# US 2026/0088445 A1 · Electrode assembly and rechargeable lithium battery including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0088445 A1
- Document ID: US20260088445A1
- Status: Published application
- Kind: A1
- Application number: 19/330,225
- Filed: 2025-09-16
- Published: 2026-03-26
- Earliest claimed: 2024-09-20
- Assignees: Samsung SDI Co., Ltd.; Industry-Academic Cooperation Foundation, Dankook University
- Applicants: Samsung SDI Co., Ltd.; Industry-Academic Cooperation Foundation, Dankook University
- Inventors: Hosung YANG; Duckjae YOU; Changwon PARK; Jiye WOO; Byoung-Sun LEE; Seok-won HONG
- Web page: https://patentgrep.com/patent/US20260088445A1

## CPC

- H01M 50/44: Fibrous material
- H01M 10/052: Li-accumulators
- H01M 50/414: Synthetic resins, e.g. thermoplastics or thermosetting resins
- H01M 50/434: Ceramics
- H01M 50/446: Composite material consisting of a mixture of organic and inorganic materials
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present disclosure relates to an electrode assembly including a negative electrode including a current collector, a negative electrode active material layer on the current collector, and a coating layer on the negative electrode active material layer; and a positive electrode. The coating layer includes an organic layer including polyimide nanofibers and a quinoline derivative. An average diameter of the polyimide nanofibers is less than or equal to about 200 nm. The present disclosure also relates to a method for manufacturing the electrode assembly.

## Claims

### Claim 1

An electrode assembly, comprising:
a negative electrode including a current collector, a negative electrode active material layer on the current collector, and a coating layer on the negative electrode active material layer; and
a positive electrode,
wherein the coating layer comprises an organic layer including polyimide nanofibers and a quinoline-based derivative, and
an average diameter of the polyimide nanofibers is less than or equal to about 200 nm.

### Claim 2 (depends on 1)

The electrode assembly as claimed in claim 1, wherein the coating layer is integrated with the negative electrode active material layer.

### Claim 3 (depends on 1)

The electrode assembly as claimed in claim 1, wherein the average diameter of the polyimide nanofibers is less than or equal to about 195 nm.

### Claim 4 (depends on 1)

The electrode assembly as claimed in claim 1, wherein:
a standard deviation of a diameter of the polyimide nanofibers is in a range of about 50 nm to about 90 nm,
a maximum value of a diameter of the polyimide nanofibers is in a range of about 250 nm to about 500 nm, and
a minimum value of a diameter of the polyimide nanofibers is in a range of about 40 nm to about 100 nm.

### Claim 5 (depends on 1)

The electrode assembly as claimed in claim 1, wherein an imidization index at 140° C. derived from FT-IR analysis data of the polyimide nanofibers is in a range of about 0.8 to about 0.9.

### Claim 6 (depends on 1)

The electrode assembly as claimed in claim 1, wherein the quinoline-based derivative comprises a compound represented by Chemical Formula 1:
wherein, in Chemical Formula 1, R1 to R7 are the same or different and each independently comprises at least one of hydrogen, a halogen, a hydroxyl group, a substituted or unsubstituted C1 to C30 alkyl group, a substituted or unsubstituted C1 to C10 alkylsilyl group, a substituted or unsubstituted C6 to C30 arylsilyl group, a substituted or unsubstituted C3 to C30 cycloalkyl group, a substituted or unsubstituted C3 to C30 heterocycloalkyl group, a substituted or unsubstituted C6 to C30 aryl group, a substituted or unsubstituted C2 to C30 heteroaryl group, a substituted or unsubstituted C1 to C20 alkoxy group, and a combination thereof.

### Claim 7 (depends on 6)

The electrode assembly as claimed in claim 6, wherein R1 to R7 each independently comprises at least one of hydrogen, a halogen, a hydroxyl group, a substituted or unsubstituted C1 to C30 alkyl group, and a combination thereof.

### Claim 8 (depends on 1)

The electrode assembly as claimed in claim 1, wherein a boiling point of the quinoline-based derivative is in a range of about 150° C. to about 300° C.

