- Inventors: Ji-Feng LIU; Chao-Hsiu LI
- Web page: https://patentgrep.com/patent/US20260089926A1

## CPC

- H10B 12/482: {Bit lines}
- H10B 12/02: {for one transistor one-capacitor [1T-1C] memory cells}
- H10B 12/485: {Bit line contacts}
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A semiconductor structure includes a semiconductor substrate, a bit-line structure, and a bit-line spacer. The bit-line structure is disposed on the semiconductor substrate. The bit-line spacer covers the bit-line structure, in which the bit-line spacer includes a SiCO layer, an insulating oxide layer, and an insulating nitride layer. The SiCO layer covers the bit-line structure, in which an oxygen concentration of the SiCO layer is equal to or greater than 55 at %. The insulating oxide layer covers the SiCO layer. The insulating nitride layer covers the insulating oxide layer.

## Claims

### Claim 1

A semiconductor structure, comprising:
a semiconductor substrate;
a bit-line structure disposed on the semiconductor substrate; and
a bit-line spacer covering the bit-line structure, wherein the bit-line spacer comprises:
a SiCO layer covering the bit-line structure, wherein an oxygen concentration of the SiCO layer is equal to or greater than 55 at %;
an insulating oxide layer covering the SiCO layer; and
an insulating nitride layer covering the insulating oxide layer.

### Claim 2 (depends on 1)

The semiconductor structure of claim 1, wherein the oxygen concentration of the SiCO layer is from 55 at % to 65 at %.

### Claim 3 (depends on 1)

The semiconductor structure of claim 1, wherein a carbon concentration of the SiCO layer is from 5 at % to 12 at %.

### Claim 4 (depends on 1)

The semiconductor structure of claim 1, wherein the SiCO layer has a thickness of 8 angstrom to 15 angstrom.

### Claim 5 (depends on 1)

The semiconductor structure of claim 1, wherein the SiCO layer has a dielectric constant of 3.9 to 4.7.

### Claim 6 (depends on 1)

The semiconductor structure of claim 1, wherein the insulating oxide layer has a thickness of 3.5 angstrom to 5 angstrom.

### Claim 7 (depends on 1)

The semiconductor structure of claim 1, wherein the SiCO layer conformally covers a sidewall of the bit-line structure.

### Claim 8 (depends on 1)

The semiconductor structure of claim 1, wherein the bit-line structure comprises:
a conductive silicon layer;
a conductive layer disposed on the conductive silicon layer; and
a hard mask layer disposed on the conductive layer.

### Claim 9 (depends on 1)

The semiconductor structure of claim 1, wherein the SiCO layer is in direct contact with the bit-line structure.

### Claim 10 (depends on 1)

The semiconductor structure of claim 1, wherein the insulating oxide layer is a silicon dioxide layer, and the insulating nitride layer is a silicon nitride.

### Claim 11 (depends on 1)

The semiconductor structure of claim 1, wherein a density of the SiCO layer is 2.2 g/cm3 to 2.5 g/cm3.

### Claim 12

A method of manufacturing a semiconductor structure, the method comprising:
forming a bit-line structure on a semiconductor substrate;
forming a SiCO layer to cover the bit-line structure, wherein an oxygen concentration of the SiCO layer is equal to or greater than 55 at %;
forming an insulating oxide layer to cover the SiCO layer; and
forming an insulating nitride layer to cover the insulating oxide layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein forming the SiCO layer comprises reacting an oxygen gas and an alkyl siloxane to form the SiCO layer.

### Claim 14 (depends on 13)

The method of claim 13, wherein a reaction temperature is 500° C. to 600° C.

### Claim 15 (depends on 13)

The method of claim 13, wherein a flow rate of the oxygen gas is 75 sccm to 155 sccm.

### Claim 16 (depends on 13)

The method of claim 13, wherein a flow rate of the alkyl siloxane is 54 sccm to 66 sccm.

### Claim 17 (depends on 13)

The method of claim 13, wherein the alkyl siloxane comprises 1,1,3,3-tetramethyldisiloxane.

### Claim 18 (depends on 12)

The method of claim 12, wherein forming the SiCO layer is performed by remote plasma-enhanced atomic layer deposition or plasma-enhanced chemical vapor deposition.

### Claim 19 (depends on 12)

The method of claim 12, further comprising:
before forming the insulating oxide layer to cover the SiCO layer, forming a nitride layer to cover the SiCO layer and to fill a plurality of trenches in the semiconductor substrate and next to the bit-line structure; and
etching the nitride layer to expose a portion of the SiCO layer and leave portions of the nitride layer in the trenches by a wet etch solution.

### Claim 20 (depends on 19)

The method of claim 19, wherein the wet etch solution comprises H3PO4, NH4OH, H2O2, and H2O.