# US 2026/0092355 A1 · Components with thermal barrier coatings having solid films thereon and methods of coating the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0092355 A1
- Document ID: US20260092355A1
- Status: Published application
- Kind: A1
- Application number: 18/899,691
- Filed: 2024-09-27
- Published: 2026-04-02
- Earliest claimed: 2024-09-27
- Assignees: Honeywell International Inc.
- Applicants: Honeywell International Inc.
- Inventors: Jason Van Sluytman; Vladimir Tolpygo
- Web page: https://patentgrep.com/patent/US20260092355A1

## CPC

- C23C 14/083: {of refractory metals or yttrium}
- C23C 4/11: Oxides
- C23C 4/134: Plasma spraying
- C23C 4/18: After-treatment
- C23C 14/08: Oxides (C23C14/10 takes precedence)
- C23C 14/221: {Ion beam deposition (C23C14/46, C23C14/48 take precedence)}
- C23C 14/30: by electron bombardment
- C23C 14/58: After-treatment
- C23C 14/5806: {Thermal treatment}
- C23C 18/1245: {Inorganic substrates other than metallic}
- C23C 18/1254: {Sol or sol-gel processing}
- C23C 28/042: {including a refractory ceramic layer, e.g. refractory metal oxides, ZrO2, rare earth oxides}
- F01D 25/005: {Selecting particular materials}
- F05D 2230/31: Layer deposition
- F05D 2300/2112: Aluminium oxides
- F05D 2300/2118: Zirconium oxides
- F05D 2300/611: Coating
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

Components and methods for coating the components are provided. The methods include depositing a coating composition on a substrate that includes about 350 wt. % rare-earth oxides, 45-96.5 wt. % zirconia, and 0.5-4 wt. % alumina, heat treating the coating composition to form a CMAS-resistant thermal barrier coating (TBC) that includes a columnar microstructure with voids in open communication with a surface thereof, wherein the alumina is homogeneously distributed throughout the TBC, contacting the TBC with a film precursor, transporting the film precursor along interior wall surfaces of the voids to form a thin film thereon, wherein the thin film has a thickness on the interior wall surfaces of 10-150 nm, and forming a solid film on the interior wall surfaces of the voids from the film precursor that includes aluminum phosphate and that does not fill the voids that have diameters of 50 nm or greater.

## Claims

### Claim 1

A method, comprising:
depositing a coating composition on a substrate, the coating composition comprising:
from about 3 to about 50 wt. % of one or more rare-earth oxides;
from about 45 to about 96.5 wt. % zirconia; and
from about 0.5 to about 4 wt. % alumina, each based on the total weight of the coating composition;
heat treating the substrate with the coating composition thereon to form a calcia-magnesia-alumina-silicate (CMAS)-resistant thermal barrier coating (TBC) on the substrate, wherein the CMAS-resistant TBC includes a columnar microstructure with voids in open communication with a surface thereof, wherein the alumina is deposited homogeneously throughout the CMAS-resistant TBC;
contacting the CMAS-resistant TBC with a film precursor;
transporting the film precursor along interior wall surfaces of the voids of the CMAS-resistant TBC to form a thin film thereon, wherein the thin film has a thickness on the interior wall surfaces of at least 10 nm and less than 150 nm; and
forming a solid film on the interior wall surfaces of the voids from the film precursor, wherein the solid film includes aluminum phosphate, wherein the solid film does not completely fill at least some of the voids that have diameters of 50 nm or greater.

### Claim 2 (depends on 1)

The method of claim 1, wherein depositing the coating composition is performed by electron beam-physical vapor deposition (EBPVD) or plasma spraying.

### Claim 3 (depends on 1)

The method of claim 1, wherein the CMAS-resistant TBC is free from second phase precipitates.

### Claim 4 (depends on 1)

The method of claim 1, wherein the alumina in the CMAS-resistant TBC have a maximum particle size of about 1 μm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the one or more rare-earth oxides of the coating composition are selected from the group consisting of yttria, ytterbia, lanthana, gadolinia, niobia, tantala, scandia, erbia, lanthana, samaria, and combinations thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein transporting the film precursor along the interior wall surfaces of the voids includes maintaining contact between the film precursor and the CMAS-resistant TBC for at least five minutes.

### Claim 7 (depends on 1)

The method of claim 1, wherein transporting the film precursor along the interior wall surfaces of the voids includes producing a pressure differential between an exterior of the CMAS-resistant TBC and the interior wall surfaces of the voids.

### Claim 8 (depends on 1)

The method of claim 1, wherein transporting the film precursor along the interior wall surfaces of the voids includes vaporizing a vaporizable component of the film precursor.

### Claim 9 (depends on 1)

The method of claim 1, further comprising producing the film precursor to have a viscosity of 150 cSt or less.

### Claim 10 (depends on 1)

The method of claim 1, further comprising producing the film precursor to have a solids yield of at least 100 g/L and an aluminum-to-phosphorus atomic ratio of at least 0.5:1.

### Claim 11 (depends on 1)

The method of claim 1, wherein forming the solid film on the interior wall surfaces includes drying the thin film to produce a solid residue on the interior wall surfaces.

### Claim 12 (depends on 1)

The method of claim 1, further comprising:
transporting the film precursor along interior wall surfaces of internal pores of a thermal barrier material of the CMAS-resistant TBC, wherein the internal pores have diameters of 300 nm or less that are open to surfaces of the thermal barrier material; and
forming the solid film on the interior wall surfaces of the internal pores from the film precursor.

### Claim 13 (depends on 1)

The method of claim 1, wherein the solid film has a thickness on the interior wall surfaces of the voids of at least 5 nm and up to 500 nm.

### Claim 14 (depends on 1)

The method of claim 1, wherein the substrate is a surface of a component of a gas turbine engine.

### Claim 15

A component of a gas turbine engine, comprising:
a substrate;
a calcia-magnesia-alumina-silicate (CMAS)-resistant thermal barrier coating (TBC) on the substrate, wherein the CMAS-resistant TBC is formed from a coating composition comprising from about 3 to about 50 wt. % of one or more rare-earth oxides, from about 45 to about 96.5 wt. % zirconia, and from about 0.5 to about 4 wt. % alumina, each based on the total weight of the coating composition, wherein the alumina is homogeneously distributed throughout the CMAS-resistant TBC, wherein the CMAS-resistant TBC includes a columnar microstructure with voids in open communication with a surface thereof; and
a solid film on the interior wall surfaces of the voids of the CMAS-resistant TBC, wherein the solid film includes aluminum phosphate, wherein the solid film does not completely fill at least some of the voids that have diameters of 50 nm or greater.

### Claim 16 (depends on 15)

The component of claim 15, wherein the CMAS-resistant TBC is free from second phase precipitates.

### Claim 17 (depends on 15)

The component of claim 15, wherein the alumina in the CMAS-resistant TBC have a maximum particle size of about 1 μm.

### Claim 18 (depends on 15)

The component of claim 15, wherein the one or more rare-earth oxides of the CMAS-resistant TBC are selected from the group consisting of yttria, ytterbia, lanthana, gadolinia, niobia, tantala, scandia, erbia, lanthana, samaria, and combinations thereof.

### Claim 19 (depends on 15)

The component of claim 15, wherein the CMAS-resistant TBC includes a thermal barrier material having internal pores having diameters of 300 nm or less that are open to surfaces of the thermal barrier material and the solid film covers interior wall surfaces of at least some of the internal pores.

### Claim 20 (depends on 15)

The component of claim 15, wherein the solid film has a thickness on the interior wall surfaces of the voids of at least 5 nm and up to 500 nm.