# US 2026/0086455 A1 · Method for manufacturing laminate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0086455 A1
- Document ID: US20260086455A1
- Status: Published application
- Kind: A1
- Application number: 19/332,437
- Filed: 2025-09-18
- Published: 2026-03-26
- Earliest claimed: 2024-09-26
- Assignees: Nichia Corporation
- Applicants: Nichia Corporation
- Inventors: Yuki KANAGAWA; Akihiko MITANI
- Web page: https://patentgrep.com/patent/US20260086455A1

## CPC

- G03F 7/0005: {Production of optical devices or components in so far as characterised by the lithographic processes or materials used therefor}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A method for manufacturing a laminate includes: disposing a resist material layer on an intermediate body; exposing the resist material layer to light using a mask including a first portion, a second portion having a light transmittance lower than that of the first portion, and a third portion having a light transmittance lower than that of the second portion; developing the exposed resist material layer to form a resist layer including a first region disposed in a region corresponding to the first portion, a second region disposed in a region corresponding to the second portion, spaced apart from the intermediate body, and connected to the first region, and an opening formed in a region corresponding to the third portion; forming a covering layer on the resist layer and the intermediate body; and removing the resist layer to remove a portion of the covering layer in contact with the resist layer.

## Claims

### Claim 1

A method for manufacturing a laminate, the method comprising:
disposing a resist material layer on an intermediate body, the resist material layer being made of a negative photoresist;
exposing the resist material layer to light using a mask comprising:
a first portion,
a second portion having a light transmittance lower than a light transmittance of the first portion, and
a third portion having a light transmittance lower than the light transmittance of the second portion, wherein:
the second portion is disposed between the first portion and the third portion in a top view;
developing the exposed resist material layer to form a resist layer comprising:
a first region disposed in a region corresponding to the first portion and in contact with the intermediate body,
a second region disposed in a region corresponding to the second portion, spaced apart from the intermediate body, and connected to the first region, and
an opening formed in a region corresponding to the third portion;
forming a covering layer on the resist layer and on the intermediate body such that at least a part of a surface of the resist layer other than an upper surface of the resist layer is exposed; and
removing the resist layer to remove a portion of the covering layer in contact with the resist layer.

### Claim 2 (depends on 1)

The method for manufacturing a laminate according to claim 1, wherein, in the step of forming the covering layer, the covering layer is formed by sputtering.

### Claim 3 (depends on 1)

The method for manufacturing a laminate according to claim 1, wherein the resist layer has a thickness in a range from 0.5 μm to 15 μm.

### Claim 4 (depends on 1)

The method for manufacturing a laminate according to claim 1, wherein the light transmittance of the second portion is in a range from 10% to 90% of the light transmittance of the first portion.

### Claim 5 (depends on 1)

The method for manufacturing a laminate according to claim 1, wherein:
the mask comprises a light-transmissive member, and a metal member disposed on the light-transmissive member;
an area of the metal member per unit area of the second portion is larger than an area of the metal member per unit area of the first portion; and
an area of the metal member per unit area of the third portion is larger than an area of the metal member per unit area of the second portion.

### Claim 6 (depends on 5)

The method for manufacturing a laminate according to claim 5, wherein:
the metal member is not disposed in the first portion;
a plurality of openings are formed in the metal member in the second portion; and
the metal member is disposed in the entire third portion.

### Claim 7 (depends on 5)

The method for manufacturing a laminate according to claim 5, wherein:
the metal member is not disposed in the first portion;
a plurality of the metal members are disposed to be spaced apart from each other in the second portion; and
the metal member is disposed in the entire third portion.

### Claim 8 (depends on 1)

The method for manufacturing a laminate according to claim 1, wherein, in the step of exposing the resist material layer, the light used for exposure is focused on an upper surface of the resist material layer.

### Claim 9 (depends on 1)

The method for manufacturing a laminate according to claim 1, wherein:
the mask further comprises a fourth portion disposed between the first portion and the second portion in a top view and having a light transmittance lower than the light transmittance of the first portion and higher than the light transmittance of the second portion; and
the resist layer comprises a third region disposed in a region corresponding to the fourth portion, spaced apart from the intermediate body, thicker than the second region, and disposed between the first region and the second region.

### Claim 10 (depends on 1)

The method for manufacturing a laminate according to claim 1, wherein:
the mask further comprises a fourth portion having a light transmittance lower than the light transmittance of the first portion and higher than the light transmittance of the second portion;
an upper surface of the intermediate body comprises a first surface and a second surface disposed at a position lower than the first surface; and
the second portion of the mask is disposed in a region corresponding to the first surface of the upper surface of the intermediate body, and the fourth portion of the mask is disposed in a region corresponding to the second surface of the upper surface of the intermediate body.

### Claim 11 (depends on 1)

The method for manufacturing a laminate according to claim 1, wherein:
the mask further comprises a fourth portion having a light transmittance lower than the light transmittance of the first portion and higher than the light transmittance of the second portion;
an upper surface of the intermediate body comprises a first surface and a second surface disposed at a position lower than the first surface;
in the step of exposing, the second portion of the mask is disposed in a region corresponding to the first surface of the upper surface of the intermediate body, and the fourth portion of the mask is disposed in a region corresponding to the second surface of the upper surface of the intermediate body; and
in the step of forming the resist layer, the resist layer comprises a third region disposed in a region corresponding to the fourth portion and spaced apart from the intermediate body, and a distance between the first surface of the intermediate body and the second region of the resist layer is equal to a distance between the second surface of the intermediate body and the third region of the resist layer.

### Claim 12 (depends on 1)

The method for manufacturing a laminate according to claim 1, wherein, in the step of forming the covering layer, a portion of the covering layer in contact with the resist layer is not connected to a portion of the covering layer in contact with the intermediate body.