# US 2026/0088283 A1 · Positive electrode active materials for all-solid-state rechargeable batteries, preparation methods of positive electrode active materials, and all-solid-state rechargeable batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0088283 A1
- Document ID: US20260088283A1
- Status: Published application
- Kind: A1
- Application number: 19/336,734
- Filed: 2025-09-23
- Published: 2026-03-26
- Earliest claimed: 2024-09-23
- Assignees: Samsung SDI Co., Ltd.
- Applicants: Samsung SDI Co., Ltd.
- Inventors: Do-Yu KIM; Jayhyok SONG; Pilsang YUN; Hwichul YANG; Tae Ho CHO
- Web page: https://patentgrep.com/patent/US20260088283A1

## CPC

- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/364: {as mixtures}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0562: Solid materials
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed are a positive electrode active material for an all-solid-state rechargeable battery, a method of preparing the positive electrode active material, and an all-solid-state rechargeable battery. The positive electrode active material includes a first positive electrode active material including a first lithium nickel-based composite oxide particle in a form of secondary particles formed by agglomeration of primary particles. A first coating layer is disposed on surfaces of the first lithium nickel-based composite oxide particles and includes boron. A second coating layer is disposed on the first coating layer and includes zirconium. The positive electrode active material also comprises a second positive electrode active material comprising a second lithium nickel-based composite oxide particle in a form of single particles. A third coating layer is disposed on surfaces of the second lithium nickel-based composite oxide particles and includes zirconium.

## Claims

### Claim 1

A positive electrode active material for an all-solid-state rechargeable battery, the positive electrode active material comprising:
a first positive electrode active material comprising a first lithium nickel-based composite oxide particle in a form of secondary particles that are each formed by agglomeration of primary particles, with a first coating layer disposed on surfaces of the first lithium nickel-based composite oxide particles and including boron, and with a second coating layer disposed on the first coating layer and including zirconium; and
a second positive electrode active material comprising a second lithium nickel-based composite oxide particle in a form of single particles, with a third coating layer disposed on surfaces of the second lithium nickel-based composite oxide particles and including zirconium.

### Claim 2 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the first lithium nickel-based composite oxide particle is formed by agglomeration of primary particles, and at least some of the primary particles have a radial arrangement structure.

### Claim 3 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein an average particle diameter (D50) of the secondary particles of the first positive electrode active material is about 8 μm to about 25 μm.

### Claim 4 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the second coating layer comprises ZrO2 and Li6Zr2O7.

### Claim 5 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the second coating layer comprises a ZrO2 crystal phase, a Li6Zr2O7 crystal phase, and a Zr-containing amorphous phase.

### Claim 6 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the third coating layer comprises ZrO2 and Li6Zr2O7.

### Claim 7 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the third coating layer comprises a ZrO2 crystal phase, a Li6Zr2O7 crystal phase, and a Zr-containing amorphous phase.

### Claim 8 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein an average particle diameter (D50) of the single particles of the second positive electrode active material is about 2 μm to about 7 μm, and
wherein, based on 100 wt % of a total of the first positive electrode active material and the second positive electrode active material, the first positive electrode active material is included in an amount of about 60 wt % to about 95 wt %, and the second positive electrode active material is included in an amount of about 5 wt % to about 40 wt %.

### Claim 9 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the first coating layer of the first positive electrode active material comprises boron oxide, lithium boron oxide, or a combination thereof, and an amount of boron is about 0.01 wt % to about 0.5 wt % based on 100 wt % of a total metal in the first positive electrode active material excluding lithium.

### Claim 10 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the first positive electrode active material further comprises a grain boundary boron coating portion on surfaces of the primary particles in internal portions of the secondary particles, and
wherein (i) a weight of boron in the first coating layer is at least four times a weight of boron in the grain boundary boron coating portion, or (ii) a ratio of the weight of boron in the first coating layer to the weight of boron in the grain boundary boron coating portion is about 70:30 to about 98:2.

### Claim 11 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the positive electrode active material further comprises a boron doping layer inside the primary particles that are exposed on surfaces of the secondary particles, and
wherein the boron doping layer is located within a range of a depth of about 10 nm from outer surfaces of the primary particles exposed to the surfaces of the secondary particles, and the boron doping layer is provided along a perimeter of the surfaces of the secondary particles.

### Claim 12 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein an amount of zirconium in the second coating layer is about 0.1 parts by mole to about 0.6 parts by mole based on 100 parts by mole of particles comprising the lithium nickel-based composite oxide.

### Claim 13 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the second coating layer of the first positive electrode active material and the third coating layer of the second positive electrode active material each comprise ZrO2 and Li6Zr2O7,
wherein a total amount of an amount of zirconium in the second coating layer of the first positive electrode active material and an amount of zirconium in the third coating layer of the second positive electrode active material is about 0.1 parts by mole to about 0.6 parts by mole based on 100 parts by mole of total metals excluding lithium in the lithium nickel-based composite oxide of the first positive electrode active material and the lithium nickel-based composite oxide of the second positive electrode active material, and
wherein a thickness of each of the second coating layer of the first positive electrode active material and the third coating layer of the second positive electrode active material is about 5 nm to about 300 nm.

