# US 2026/0091986 A1 · Method for improving particle size and morphology of neutralizer for laterite nickel ore hydrometallurgy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0091986 A1
- Document ID: US20260091986A1
- Status: Published application
- Kind: A1
- Application number: 18/870,504
- Filed: 2023-07-03
- Published: 2026-04-02
- Earliest claimed: 2023-07-03
- Assignees: Pt Qmb New Energy Materials; Pt Esg New Energy Material; Gem Co., Ltd.; Pt Gem Indonesia New Energy Materials
- Applicants: Pt Qmb New Energy Materials; Pt Esg New Energy Material; Gem Co., Ltd.; Pt Gem Indonesia New Energy Materials
- Inventors: KAIHUA XU; SATRYO SOEMANTRI BRODJONEGORO; TEGAR MUKTI AJI; RIZKY WANALDI; ANDI SYAPUTRA HASIBUAN; PIYAN RAHMADI; ULFI ROHMAWATI; WENZE LIU
- Web page: https://patentgrep.com/patent/US20260091986A1

## CPC

- C01G 53/84: Hydroxides
- C22B 23/0461: {by chemical methods}
- C22B 3/04: by leaching (C22B3/18 takes precedence)
- C22B 3/06: in inorganic acid solutions {, e.g. with acids generated in situ; in inorganic salt solutions other than ammonium salt solutions}
- C22B 3/22: by physical processes, e.g. by filtration, by magnetic means {, or by thermal decomposition} (treatment or purification of solutions by liquid-liquid extraction C22B3/26)
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 21/0015: {by wet processes (C22B21/02, C22B21/04 and C22B21/06 take precedence)}
- C22B 23/0415: {with acids or salt solutions except ammonium salts solutions}
- C22B 47/00: Obtaining manganese
- Y02P 10/20: Recycling
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for improving the particle size and morphology of a neutralizing agent used in the laterite nickel ore hydrometallurgy, in a process flow for producing nickel-cobalt-manganese hydroxide by the laterite nickel ore hydrometallurgy, a nickel-cobalt-manganese-containing feed liquid is subjected to one-stage iron-aluminum removal treatment and two-stage iron-aluminum removal treatment by using a neutralizing agent successively, wherein the −200 mesh sieving rate by mass ratio of the neutralizing agent is 85%-90%, and the spherical coefficient of solid particles of the neutralizing agent is not less than 0.6. In the disclosure, the particle size and morphology of the neutralizing agent are respectively improved so as to be used in the steps of one-stage iron-aluminum removal treatment and two-stage iron-aluminum removal treatment. The iron-aluminum removal rates in the steps of one-stage iron-aluminum removal treatment and two-stage iron-aluminum removal treatment can be effectively increased, and at the same time, the surface roughness of the solid particles of the neutralizing agent can be ensured to be lower, thereby reducing the rates of nickel, cobalt, and manganese ions reacting with local alkali to generate precipitations, thereby reducing the loss of nickel, cobalt, and manganese and further improving the yield of nickel-cobalt-manganese hydroxide produced by the laterite nickel ore hydrometallurgy.

## Claims

### Claim 1

A method for improving the particle size and morphology of a neutralizer for laterite nickel ore hydrometallurgy, characterized in that in a process flow for producing nickel-cobalt-manganese hydroxide by the laterite nickel ore hydrometallurgy, a nickel-cobalt-manganese-containing feed liquid being subjected to one-stage iron-aluminum removal treatment and two-stage iron-aluminum removal treatment by using a neutralizer successively;
wherein the passing rate through a 200-mesh sieve of the neutralizer is 85%-90%, and the spherical coefficient of solid particles of the neutralizer is not less than 0.6.

### Claim 2 (depends on 1)

The method for improving the particle size and morphology of the neutralizer for laterite nickel ore hydrometallurgy according to claim 1, characterized in that in the process flow for producing nickel-cobalt-manganese hydroxide by the laterite nickel ore hydrometallurgy, the nickel-cobalt-manganese-containing feed liquid is subjected to the one-stage iron-aluminum removal treatment by using the neutralizer, and a one-stage iron-aluminum-containing residue and a one-stage iron-aluminum removal liquid are obtained after solid-liquid separation; the one-stage iron-aluminum removal liquid is subjected to a two-stage iron-aluminum removal treatment by using the neutralizer, and a two-stage iron-aluminum-containing residue and a two-stage iron-aluminum removal liquid are obtained after solid-liquid separation.

