# US 2026/0090000 A1 · Semiconductor structure and manufacturing method thereof, and high electron mobility transistor and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0090000 A1
- Document ID: US20260090000A1
- Status: Published application
- Kind: A1
- Application number: 19/054,614
- Filed: 2025-02-14
- Published: 2026-03-26
- Earliest claimed: 2024-09-20
- Assignees: National Tsing Hua University
- Applicants: National Tsing Hua University
- Inventors: King-Yuen WONG; Chun-Hao LAI
- Web page: https://patentgrep.com/patent/US20260090000A1

## CPC

- H10D 30/475: {having wider bandgap layer formed on top of lower bandgap active layer, e.g. undoped barrier HEMTs such as i-AlGaN/GaN HEMTs}
- H10D 30/015: {of FETs having heterojunction interface channels or heterojunction gate electrodes, e.g. HEMT}
- H10D 30/474: {having multiple parallel 2D charge carrier gas channels}
- H10D 62/343: {Gate regions of field-effect devices having PN junction gates}
- H10D 62/824: comprising only Group III-V materials heterojunctions, e.g. GaN/AlGaN heterojunctions
- H10P 14/3416: {Nitrides}
- H10P 14/3802: {Crystallisation or recrystallisation of non-monocrystalline semiconductor materials, e.g. regrowth}
- H10W 74/137: {the encapsulations being directly on the semiconductor body (H10W74/134 takes precedence)}
- H10W 74/147: {the encapsulations being multilayered}
- H10D 62/102: {Constructional design considerations for preventing surface leakage or controlling electric field concentration}
- H10D 62/117: {Shapes of semiconductor bodies}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor structure includes a substrate, a channel layer, a barrier layer, a gate structure, a first passivation layer and a second passivation layer. The channel layer is disposed on the substrate. The barrier layer is disposed on the channel layer. The gate structure and the first passivation layer are disposed on the barrier layer. The second passivation layer is disposed on the first passivation layer, and a material composition of the second passivation layer is different from a material composition of the first passivation layer. The channel layer has two first two-dimensional electron gas regions near the barrier layer, and the first two-dimensional electron gas regions are located on two sides of the gate structure. The barrier layer has two second two-dimensional electron gas regions near the first passivation layer, and the second two-dimensional electron gas regions are located on two sides of the gate structure.

## Claims

### Claim 1

A semiconductor structure, comprising:
a substrate;
a channel layer disposed on the substrate;
a barrier layer disposed on the channel layer;
a gate structure disposed on the barrier layer;
a first passivation layer disposed on the barrier layer and in contact with a side surface of the gate structure; and
a second passivation layer disposed on the first passivation layer, wherein a material composition of the second passivation layer is different from a material composition of the first passivation layer;
wherein the channel layer has two first two-dimensional electron gas regions near the barrier layer, and the two first two-dimensional electron gas regions are respectively located on two sides of the gate structure;
wherein the barrier layer has two second two-dimensional electron gas regions near the first passivation layer, and the two second two-dimensional electron gas regions are respectively located on the two sides of the gate structure.

### Claim 2 (depends on 1)

The semiconductor structure of claim 1, wherein the barrier layer has a thickness less than 10 nanometers, and the barrier layer is a III-V compound barrier layer.

### Claim 3 (depends on 1)

The semiconductor structure of claim 1, wherein the barrier layer is an aluminum gallium nitride (AlGaN) layer, and an aluminum atomic concentration of the barrier layer is less than 10%.

### Claim 4 (depends on 1)

The semiconductor structure of claim 1, wherein the gate structure comprises:
a semiconductor layer disposed on the barrier layer; and
a gate electrode disposed on the semiconductor layer.

### Claim 5 (depends on 4)

The semiconductor structure of claim 4, wherein the semiconductor layer has a thickness ranging from 30 nanometers to 80 nanometers, and the semiconductor layer is an undoped III-V compound semiconductor layer.

### Claim 6 (depends on 4)

The semiconductor structure of claim 4, further comprising:
a buffer layer disposed between the substrate and the channel layer;
wherein the buffer layer, the channel layer, the barrier layer and the semiconductor layer form an epitaxial structure.

### Claim 7 (depends on 1)

The semiconductor structure of claim 1, further comprising:
a spacer layer disposed between the channel layer and the barrier layer.

### Claim 8

A manufacturing method of a semiconductor structure, comprising:
providing a substrate and sequentially epitaxially growing a buffer layer, a channel layer, a barrier layer and a semiconductor layer on the substrate;
depositing a metal layer on the semiconductor layer;
etching the semiconductor layer and the metal layer to form a gate structure on the barrier layer;
sequentially depositing a first passivation layer and a second passivation layer to cover the barrier layer and the gate structure;
performing an annealing process to convert the first passivation layer from an amorphous structure to a crystal structure to form two first two-dimensional electron gas regions in the channel layer near the barrier layer and form two second two-dimensional electron gas regions in the barrier layer near the first passivation layer, wherein the two first two-dimensional electron gas regions are respectively located on two sides of the gate structure, and the two second two-dimensional electron gas regions are respectively located on the two sides of the gate structure; and
etching the first passivation layer and the second passivation layer to expose a gate electrode of the gate structure.

