# US 2026/0092364 A1 · Methods for depositing metal nitride layers on a substrate by cyclical deposition processes including cyclic compounds

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0092364 A1
- Document ID: US20260092364A1
- Status: Published application
- Kind: A1
- Application number: 19/343,820
- Filed: 2025-09-29
- Published: 2026-04-02
- Earliest claimed: 2024-09-30
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Mikko Leander Nisula; Charles Dezelah; Petro Deminskyi; Hoang Nguyen; Patricio Eduardo Romero; Emre Yarali; Giuseppe Alessio Verni; Jocelyn Kofi Brobbey; Serges Zambou; Ranjith Karuparambil Ramachandran; Aditya Chauhan; Andrea Illiberi; Alessandra Leonhardt
- Web page: https://patentgrep.com/patent/US20260092364A1

## CPC

- C23C 16/45527: {characterized by the ALD cycle, e.g. different flows or temperatures during half-reactions, unusual pulsing sequence, use of precursor mixtures or auxiliary reactants or activations}
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- C23C 16/45529: {specially adapted for making a layer stack of alternating different compositions or gradient compositions}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/46: characterised by the method used for heating the substrate (C23C16/48, C23C16/50 take precedence)
- H10P 14/412: {Deposition of metallic or metal-silicide materials}
- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10W 20/032: {of conductive barrier, adhesion or liner layers}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Methods of depositing metal nitride layers employing low temperature cyclical deposition processes including cyclic compounds are disclosed. The cyclical deposition processes include repeatedly performing a deposition cycle including introducing a metal precursor into a reaction chamber, introducing a nitrogen reactant into the reaction chamber, and introducing a reducing agent comprising a cyclic compound into the reaction chamber. Metal nitride layers and semiconductor structures including metal nitride layers are also disclosed.

## Claims

### Claim 1

A method for depositing a metal nitride layer on a substrate seated in a reaction chamber by a cyclical deposition process including one or more repeated deposition cycles, each deposition cycle comprising:
(a) initially introducing a metal precursor into the reaction chamber;
(b) introducing a nitrogen reactant into the reaction chamber; and
(c) introducing a reducing agent comprising a cyclic compound into the reaction chamber,
wherein step (c) is either performed after step (b) or step (c) is performed concurrently with step (b).

### Claim 2 (depends on 1)

The method of claim 1, wherein the cyclical deposition process is an atomic layer deposition process and each deposition cycle comprises:
(a) initially contacting the substrate with the metal precursor;
after step (a), (b) contacting the substrate with the nitrogen reactant; and
after step (b), (c) contacting the substrate with the cyclic compound.

### Claim 3 (depends on 1)

The method of claim 1, wherein the cyclical deposition process is an atomic layer deposition process and each deposition cycle comprises:
(a) initially contacting the substrate with the metal precursor; and
after step (a), (b)(c) concurrently contacting the substrate with the nitrogen reactant and the cyclic compound.

### Claim 4 (depends on 1)

The method of claim 1, wherein the cyclical deposition process is an atomic layer deposition process and each deposition cycle comprises a deposition super-cycle, each deposition super-cycle comprising:
performing one or more first sub-cycles comprising:
contacting the substrate with the metal precursor; and
contacting the substrate with the nitrogen reactant; and
performing one or more second sub-cycles comprising:
contacting the substrate with the cyclic compound.

### Claim 5 (depends on 1)

The method of claim 1, wherein the cyclic compound comprises a cyclic diene compound.

### Claim 6 (depends on 5)

The method of claim 5, wherein the cyclic diene compound is selected from 1,4-cyclohexadiene, 1,3-cyclohexadiene, and 1-methyl-1,4-cyclohexadiene.

### Claim 7 (depends on 1)

The method of claim 1, wherein the cyclic compound comprises a polycyclic hydrocarbon compound.

### Claim 8 (depends on 7)

The method of claim 7, wherein the polycyclic hydrocarbon compound is selected from 1,2,3,4-tetrahydronaphthalene and 9,10-Dihydroanthracene.

### Claim 9 (depends on 1)

The method of claim 1, wherein the metal precursor is selected from a titanium precursor, a molybdenum precursor, a hafnium precursor, and a niobium precursor.

### Claim 10 (depends on 1)

The method of claim 1, wherein the cyclical deposition process is performed at a deposition temperature between 350° C. and 500° C.

### Claim 11

A method for thermally depositing a metal nitride layer on a substrate, the method comprising:
heating the substrate to a deposition temperature between 350° C. and 500° C.; and
repeatedly performing a deposition cycle of an atomic layer deposition process, each deposition cycle comprising:
(a) initially contacting the substrate with a transition metal precursor;
after contacting the substrate the transition metal precursor, (b) contacting the substrate with a nitrogen reactant; and
after contacting the substrate with the nitrogen reactant, (c) contacting the substrate with a reducing agent comprising a cyclic diene compound selected from 1,4-cyclohexadiene, 1,3-cyclohexadiene, and 1-methyl-1,4-cyclohexadiene.

### Claim 12 (depends on 11)

The method of claim 11, wherein the transition metal precursor is selected from a titanium halide precursor, and a molybdenum halide precursor.

### Claim 13 (depends on 12)

The method of claim 12, wherein the molybdenum halide precursor comprises a molybdenum oxyhalide precursor.

### Claim 14

A method of forming a semiconductor structure, the method comprising:
seating a substrate within a reaction chamber, the substrate including a metal oxide layer;
heating the substrate to a deposition temperature between 350°C. and 500° C.; and
depositing a metal nitride layer over the metal oxide layer by repeatedly performing a deposition cycle of an atomic layer deposition process, each deposition cycle comprising:
(a) initially contacting the substrate with a metal precursor;
after contacting the substrate the metal precursor, (b) contacting the substrate with a nitrogen reactant; and
after contacting the substrate with the nitrogen reactant, (c) contacting the substrate with reducing agent comprising a cyclic diene compound selected from 1,4-cyclohexadiene, 1,3-cyclohexadiene, and 1-methyl-1,4-cyclohexadiene.

### Claim 15 (depends on 14)

The method of claim 14, further comprising depositing a metal nitride interlayer directly on the metal oxide layer prior to depositing the metal nitride layer directly on the metal nitride interlayer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the metal nitride interlayer is deposited by a second atomic layer deposition process comprising sequentially and alternating contacting the substrate with the metal precursor and the nitrogen reactant.

### Claim 17 (depends on 16)

The method of claim 16, wherein the metal nitride layer is a conductive layer and the metal nitride interlayer is an insulating layer.

### Claim 18 (depends on 16)

The method of claim 16, wherein the metal nitride layer has a first stoichiometry and the metal nitride interlayer has a second stoichiometry, wherein the first stoichiometry and the second stoichiometry are different from each other.

### Claim 19 (depends on 17)

The method of claim 17, wherein the metal nitride layer comprises a first hafnium nitride layer and the metal nitride interlayer comprise a second hafnium nitride layer.

### Claim 20 (depends on 19)

The method of claim 19, wherein the first hafnium nitride layer has a HfN stoichiometry and the second hafnium nitride layer has a Hf3N4 stoichiometry.