# US 2026/0091157 A1 · Injectable and temperature-responsive enhanced composite dual-network magnetic particle gel, and preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0091157 A1
- Document ID: US20260091157A1
- Status: Published application
- Kind: A1
- Application number: 19/414,178
- Filed: 2025-12-09
- Published: 2026-04-02
- Earliest claimed: 2025-07-08
- Assignees: Hefei University of Technology
- Applicants: Hefei University of Technology
- Inventors: Yang LU; Huai YANG; Xu YAN; Chaowei LU; Haojie LU; Xi JING
- Web page: https://patentgrep.com/patent/US20260091157A1

## CPC

- A61L 24/104: {Gelatin}
- A61L 24/001: {Use of materials characterised by their function or physical properties}
- A61L 24/0031: {Hydrogels or hydrocolloids}
- A61L 24/0089: {containing inorganic fillers not covered by groups A61L24/0078 or A61L24/0084}
- A61L 24/02: containing inorganic materials
- A61L 2400/06: Flowable or injectable implant compositions
- A61L 2400/12: Nanosized materials, e.g. nanofibres, nanoparticles, nanowires, nanotubes; Nanostructured surfaces
- A61L 2430/36: for embolization or occlusion, e.g. vaso-occlusive compositions or devices
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)

## Abstract

An injectable and temperature-responsive enhanced composite dual-network magnetic particle gel is a hydrogel, including a particle gel network formed by gelatin nanoparticles and Fe3O4 nanoparticles via an electrostatic interaction and a poly(N-isopropylacrylamide) (PNIPAM)-based temperature-sensitive polymer gel network. At room temperature, the hydrogel exhibits excellent shear-thinning and self-healing properties, and is easily injectable through needles and microcatheters. When raised to a human body temperature (37° C.), the temperature-sensitive polymer undergoes phase transition cross-linking, enhancing mechanical properties of the gel network. The hydrogel is injectable in vitro and exhibits temperature-responsive strengthening in vivo, meeting the requirements of a vascular interventional embolization material. The hydrogel can also generate magnetothermal heating under an alternating magnetic field, thereby achieving the embolization combined with magnetothermal therapy for liver cancer. The preparation method is simple, with high biocompatibility and a great potential for clinical applications.