### Claim 14 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the first lithium nickel-based composite oxide particle comprises a lithium nickel-cobalt-aluminum-based composite oxide represented by Chemical Formula 1,
wherein the second lithium nickel-based composite oxide particle comprises a lithium nickel-cobalt-aluminum-manganese-based composite oxide represented Chemical Formula 2,
wherein Chemical Formula 1 is:
wherein, in Chemical Formula 1, 0.9≤a1≤1.2, 0.7≤x1<1, 0<y1<0.3, 0<z1<0.3, 0≤w1<0.3, 0.9≤x1+y1+z1+w1≤1.1, and 0≤b1≤0.1, M1 is at least one of B, Ba, Ca, Ce, Cr, Cu, Fe, Mg, Mo, Nb, Si, Sr, Sn, Ti, V, W, Y, Se, Zn, and Zr, and X is at least one of F, P, and S,
wherein Chemical Formula 2 is:
wherein, in Chemical Formula 2, 0.9≤a2≤1.2, 0.7≤x2<1, 0<y2<0.3, 0<z2<0.3, 0<w2<0.3, 0≤v2<0.3, 0.9≤x2+y2+z2+w2+v2≤1.1, and 0≤b2≤0.1, M2 is at least one of B, Ba, Ca, Ce, Cr, Cu, Fe, Mg, Mo, Nb, Si, Sr, Sn, Ti, V, W, Y, Se, Zn, and Zr, and X is at least one of F, P, and S.

### Claim 15

A method of preparing a positive electrode active material for an all-solid-state rechargeable battery, the method comprising
(i) mixing a first positive electrode active material precursor in a form of secondary particles comprising a first nickel-based composite hydroxide and formed by agglomeration of primary particles, a lithium raw material, and a boron raw material, to thereby form a mixture,
(ii) performing a first heat treatment on the mixture at a temperature of about 650° C. to about 850° C. to obtain a boron-coated first preliminary positive electrode active material,
(iii) dry mixing the boron-coated first preliminary positive electrode active material, a second preliminary positive electrode active material comprising a second lithium nickel-based composite oxide and having a form of a single particle, and a zirconium raw material, to thereby form a dry mixture and
(iv) performing a second heat treatment on the dry mixture to obtain a positive electrode active material.

### Claim 16 (depends on 15)

The method as claimed in claim 15, wherein the lithium raw material is mixed so that a molar ratio of lithium to a total metal of the first nickel-based composite hydroxide is about 0.8 to about 0.995,
wherein the boron raw material comprises H3BO3, HBO2, B2O3, C6H5B(OH)2, (C6H5O)3B, [CH3(CH2)3O]3B, C13H19BO3, C3H9B3O6, (C3H7O)3B, or a combination thereof, and
wherein boron is mixed in an amount of about 0.01 parts by mole to about 0.5 parts by mole based on 100 parts by mole of total metals in the first nickel-based composite hydroxide excluding lithium.

### Claim 17 (depends on 15)

The method as claimed in claim 15, wherein the first heat treatment is performed for about 5 hours to about 25 hours.

### Claim 18 (depends on 15)

The method as claimed in claim 15, wherein the first heat treatment comprises a temperature increase step and a temperature maintenance step,
wherein a temperature increase time in the first heat treatment is longer than a temperature maintenance time in the first heat treatment,
wherein a ratio of the temperature increase time to the temperature maintenance time is about 1.1:1 to about 10:1, and
wherein the temperature increase time is about 6 hours to about 16 hours and the temperature maintenance time is about 1 hours to about 9 hours.

### Claim 19 (depends on 1)

An all-solid-state rechargeable battery comprising
a positive electrode comprising the positive electrode active material for the all-solid-state rechargeable battery as claimed in claim 1,
a sulfide-based solid electrolyte,
a negative electrode, and
a solid electrolyte layer between the positive electrode and the negative electrode.

### Claim 20 (depends on 19)

The all-solid-state rechargeable battery as claimed in claim 19, wherein the negative electrode comprises a negative electrode current collector and a negative electrode coating layer disposed on the negative electrode current collector, the negative electrode coating layer comprising a compound in which a lithiophilic metal is supported on a carbon material, or a mixture of lithiophilic metal particles and carbon material particles,
wherein a lithium metal layer formed by charging is included between the negative electrode current collector and the negative electrode coating layer,
wherein, in the negative electrode coating layer, the lithiophilic metal comprises Al, Ag, Au, Bi, Cu, Ge, In, Mg, Ni, Pd, Pt, Si, Sn, Zn, or a combination thereof, and the carbon material is crystalline carbon, amorphous carbon, or a combination thereof, and