaxial layer in which a carrier lifetime can be estimated and a variation in a density of a Z1/2 center in a depth direction is curbed. The SiC epitaxial wafer includes a substrate and a SiC epitaxial layer formed on a first surface of the substrate, wherein a uniformity of the density of the Z1/2 centers in the depth direction in the SiC epitaxial layer is less than 0.5 (%/μm).

## Claims

### Claim 1

A SiC epitaxial wafer comprising:
a SiC substrate; and
a SiC epitaxial layer formed on a first surface of the SiC substrate,
wherein a uniformity of a density of a Z1/2 center in a depth direction in the SiC epitaxial layer is less than 0.5 (%/μm).

### Claim 2 (depends on 1)

The SiC epitaxial wafer of claim 1, wherein a diameter is 149 mm or more.

### Claim 3 (depends on 1)

The SiC epitaxial wafer of claim 1, wherein a diameter is 199 mm or more.

### Claim 4 (depends on 1)

The SiC epitaxial wafer of claim 1, wherein, when central coordinates in a plan view are (0,0) and a radius is R, the density of the Z1/2 centers at 10 locations on a surface in the vicinity of an outermost surface in the depth direction and on a surface in the vicinity of the first surface at coordinates (0,0), (±R/2,0) and (0,±R/2) is 1×1011 cm−3 or more and 1.0×1013 cm−3 or less.

### Claim 5 (depends on 1)

The SiC epitaxial wafer of claim 1, wherein, when central coordinate in a plan view are (0,0) and a radius is R, a maximum value Max and a minimum value Min of the density of the Z1/2 centers at 10 locations on the surface in the vicinity of the outermost surface in the depth direction and on the surface in the vicinity of the first surface at coordinates (0, 0), (±R/2, 0), and (0, ±R/2) satisfy Equation (1):
[
{
(
Max
-
Min
)
/
mean
}
×
100
]
<
(
5
+
0.5
×
D
)
(
1
)
(D: distance (μm) between the surface in the vicinity of the outermost surface and the surface in the vicinity of the first surface,
mean: average value (cm−3) of the density of the Z1/2 centers at 10 locations).

### Claim 6

A method for manufacturing a SiC epitaxial wafer, comprising:
a formation step of forming a SiC epitaxial layer on a first surface of a SiC substrate by a chemical vapor deposition method using a growth apparatus having a gas supply port for supplying a Si-based gas and a C-based gas and a gas discharge port,
wherein the formation step includes an adjustment step of analyzing a gas discharged from the gas discharge port by quadrupole mass spectrometry, increasing an amount of supply of the C-based gas relative to the Si-based gas when an analyzed C/Si ratio is lower than a target value, and decreasing the amount of supply of the C-based gas relative to the Si-based gas when the analyzed C/Si ratio is higher than the target value.

### Claim 7 (depends on 6)

The method for manufacturing a SiC epitaxial wafer of claim 6, further comprising a test step, and a feedback step before the formation step,
wherein the test step includes:
a preliminary measurement step of measuring a weight and a surface area of a by-product in a growth apparatus;
a first formation step of forming a SiC epitaxial layer on a first surface of a test SiC substrate while analyzing a gas discharged from a gas discharge port by quadrupole mass spectrometry using the growth apparatus in which the preliminary measurement step has been performed;
an analysis step of analyzing a uniformity of a density of a Z1/2 center in a depth direction in the SiC epitaxial layer of the SiC epitaxial wafer formed in the first formation step; and
a measurement step of measuring the weight and the surface area of the by-product in the growth apparatus after the first forming step, and
the feedback step sets the target value based on a result of the test step.

### Claim 8 (depends on 7)

The method for manufacturing a SiC epitaxial wafer of claim 7, wherein the analysis step includes:
a film thickness measurement step of measuring a film thickness of a SiC epitaxial layer on a SiC epitaxial wafer having a center (0,0) in a plan view and a radius R;
a first evaluation step of evaluating the density of the Z1/2 centers at five locations of (0,0), (±R/2,0), and (0,±R/2) from an outermost surface of the SiC epitaxial wafer by a deep level transient spectroscopy (DLTS) method;
a removal step of removing a predetermined thickness of the SiC epitaxial layer; and
a second evaluation step of evaluating, after the removal step, the density of the Z1/2 centers at five positions of (0, 0), (±R/2, 0), and (0, ±R/2) from the outermost surface of the SiC epitaxial wafer by the DLTS method, and
the uniformity of the density of the Z1/2 centers in the depth direction, which is obtained by dividing a difference between the density of the Z1/2 centers in the first evaluation step and the density of the Z1/2 centers in the second evaluation step at the same location in a plan view by a predetermined thickness, is analyzed.

### Claim 9

A SiC device comprising:
a SiC substrate; and
a SiC epitaxial layer formed on a first surface of the SiC substrate, wherein a uniformity of a Z1/2 center density in a depth direction in the SiC epitaxial layer is less than 0.5 (%/μm).