# US 2026/0092350 A1 · Pre-oxidized, coating-free press hardened steel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0092350 A1
- Document ID: US20260092350A1
- Status: Published application
- Kind: A1
- Application number: 18/917,542
- Filed: 2024-10-16
- Published: 2026-04-02
- Earliest claimed: 2024-09-30
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Zhou Wang; Zhao Li; MingFeng Shi; Sarah Tedesco; Jianfeng Wang; Jiachen Pang; Zhen Chen
- Web page: https://patentgrep.com/patent/US20260092350A1

## CPC

- C23C 8/10: Oxidising
- C21D 9/46: for sheet metals
- C22C 38/06: containing aluminium
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C22C 38/32: with boron
- C22C 38/38: with more than 1.5% by weight of manganese
- C21D 1/673: for die quenching
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/48: with niobium or tantalum
- C22C 38/58: with more than 1.5% by weight of manganese
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A pre-oxidized steel sheet for press hardening, a press hardened, pre-oxidized steel sheet for a vehicle component, and a method of forming a pre-oxidized steel sheet. The pre-oxidized steel sheet includes a surface, a bulk region beneath the surface, and an oxide layer disposed on the surface. The oxide layer exhibits a thickness in the range of 20 nanometers to 60 nanometers and includes at least one of a manganese oxide, an iron oxide, a manganese iron oxide, a chromium oxide, and an amorphous silicon oxide.

## Claims

### Claim 1

A pre-oxidized steel sheet for press hardening, comprising:
a surface;
a bulk region beneath the surface, the bulk region comprising a steel composition including
carbon (C) present in the range of 0.05 weight percent to 0.35 weight percent of the total weight percent of the composition,
manganese (Mn) present in the range of 0.5 weight percent to 5.0 weight percent of the total weight percent of the composition,
silicon (Si) present in the range of 0.5 weight percent to 2.0 weight percent of the total weight percent of the composition,
chromium (Cr) present in the range of 0.6 weight percent to 4.0 weight percent of the total weight percent of the composition,
optionally niobium (Nb) present in the range of 0.02 weight percent to 0.05 weight percent of the total weight percent of the composition, and
iron present in the remainder of the composition to provide a total weight percent of 100 percent; and
an oxide layer disposed on the surface, the oxide layer comprising at least one of a manganese oxide, an iron oxide, a manganese iron oxide, a chromium oxide, and an amorphous silicon oxide, the oxide layer exhibiting a thickness in the range of 20 nanometers to 60 nanometers.

### Claim 2 (depends on 1)

The pre-oxidized steel sheet of claim 1, further comprising a subsurface depletion zone between the bulk region and the surface, wherein the subsurface depletion zone exhibits a thickness of less than 0.7 micrometers and includes manganese present in the range of 25 percent to 50 percent of the amount of manganese in the bulk region.

### Claim 3 (depends on 1)

The pre-oxidized steel sheet of claim 1, wherein the oxide layer includes a relative weight percent ratio of MnFe2O4 to Fe2O3 in the range of 1:1 to 5:1.

### Claim 4 (depends on 1)

The pre-oxidized steel sheet of claim 1, wherein the oxide layer includes a relative weight percent ratio of Mn2O3 to MnFe2O4 in the range of 0.35:1 to 3:1.

### Claim 5

A press hardened, pre-oxidized steel sheet for a vehicle component, comprising:
a surface;
a bulk region beneath the surface, the bulk region comprising a steel composition including
carbon (C) present in the range of 0.05 weight percent to 0.35 weight percent of the total weight percent of the composition,
manganese (Mn) present in the range of 0.5 weight percent to 5.0 weight percent of the total weight percent of the composition,
silicon (Si) present in the range of 0.5 weight percent to 2.0 weight percent of the total weight percent of the composition,
chromium (Cr) present in the range of 0.6 weight percent to 4.0 weight percent of the total weight percent of the composition,
optionally niobium (Nb) present in the range of 0.02 weight percent to 0.05 weight percent of the total weight percent of the composition, and
iron present in the remainder of the composition to provide a total weight percent of 100 percent; and
an oxide layer disposed on the surface, the oxide layer comprising at least one of a manganese oxide, an iron oxide, a manganese iron oxide, a chromium oxide, and an amorphous silicon oxide, the oxide layer exhibiting a thickness in the range of 60 nanometers to 1 micrometer.

