# US 2026/0090343 A1 · Line edge roughness reduction through application of tensile stress

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0090343 A1
- Document ID: US20260090343A1
- Status: Published application
- Kind: A1
- Application number: 19/309,403
- Filed: 2025-08-25
- Published: 2026-03-26
- Earliest claimed: 2024-09-20
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials Inc.
- Inventors: SIVANANDHA KANAKASABAPATHY; ZHIYU HUANG; RUDY WOJTECKI; CHARITH NANAYAKKARA; JOHN HAUTALA
- Web page: https://patentgrep.com/patent/US20260090343A1

## CPC

- H10P 76/2041: {Photolithographic processes}
- H10P 76/2043: {using an anti-reflective coating}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Embodiments described herein relate to a method, that obtaining a substrate with a patterned resist layer positioned over a patterning stack, wherein the patterned resist layer comprises a first low frequency roughness. In an embodiment, the method further includes forming a capping layer on the patterned resist layer. In an embodiment, a bottom of the patterned resist layer is exposed, and the patterned resist layer has a second low frequency line edge roughness that is lower than the first low frequency line edge roughness after the capping layer is formed.

## Claims

### Claim 1

A method, comprising:
obtaining a substrate with a patterned resist layer positioned over a patterning stack, wherein the patterned resist layer comprises a first low frequency roughness; and
forming a capping layer on the patterned resist layer, wherein a bottom of the patterned resist layer is exposed, and wherein the patterned resist layer has a second low frequency line edge roughness that is lower than the first low frequency line edge roughness after the capping layer is formed.

### Claim 2 (depends on 1)

The method of claim 1, wherein the patterned resist layer comprises a metal oxide resist material or a chemically amplified resist.

### Claim 3 (depends on 1)

The method of claim 1, wherein the patterned resist layer comprises an organic molecular resist, an organometallic resist, or a self-immolative polymer resist.

### Claim 4 (depends on 1)

The method of claim 1, wherein the capping layer is applied with an angled chemical vapor deposition process or an angled physical vapor deposition process.

### Claim 5 (depends on 4)

The method of claim 4, wherein an angle of the angled chemical vapor deposition process or the angled physical vapor deposition process is between approximately 30° and approximately 60°.

### Claim 6 (depends on 1)

The method of claim 1, wherein the capping layer comprises one or more of silicon, carbon, or nitrogen.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
trimming the capping layer so that the capping layer has a first width that substantially matches a second width of an individual line of the patterned resist layer.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
applying a treatment to the patterned resist layer before the capping layer is formed, after the capping layer is formed, or during the formation of the capping layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein the treatment comprises one or more of an ultraviolet treatment, a thermal annealing treatment, or an oxidation treatment.

### Claim 10 (depends on 1)

The method of claim 1, wherein the patterned resist layer is formed through an extreme ultraviolet exposure and development process.

### Claim 11

A method, comprising:
obtaining a substrate with a patterned resist layer positioned over a patterning stack, wherein the patterned resist layer comprises a line, and wherein the line has a curvature with a first magnitude;
forming a capping layer over the line, wherein the capping layer covers a portion of a sidewall of the line, and wherein the capping layer induces a tensile stress into the line to change the curvature so that the curvature has a second magnitude that is smaller than the first magnitude.

### Claim 12 (depends on 11)

The method of claim 11, further comprising:
trimming the capping layer so that an entire sidewall of the line is exposed.

### Claim 13 (depends on 11)

The method of claim 11, wherein the capping layer is applied with an angled chemical vapor deposition process or an angled physical vapor deposition process.

### Claim 14 (depends on 11)

The method of claim 11, wherein the capping layer comprises one or more of silicon, carbon, or nitrogen.

### Claim 15 (depends on 11)

The method of claim 11, further comprising:
applying a treatment to the patterned resist layer before the capping layer is formed, after the capping layer is formed, or during the formation of the capping layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the treatment comprises one or more of an ultraviolet treatment, a thermal annealing treatment, or an oxidation treatment.

### Claim 17 (depends on 11)

The method of claim 11, wherein the patterned resist layer comprises a chemically amplified resist layer or a metal oxide resist layer.

### Claim 18

A method, comprising:
obtaining a substrate with a patterned resist layer with a plurality of lines positioned over a patterning stack, wherein the patterned resist layer comprises a chemically amplified resist layer or a metal oxide resist layer;
forming a capping layer over the plurality of lines, wherein the capping layer covers upper portions of the plurality of lines, and wherein bottom portions of the plurality of lines are exposed; and
transferring a pattern of the patterned resist layer into the patterning stack.

### Claim 19 (depends on 18)

The method of claim 18, wherein the capping layer comprises one or more of silicon, carbon, or nitrogen.

### Claim 20 (depends on 18)

The method of claim 18, further comprising:
applying a treatment to the patterned resist layer before the capping layer is formed, after the capping layer is formed, or during the formation of the capping layer, wherein the treatment comprises one or more of an ultraviolet treatment, a thermal annealing treatment, or an oxidation treatment.