# US 2026/0089910 A1 · Method for fabricating a capacitor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0089910 A1
- Document ID: US20260089910A1
- Status: Published application
- Kind: A1
- Application number: 18/892,575
- Filed: 2024-09-23
- Published: 2026-03-26
- Earliest claimed: 2024-09-23
- Assignees: Nanya Technology Corporation
- Applicants: Nanya Technology Corporation
- Inventors: Ning-Shuang HSU
- Web page: https://patentgrep.com/patent/US20260089910A1

## CPC

- H10B 12/03: {Making the capacitor or connections thereto}
- H10D 1/696: {comprising multiple layers, e.g. comprising a barrier layer and a metal layer (barrier layers to prevent diffusion of hydrogen or oxygen in perovskite based capacitors H10D1/688)}
- H10D 1/716: {having vertical extensions}
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for fabricating a capacitor is provided. The method includes following steps. A mold is formed on an interconnect layer. A recess is formed in the mold. A bottom electrode layer is deposited on the mold and into the recess. A metal oxide layer is disposed on the bottom electrode layer and into the recess. A surface oxide layer is formed on the metal oxide layer. A non-O2 wet etching process is performed to remove the surface oxide layer, the metal oxide layer, and the mold from the bottom electrode layer.

## Claims

### Claim 1

A method for fabricating a capacitor, comprising:
forming a mold on an interconnect layer;
forming a recess in the mold;
depositing a bottom electrode layer on the mold and into the recess;
disposing a metal oxide layer on the bottom electrode layer and into the recess;
forming a surface oxide layer on the metal oxide layer; and
performing a non-O2 wet etching process to remove the surface oxide layer, the metal oxide layer, and the mold from the bottom electrode layer.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
lowering a top surface of the mold prior to depositing the bottom electrode layer.

### Claim 3 (depends on 1)

The method of claim 1, further comprising:
after the non-O2 wet etching process, forming a dielectric layer on the bottom electrode layer.

### Claim 4 (depends on 3)

The method of claim 3, further comprising:
depositing a top electrode layer on the dielectric layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the interconnection layer comprises a metal feature, and forming the recess is performed such that the recess is directly over the metal feature.

### Claim 6 (depends on 1)

The method of claim 1, wherein depositing the bottom electrode layer is performed such that the bottom electrode layer is in contact with a top surface of the mold.

### Claim 7 (depends on 1)

The method of claim 1, wherein the bottom electrode layer comprises a metal nitride layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein a thickness of the metal oxide layer is 5 Å to 10 Å.

### Claim 9 (depends on 1)

The method of claim 1, wherein the metal oxide layer comprises TiOx.

### Claim 10 (depends on 1)

The method of claim 1, wherein depositing the bottom electrode layer is performed such that a side surface of the bottom electrode layer is in contact with the mold.

### Claim 11 (depends on 10)

The method of claim 10, wherein forming the surface oxide layer is performed such that the surface oxide layer is spaced apart from the bottom electrode layer by the metal oxide layer.

### Claim 12

A method for fabricating a capacitor, comprising:
forming a mold on an interconnect layer;
depositing a bottom electrode layer on the mold;
disposing a metal oxide layer on a top surface of the bottom electrode layer, wherein the metal oxide layer is in direct contact with the bottom electrode layer;
oxidizing a top surface of the metal oxide layer; and
etching the metal oxide layer and the mold away from the bottom electrode layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the bottom electrode layer comprises a metal silicide nitride layer.

### Claim 14 (depends on 12)

The method of claim 12, wherein etching the metal oxide layer is performed with a non-O2 etchant.

### Claim 15 (depends on 12)

The method of claim 12, wherein a thickness of the bottom electrode layer is 5 Å to 10 Å.