### Claim 9 (depends on 1)

The electrode assembly as claimed in claim 1, wherein a vapor pressure of the quinoline-based derivative is in a range of about 0.1 Pa to about 20 Pa.

### Claim 10 (depends on 1)

The electrode assembly as claimed in claim 1, wherein a content of the polyimide nanofibers is in a range of about 50 wt % to about 100 wt % based on 100 wt % of the coating layer.

### Claim 11 (depends on 1)

The electrode assembly as claimed in claim 1, wherein a content of the quinoline-based derivative is in a range of about 0.1 wt % to about 5 wt % based on 100 wt % of the coating layer.

### Claim 12 (depends on 1)

The electrode assembly as claimed in claim 1, wherein:
the organic layer is a porous layer including a plurality of pores, and
an average diameter of the pores is less than or equal to about 200 nm.

### Claim 13 (depends on 1)

The electrode assembly as claimed in claim 1, wherein at least a portion of the polyimide nanofibers is penetrated into the inside of the negative electrode active material layer.

### Claim 14 (depends on 1)

The electrode assembly as claimed in claim 1, wherein:
the coating layer further comprises an inorganic layer, and
the inorganic layer comprises at least one of alumina (Al2O3), boehmite (aluminum oxide hydroxide), zirconia, titanium oxide (TiO2), silica (SiO2), and a combination thereof.

### Claim 15 (depends on 1)

The electrode assembly as claimed in claim 1, wherein a thickness of the coating layer is in a range of about 1 μm to about 25 μm.

### Claim 16 (depends on 1)

The electrode assembly as claimed in claim 1, wherein a thickness of the organic layer is in a range of about 1 μm to about 25 μm.

### Claim 17 (depends on 1)

The electrode assembly as claimed in claim 1, wherein a peel strength of the coating layer is in a range of about 0.1 gf/mm to about 3.0 gf/mm.

### Claim 18

A method for manufacturing an electrode assembly, the method comprising:
mixing polyamic acid, a solvent, and a quinoline-based derivative to prepare a solution for forming an organic layer;
electrospinning the solution for forming the organic layer onto a negative electrode active material layer to manufacture a negative electrode active material layer coated with an organic layer; and
heat-treating a negative electrode active material layer coated with the organic layer at a temperature greater than or equal to about 50° C. and less than about 200° C. to form a coating layer on the negative electrode active material layer.

### Claim 19 (depends on 18)

The method as claimed in claim 18, wherein the quinoline-based derivative comprises a compound represented by Chemical Formula 1:
wherein, in Chemical Formula 1, R1 to R7 are the same or different and each independently comprises at least one of hydrogen, a halogen, a hydroxyl group, a substituted or unsubstituted C1 to C30 alkyl group, a substituted or unsubstituted C1 to C10 alkylsilyl group, a substituted or unsubstituted C6 to C30 arylsilyl group, a substituted or unsubstituted C3 to C30 cycloalkyl group, a substituted or unsubstituted C3 to C30 heterocycloalkyl group, a substituted or unsubstituted C6 to C30 aryl group, a substituted or unsubstituted C2 to C30 heteroaryl group, a substituted or unsubstituted C1 to C20 alkoxy group, and a combination thereof.

### Claim 20 (depends on 19)

The method as claimed in claim 19, wherein R1 to R7 each independently comprises at least one of hydrogen, a halogen, a hydroxyl group, a substituted or unsubstituted C1 to C30 alkyl group, and a combination thereof.

### Claim 21 (depends on 18)

The method as claimed in claim 18, wherein a boiling point of the quinoline-based derivative is in a range of about 150° C. to about 300° C.

### Claim 22 (depends on 18)

The method as claimed in claim 18, wherein a vapor pressure of the quinoline-based derivative is in a range of about 0.1 Pa to about 20 Pa.

### Claim 23 (depends on 1)

A rechargeable lithium battery comprising:
the electrode assembly as claimed in claim 1; and
an electrolyte.