# US 2026/0090049 A1 · Selective Formation Of Titanium Silicide And Titanium Nitride Byhydrogen Gas Control

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0090049 A1
- Document ID: US20260090049A1
- Status: Published application
- Kind: A1
- Application number: 19/409,322
- Filed: 2025-12-04
- Published: 2026-03-26
- Earliest claimed: 2018-05-18
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Cheng-Wei Chang; Kao-Feng Lin; Min-Hsiu Hung; Yi-Hsiang Chao; Huang-Yi Huang; Yu-Ting Lin
- Web page: https://patentgrep.com/patent/US20260090049A1

## CPC

- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 30/6219: {characterised by the source or drain electrodes}
- H10D 64/01312: {the additional layer comprising a metal or metal silicide formed by deposition, i.e. without a silicidation reaction, e.g. sputter deposition}
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10D 64/663: {the additional layers comprising a silicide layer contacting the layer of silicon, e.g. polycide gates}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present disclosure relates to a method for fabricating a semiconductor structure. The method includes providing a substrate with a gate structure, an insulating structure over the gate structure, and a S/D region; depositing a titanium silicide layer over the S/D region with a first chemical vapor deposition (CVD) process. The first CVD process includes a first hydrogen gas flow. The method also includes depositing a titanium nitride layer over the insulating structure with a second CVD process. The second CVD process includes a second hydrogen gas flow. The first and second CVD processes are performed in a single reaction chamber and a flow rate of the first hydrogen gas flow is higher than a flow rate of the second hydrogen gas flow.

## Claims

### Claim 1

A method, comprising:
depositing a gate dielectric layer on a substrate;
depositing a gate electrode on the gate dielectric layer;
forming a source/drain region on the substrate;
forming a metal silicide layer on the source/drain region;
forming, on the metal silicide layer, a metal nitride layer with a protruding region between a sidewall and a bottom surface of the metal nitride layer; and
depositing a conductive layer on the metal nitride layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the metal silicide layer comprises depositing a titanium layer on the source/drain region.

### Claim 3 (depends on 1)

The method of claim 1, wherein forming the metal nitride layer comprises depositing a titanium layer on the metal silicide layer.

### Claim 4 (depends on 3)

The method of claim 3, wherein forming the metal nitride layer further comprises performing a nitridation process on the titanium layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein forming the metal silicide layer comprises treating the source/drain region with a metal precursor at a first gas flow rate and a hydrogen gas at a second gas flow rate higher than the first gas flow rate.

### Claim 6 (depends on 1)

The method of claim 1, wherein forming the metal nitride layer comprises forming the metal nitride layer with the protruding region at a top corner of the metal silicide layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein forming the metal nitride layer comprises forming the metal nitride layer with the protruding region extending into the conductive layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein forming the metal nitride layer comprises forming the metal nitride layer with a U-shaped cross-sectional profile.

### Claim 9 (depends on 1)

The method of claim 1, wherein forming the metal nitride layer comprises forming the metal nitride layer with a thickness less than a thickness of the metal silicide layer.

### Claim 10 (depends on 1)

The method of claim 1, wherein forming the metal silicide layer comprises depositing a first titanium layer using a metal precursor at a first gas flow rate, and wherein forming the metal nitride layer comprises depositing a second titanium layer using the metal precursor at a second gas flow rate higher than the first gas flow rate.

### Claim 11

A method, comprising:
depositing a gate dielectric layer on a fin structure;
depositing a gate electrode on the gate dielectric layer;
forming a gate spacer along sidewalls of the gate dielectric layer and the gate electrode;
epitaxially growing a source/drain region on the fin structure;
forming a metal silicide layer on the source/drain region and on the gate spacer; and
forming, on the metal silicide layer and on the gate spacer, a metal nitride layer with a curved interface between the metal silicide layer and the metal nitride layer, wherein a curvature of the curved interface faces the metal nitride layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein forming the metal silicide layer comprises depositing a metal layer with a first portion on the source/drain region and a second portion on the gate spacer.

### Claim 13 (depends on 11)

The method of claim 11, wherein forming the metal nitride layer comprises:
depositing a metal layer on the metal silicide layer; and
performing a nitridation process on the metal layer.

### Claim 14 (depends on 11)

The method of claim 11, wherein forming the metal silicide layer comprises treating the source/drain region and the gate spacer with a metal precursor at a first gas flow rate and a hydrogen gas at a second gas flow rate higher than the first gas flow rate.

### Claim 15 (depends on 11)

The method of claim 11, wherein forming the metal silicide layer comprises depositing a first titanium layer using a metal precursor at a first gas flow rate, and wherein forming the metal nitride layer comprises depositing a second titanium layer using the metal precursor at a second gas flow rate higher than the first gas flow rate.

### Claim 16 (depends on 11)

The method of claim 11, further comprising depositing a conductive layer on the metal nitride layer.

### Claim 17

A method, comprising:
forming a source/drain region on a fin structure;
forming, on the source/drain region, a titanium silicide layer with protruding regions on a top surface of the titanium silicide layer;
depositing a titanium layer on the titanium silicide layer;
converting the titanium layer to a titanium nitride layer; and
depositing a conductive layer on the titanium nitride layer.

### Claim 18 (depends on 17)

The method of claim 17, wherein converting the titanium layer to the titanium nitride layer comprises exposing the titanium layer to ammonia gas.

### Claim 19 (depends on 17)

The method of claim 17, forming the titanium silicide layer with the protruding regions comprises forming the protruding regions of the titanium silicide layer extending into the titanium nitride layer.

### Claim 20 (depends on 17)

The method of claim 17, wherein forming the titanium nitride layer comprises forming the titanium nitride layer with a U-shaped cross-sectional profile.