### Claim 9 (depends on 8)

The manufacturing method of the semiconductor structure of claim 8, wherein the barrier layer has a thickness less than 10 nanometers, the barrier layer is an aluminum gallium nitride (AlGaN) layer, and an aluminum atomic concentration of the barrier layer is less than 10%.

### Claim 10 (depends on 8)

The manufacturing method of the semiconductor structure of claim 8, wherein the semiconductor layer has a thickness ranging from 30 nanometers to 80 nanometers, and the semiconductor layer is an undoped III-V compound semiconductor layer.

### Claim 11

A high electron mobility transistor, comprising:
a substrate;
a channel layer disposed on the substrate;
a barrier layer disposed on the channel layer;
a drain electrode disposed on the barrier layer;
a source electrode disposed on the barrier layer;
a gate structure disposed on the barrier layer and located between the drain electrode and the source electrode;
a first passivation layer disposed on the barrier layer;
a second passivation layer disposed on the first passivation layer; and
a protection layer covering the second passivation layer and the gate structure;
wherein the channel layer has two first two-dimensional electron gas regions near the barrier layer, and the two first two-dimensional electron gas regions are respectively located on two sides of the gate structure;
wherein the barrier layer has two second two-dimensional electron gas regions near the first passivation layer, and the two second two-dimensional electron gas regions are respectively located on the two sides of the gate structure.

### Claim 12 (depends on 11)

The high electron mobility transistor of claim 11, wherein the barrier layer has a thickness less than 10 nanometers, and the barrier layer is a III-V compound barrier layer.

### Claim 13 (depends on 11)

The high electron mobility transistor of claim 11, wherein the barrier layer is an aluminum gallium nitride (AlGaN) layer, and an aluminum atomic concentration of the barrier layer is less than 10%.

### Claim 14 (depends on 11)

The high electron mobility transistor of claim 11, wherein the gate structure comprises:
a semiconductor layer disposed on the barrier layer; and
a gate electrode disposed on the semiconductor layer.

### Claim 15 (depends on 14)

The high electron mobility transistor of claim 14, wherein the semiconductor layer has a thickness ranging from 30 nanometers to 80 nanometers, and the semiconductor layer is an undoped III-V compound semiconductor layer.

### Claim 16 (depends on 14)

The high electron mobility transistor of claim 14, further comprising:
a buffer layer disposed between the substrate and the channel layer, wherein the buffer layer, the channel layer, the barrier layer and the semiconductor layer form an epitaxial structure;
a spacer layer disposed between the channel layer and the barrier layer; and
a gate spacer disposed on the semiconductor layer and in contact with two opposite sidewalls of the gate electrode.

### Claim 17 (depends on 11)

The high electron mobility transistor of claim 11, wherein a first access region is formed between the drain electrode and the gate structure, a second access region is formed between the source electrode and the gate structure, the two first two-dimensional electron gas regions are respectively located in the first access region and the second access region, and the two second two-dimensional electron gas regions are respectively located in the first access region and the second access region.

### Claim 18

A manufacturing method of a high electron mobility transistor, comprising:
providing a substrate and sequentially epitaxially growing a buffer layer, a channel layer, a barrier layer and a semiconductor layer on the substrate;
depositing a metal layer on the semiconductor layer;
etching the semiconductor layer and the metal layer to form a gate structure on the barrier layer;
sequentially depositing a first passivation layer and a second passivation layer to cover the barrier layer and the gate structure;
performing an annealing process to convert the first passivation layer from an amorphous structure to a crystal structure to form two first two-dimensional electron gas regions in the channel layer near the barrier layer and form two second two-dimensional electron gas regions in the barrier layer near the first passivation layer, wherein the two first two-dimensional electron gas regions are respectively located on two sides of the gate structure, and the two second two-dimensional electron gas regions are respectively located on the two sides of the gate structure;
etching the first passivation layer and the second passivation layer to expose a gate electrode of the gate structure;
depositing a protection layer to cover the second passivation layer and the gate electrode;
etching the first passivation layer, the second passivation layer and the protection layer to form a first opening and a second opening; and
forming a drain electrode on the barrier layer and in the first opening, and forming a source electrode on the barrier layer and in the second opening.

### Claim 19 (depends on 18)

The manufacturing method of the high electron mobility transistor of claim 18, wherein the barrier layer has a thickness less than 10 nanometers, the barrier layer is an aluminum gallium nitride (AlGaN) layer, and an aluminum atomic concentration of the barrier layer is less than 10%.

### Claim 20 (depends on 18)

The manufacturing method of the high electron mobility transistor of claim 18, wherein the semiconductor layer has a thickness ranging from 30 nanometers to 80 nanometers, and the semiconductor layer is an undoped III-V compound semiconductor layer.