### Claim 3 (depends on 2)

The method for improving the particle size and morphology of the neutralizer for laterite nickel ore hydrometallurgy according to claim 2, characterized in that the material of the neutralizer is selected from at least one of limestone, lime milk, magnesite pulp, magnesia pulp, magnesium ore in laterite nickel ores, magnesium oxide, and sodium hydroxide.

### Claim 4 (depends on 1)

The method for improving the particle size and morphology of the neutralizer for laterite nickel ore hydrometallurgy according to claim 1, characterized in that the neutralizer is prepared from a raw ore material by a one-stage grinding treatment and a two-stage grinding treatment, respectively, wherein the one-stage grinding treatment adopts a vertical mill to grind the raw ore material so as to obtain a first powder, and the two-stage grinding treatment adopts a ball mill to grind and shape the first powder so as to obtain a second powder;
wherein the spherical coefficient of the second powder is greater than the spherical coefficient of the first powder.

### Claim 5 (depends on 4)

The method for improving the particle size and morphology of the neutralizer for laterite nickel ore hydrometallurgy according to claim 4, characterized in that the passing rate through a 200-mesh sieve of the raw ore material after the one-stage grinding treatment is 75% and the passing rate through a 200-mesh sieve of the raw ore material after the two-stage grinding treatment is 88%.

### Claim 6 (depends on 4)

The method for improving the particle size and morphology of the neutralizer for laterite nickel ore hydrometallurgy according to claim 4, characterized in that the particle size density distribution pattern of the solid particles of the neutralizer is a bimodal distribution pattern; the particle size density distribution of the solid particles of the neutralizer in a particle size range of 1 um to 10 um accounts for 2.5% to 4.5%; and the particle size density distribution of the solid particles of the neutralizer in a particle size range of 10 um to 20 um accounts for 2.5% to 2.8%.

### Claim 7 (depends on 1)

The method for improving the particle size and morphology of the neutralizer for laterite nickel ore hydrometallurgy according to claim 1, characterized in that the pH value of the one-stage iron-aluminum removal liquid is in a range of 3 to 4.2, and the pH value of the two-stage iron-aluminum removal liquid is in a range of 4.5 to 5.5.

### Claim 8 (depends on 1)

The method for improving the particle size and morphology of the neutralizer for laterite nickel ore hydrometallurgy according to claim 1, characterized in that the iron removal rate in the one-stage iron-aluminum removal treatment process is greater than 88.46%; the aluminum removal rate in the one-stage iron-aluminum removal treatment process is greater than 93.03%; the nickel precipitation rate in the one-stage iron-aluminum removal treatment process is less than 4.36%, the cobalt precipitation rate in the one-stage iron-aluminum removal treatment process is less than 4.47%; and the manganese precipitation rate in the one-stage iron-aluminum removal treatment process is less than 5.74%.

### Claim 9 (depends on 2)

The method for improving the particle size and morphology of the neutralizer for laterite nickel ore hydrometallurgy according to claim 2, characterized in that the iron removal rate in the two-stage iron-aluminum removal treatment process is greater than 51.95%; the aluminum removal rate in the two-stage iron-aluminum removal treatment process is greater than 99.03%; the nickel precipitation rate in the two-stage iron-aluminum removal treatment process is less than 17.20%, the cobalt precipitation rate in the two-stage iron-aluminum removal treatment process is less than 10.94%; and the manganese precipitation rate in the two-stage iron-aluminum removal treatment process is less than 10.20%.

### Claim 10 (depends on 1)

The method for improving the particle size and morphology of the neutralizer for laterite nickel ore hydrometallurgy according to claim 1, characterized in that before the step of subjecting the nickel-cobalt-manganese-containing feed liquid to the one-stage iron-aluminum removal treatment step using the neutralizer, the method further comprises:
subjecting the laterite nickel ore to an acid-leaching treatment to obtain a leached ore pulp;
subjecting the leached ore pulp to cycle leaching and pre-neutralization treatment to obtain a pre-neutralized slurry; and
subjecting the pre-neutralized slurry to counter-current washing, and solid-liquid separation to obtain a leaching tailing and the nickel-cobalt-manganese-containing feed liquid.