### Claim 6 (depends on 5)

The press hardened, pre-oxidized steel sheet of claim 5, wherein the bulk region exhibits a martensitic structure present in the range of 85 to 99.8 percent by volume of the total volume of the bulk region with austenite present in the range of 0. 1 to 8 percent by volume of the total volume of the bulk region and carbide phases present in the range of 0.1 to 7 percent by volume of the total volume of the bulk region, wherein the total volume of the bulk region is 100 percent.

### Claim 7 (depends on 6)

The press hardened, pre-oxidized steel sheet of claim 6, wherein the carbide phases are enriched with chromium and a chromium content of the carbide phases is in the range of 5 weight percent to 51 weight percent of the carbide phases.

### Claim 8 (depends on 5)

The press hardened, pre-oxidized steel sheet of claim 5, wherein the press hardened, pre-oxidized steel sheet component exhibits a yield strength in the range of 1,000 Megapascals to 1,500 Megapascals, an ultimate tensile strength in the range of 1,400 Megapascals to 1,900 Megapascals, and a total elongation in the range of 5 percent to 10 percent.

### Claim 9

A method of forming a pre-oxidized steel sheet for a vehicle component, comprising:
heating a steel sheet in a first process environment at a pre-oxidization temperature in the range of 600 degrees Celsius to 850 degrees Celsius for a pre-oxidation time period in the range of 0.1 seconds to 1,000 seconds, wherein the steel sheet includes the following steel composition:
carbon (C) present in the range of 0.05 weight percent to 0.35 weight percent of the total weight percent of the composition,
manganese (Mn) present in the range of 0.5 weight percent to 5.0 weight percent of the total weight percent of the composition,
silicon (Si) present in the range of 0.5 weight percent to 2.0 weight percent of the total weight percent of the composition,
chromium (Cr) present in the range of 0.6 weight percent to 4.0 weight percent of the total weight percent of the composition,
optionally niobium (Nb) present in the range of 0.02 weight percent to 0.05 weight percent of the total weight percent of the composition, and
iron present in the remainder of the composition to provide a total weight percent of the composition of 100 percent; and
forming an oxide layer on a surface of the steel sheet exhibiting a thickness in the range of 20 nanometers to 60 nanometers on a surface of the steel sheet, the oxide layer comprising at least one of a manganese oxide, an iron oxide, a manganese iron oxide, a chromium oxide, and an amorphous silicon oxide to provide a pre-oxidized steel sheet.

### Claim 10 (depends on 9)

The method of claim 9, further comprising exposing the steel sheet to air in the first process environment.

### Claim 11 (depends on 9)

The method of claim 9, further comprising exposing the steel sheet in the first process environment to dry air exhibiting a first dew point in the range of minus 40 degrees Celsius to 50 degrees Celsius.

### Claim 12 (depends on 9)

The method of claim 9, further comprising exposing the steel sheet in the first process environment to moisture and at least one of nitrogen, hydrogen, and carbon monoxide, wherein the moisture in the process environment provides the oxygen to form the oxide layer.

### Claim 13 (depends on 9)

The method of claim 9, further comprising forming a subsurface depletion zone between a bulk region below the surface and the surface.

### Claim 14 (depends on 13)

The method of claim 13, further comprising forming the subsurface depletion zone to a thickness in the range of 0.01 to 0.7 micrometers and includes manganese present in the range of 25 percent to 50 percent of the amount of manganese in the bulk region.

### Claim 15 (depends on 9)

The method of claim 9, further comprising annealing the steel sheet concurrently with heating the steel sheet.

### Claim 16 (depends on 9)

The method of claim 9, wherein the steel sheet includes an oil layer and the method further comprises burning the oil layer off of the steel sheet.

### Claim 17 (depends on 9)

The method of claim 9, further comprising heating the pre-oxidized steel sheet to a press hardening temperature in the range of 850 degrees Celsius to 1200 degrees Celsius in a second process environment.

### Claim 18 (depends on 17)

The method of claim 17, further comprising exposing the pre-oxidized steel sheet to air in the second process environment.

### Claim 19 (depends on 17)

The method of claim 17, further comprising exposing the pre-oxidized steel sheet to dry air exhibiting a first dew point in the range of minus 40 degrees Celsius to 10 degrees Celsius in the second process environment.

### Claim 20 (depends on 17)

The method of claim 17, further comprising pressing the pre-oxidized steel sheet in a die after heating; and quenching the pre-oxidized steel sheet at a cooling rate in the range of 20 degrees Celsius per second to 200 degrees Celsius per second.