## Claims

### Claim 1

A preparation method of an injectable and temperature-responsive enhanced composite dual-network magnetic particle gel, comprising following steps:
S1, dissolving a temperature-sensitive polymer respectively in a solution of gelatin nanoparticles and a solution of Fe3O4 nanoparticles in an ice bath, and mixing two obtained solutions to obtain a reaction system;
S2, adding a glucono-δ-lactone (GDL) powder to adjust a pH of the reaction system to less than 7, such that a surface charge of the gelatin nanoparticles changes from negative to positive while a surface charge of the Fe3O4 nanoparticles remains negative, and an electrostatic interaction occurs between the gelatin nanoparticles and the Fe3O4 nanoparticles to achieve assembly, thereby forming a primary gel network; and
S3, heating the reaction system to 37° C, such that the temperature-sensitive polymer dispersed in the primary gel network undergoes hydrophilic-to-hydrophobic phase transition cross-linking to form a secondary gel network, thereby obtaining the injectable and temperature-responsive enhanced composite dual-network magnetic particle gel.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein a preparation process of the gelatin nanoparticles in the step S1 comprises following steps:
S11, dissolving a gelatin powder in deionized water, adding acetone, allowing an obtained mixture to stand at room temperature for 1 h, discarding an obtained supernatant, redissolving an obtained lower gelatin precipitate in the deionized water, and conducting freeze-drying to obtain purified gelatin, wherein the gelatin powder is added at a mass of 1 g to 50 g, and the deionized water and the acetone each are added at a volume of 50 mL to 500 mL;
S12, dissolving the purified gelatin obtained in the step S11 in the deionized water, adding dilute hydrochloric acid to adjust a pH of an obtained solution to 2.3, dropwise adding the acetone under vigorous stirring, adding glutaraldehyde, stirring overnight, adding an aqueous solution of glycine to an obtained gelatin dispersion, stirring for 1 h, and conducting centrifugation and washing to obtain the gelatin nanoparticles, wherein the purified gelatin and the glycine are added at masses of 1 g to 10 g and 1 g to 5 g, respectively, and the deionized water, the acetone, and the glutaraldehyde are added at volumes of 50 mL to 100 mL, 200 mL to 400 mL, and 0.1 mL to 2 mL, respectively;
a preparation process of the temperature-sensitive polymer in the step S1 comprises following steps: dissolving polyethylene glycol (PEG) and triethylamine (TEA) in dichloromethane (DCM), introducing argon for protection, dropwise adding 2-bromoisobutyryl bromide at 0° C., stirring to allow a reaction at room temperature for 24 h, and subjecting an obtained reaction product to dialysis and freeze-drying in sequence to obtain an atom transfer radical polymerization initiator; and dissolving the atom transfer radical polymerization initiator in an isopropanol (IPA)/water mixed solvent, adding N-isopropylacrylamide (NIPAM), n-butyl acrylate (nBA), and cuprous chloride (CuCl) to allow full dissolution, introducing the argon for protection, conducting three freeze-thaw cycles under argon protection to allow oxygen removal, injecting tris[2-(dimethylamino)ethyl]amine via a microsyringe to allow polymerization at room temperature for 72 h, subjecting an obtained polymerized product to separation with a neutral alumina column, and subjecting an obtained separated product to dialysis and freeze-drying in sequence to obtain the temperature-sensitive polymer.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein a preparation process of the Fe3O4 nanoparticles in the step S1 comprises following steps: dissolving FeCl3·6H2O in a mixed solvent of ethylene glycol (EG) and diethylene glycol (DEG), adding polyacrylic acid (PAA) and stirring to allow a reaction for 1 h, adding sodium acetate (NaAc) and stirring to allow a reaction for 1 h, thereby obtaining a viscous precursor solution; and placing the viscous precursor solution in a 50 mL hydrothermal autoclave, conducting a hydrothermal reaction at 200° C. for 12 h, cooling, subjecting an obtained reaction product to centrifugation and washing with the deionized water 3 times, followed by freeze-drying to obtain the Fe3O4 nanoparticles.

### Claim 4 (depends on 3)

The preparation method according to claim 3, wherein the FeCl3·6H2O, the PAA, and the NaAc are added at masses of 1 g to 10 g, 0.1 g to 1 g, and 1 g to 10 g, respectively, and the EG and the DEG are added at volumes of 1 mL to 20 mL and 1 mL to 30 mL, respectively.

### Claim 5 (depends on 2)

The preparation method according to claim 2, wherein the PEG, the TEA, and the 2-bromoisobutyryl bromide are added at masses of 10 g to 30 g, 1 g to 10 g, and 2 g to 8 g, respectively.

### Claim 6 (depends on 2)

The preparation method according to claim 2, wherein the atom transfer radical polymerization initiator, the NIPAM, the nBA, and the CuCl are added at masses of 0.1 g to 0.5 g, 1 g to 10 g, 0.1 g to 0.5 g, and 10 mg to 50 mg, respectively, and the tris[2-(dimethylamino)ethyl]amine is added at a volume of 50 μL to 200 μL.

### Claim 7 (depends on 1)

The preparation method according to claim 1, wherein the gelatin nanoparticles, the Fe3O4 nanoparticles, and the temperature-sensitive polymer have solid contents of 4% to 8% weight by volume (w/v), 2% to 6% w/v, and 5% to 15% w/v, respectively, and the gelatin nanoparticles and the Fe3O4 nanoparticles each have a particle size of 100 nm to 300 nm in the injectable and temperature-responsive enhanced composite dual-network magnetic particle gel obtained in the step S3.