# US 2026/0088296 A1 · Lithium-ion batteries with highly stable electrodes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0088296 A1
- Document ID: US20260088296A1
- Status: Published application
- Kind: A1
- Application number: 18/894,017
- Filed: 2024-09-24
- Published: 2026-03-26
- Earliest claimed: 2024-09-24
- Assignees: Nano and Advanced Materials Institute Limited
- Applicants: Nano and Advanced Materials Institute Limited
- Inventors: Yong ZHU; Jianping HAN; Pao Chieh WANG; Tze Lok Andy CHAN; Yingshun LI; Yangfan ZHOU; Shengbo LU; Li FU; Chenmin LIU
- Web page: https://patentgrep.com/patent/US20260088296A1

## CPC

- H01M 4/623: {fluorinated polymers}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/622: {being polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 50/411: Organic material
- H01M 50/491: Porosity
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A lithium-ion battery is provided, including a cathode with one or more nickel-rich ternary cathode materials, specifically LiNixMnyCozO2 or LiNixAlyCozO2, where x, y, and z sum to 1 and x is at least 0.8. The battery also includes an anode made from materials such as silicon, silicon oxide, carbon nanotubes, lithium metal, graphene, and graphite, and features a porous polymer separator with a porosity of 30% to 90%. An electrolyte is also included. A key aspect is the use of a gel-free binder, which is a modified polyvinylidene fluoride (PVDF) grafted with monomers containing at least one unsaturated carbon-carbon double bond and functional groups. This modification prevents defluorination and crosslinking of the PVDF when in contact with the nickel-rich cathode materials.

## Claims

### Claim 1

A lithium-ion battery, comprising:
a cathode comprising one or more nickel-rich ternary cathode materials selected from the materials having the following formula: LiNixMnyCozO2 or LiNixAlyCozO2, one or more conductive agents and a gel-free binder, wherein the sum of x, y and z equals 1, and x is greater than or equal to 0.8;
an anode including one or more materials selected from the group consisting of silicon, silicon oxide, carbon nanotubes, lithium metal, graphene, and graphite;
at least one porous polymer separator having a porosity from approximately 30% to 90%; and
an electrolyte;
wherein the gel-free binder is a modified polyvinylidene fluoride (PVDF) grafted with one or more monomers wherein the monomers comprise at least one unsaturated carbon-carbon double bond and one or more functional groups, such that the modified PVDF is prevented from defluorination and crosslinking when exposed to the nickel-rich cathode materials;
wherein the functional groups are selected from the group consisting of acrylic acid group, methacrylic acid group, phosphate group, polyethylene oxide group, sulfonate group, sulfate group, sulfite group, and cyano group.

### Claim 2 (depends on 1)

The lithium-ion battery of claim 1, wherein the gel-free binder enables the formation of an inorganic-rich cathode electrolyte interphase (CEI) on the surface of the cathode.

### Claim 3 (depends on 1)

The lithium-ion battery of claim 1, wherein the gel-free binder has a molecular weight of at least 1.1×106 Dalton.

### Claim 4 (depends on 2)

The lithium-ion battery of claim 2, wherein the inorganic-rich CEI has a LiF/C—O ratio higher than 1.0 and a LiF/Li2CO3 ratio higher than 2.0.

### Claim 5 (depends on 1)

The lithium-ion battery of claim 1, wherein the modified PVDF grafted with one or more monomers is fabricated by:
activating a PVDF main chain to generate reactive sites thereon; and
grafting the one or more monomers onto the reactive sites.

### Claim 6 (depends on 5)

The lithium-ion battery of claim 5, wherein the activation of the PVDF main chain is achieved by ozone treatment, plasma treatment, UV treatment or gamma ray radiation treatment.

### Claim 7 (depends on 5)

The lithium-ion battery of claim 5, wherein the grafting is conducted in a water or water/alcohol solution.

### Claim 8 (depends on 7)

The lithium-ion battery of claim 7, wherein the grafting is conducted under an inert atmosphere with a reaction temperature ranging from 40° C. to 80° C. and a reaction time of 1 to 50 hrs.

### Claim 9 (depends on 1)

The lithium-ion battery of claim 1, wherein the gel-free binder enhances the thermal stability of the cathode at temperatures up to 120° C.

### Claim 10 (depends on 1)

The lithium-ion battery of claim 1, wherein the battery has a specific energy density of at least 300 Wh/kg.