# US 2026/0085638 A1 · Coated components for coke abatement in gas turbine engines

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0085638 A1
- Document ID: US20260085638A1
- Status: Published application
- Kind: A1
- Application number: 18/889,990
- Filed: 2024-09-19
- Published: 2026-03-26
- Earliest claimed: 2024-03-28
- Assignees: General Electric Company
- Applicants: General Electric Company
- Inventors: Arundhati Sengupta; Narayanan Janakiraman; Karthick Gourishankar; Sanjay Kumar Sondhi; Sreerama Prasad Ramaswamy; Lawrence B. Kool; Byron A. Pritchard; Kevin H. Janora
- Web page: https://patentgrep.com/patent/US20260085638A1

## CPC

- F02C 7/30: Preventing corrosion {or unwanted deposits} in gas-swept spaces
- B01J 23/10: of rare earths
- B01J 23/681: {with arsenic, antimony or bismuth}
- B01J 23/8913: {Cobalt and noble metals}
- B01J 23/8953: {with zinc, cadmium or mercury}
- B01J 35/19: {Catalysts containing parts with different compositions}
- B01J 35/393: {Metal or metal oxide crystallite size}
- B01J 35/395: {Thickness of the active catalytic layer}
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 35/45: Nanoparticles
- B01J 35/77: Compounds characterised by their crystallite size
- B01J 37/009: {Preparation by separation, e.g. by filtration, decantation, screening}
- B01J 37/0244: {Coatings comprising several layers}
- B01J 37/031: {Precipitation}
- B01J 37/036: {to form a gel or a cogel}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/343: {of ultrasonic wave energy}
- B08B 17/02: Preventing deposition of fouling or of dust
- B64D 33/00: Arrangement in aircraft of power plant parts or auxiliaries not otherwise provided for
- F23R 3/40: characterised by the use of catalytic means
- F02C: GAS-TURBINE PLANTS; AIR INTAKES FOR JET-PROPULSION PLANTS; CONTROLLING FUEL SUPPLY IN AIR-BREATHING JET-PROPULSION PLANTS (construction of turbines F01D; jet-propulsion plants F02K; construction of compressors or fans F04; generating combustion products of high pressure or high velocity F23R; using gas turbines in compression refrigeration plants F25B11/00)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B08B: CLEANING IN GENERAL; PREVENTION OF FOULING IN GENERAL
- B64D: EQUIPMENT FOR FITTING IN OR TO AIRCRAFT; FLIGHT SUITS; PARACHUTES; ARRANGEMENT OR MOUNTING OF POWER PLANTS OR PROPULSION TRANSMISSIONS IN AIRCRAFT
- F23R: GENERATING COMBUSTION PRODUCTS OF HIGH PRESSURE OR HIGH VELOCITY, e.g. GAS-TURBINE COMBUSTION CHAMBERS (fluidised bed combustion apparatus specially adapted for operation at superatmospheric pressures F23C10/16)

## Abstract

A coated component for coke abatement in a gas turbine engine. The coated component includes a substrate, and a catalytic coating. The catalytic coating includes a phase enriched in metal oxide and a phase enriched in noble metal. The metal oxide is of formula AxEyLzMOu where A is one or more alkaline earth elements, x ranges from zero to one, E is one or more alkali metals, y ranges from zero to one, L is one or more lanthanide elements, z ranges from zero to one, M is one or more d-block or p-block elements, O is oxygen, and u ranges from 0.95 to six.

## Claims

### Claim 1

A coated component for coke abatement in a gas turbine engine, the coated component comprising:
a substrate; and
a catalytic coating on the substrate, the catalytic coating including:
a metal oxide enriched region having an average crystallite size with a diameter ranging from three nanometers to eighty nanometers wherein the metal oxide enriched region is enriched in a metal oxide of formula AxEyLzMOu wherein:
A is one or more alkaline earth elements chosen from beryllium, magnesium, calcium, strontium, and barium; x ranges from zero to one; E is one or more alkali metals chosen from lithium, sodium, potassium, rubidium, and cesium; y ranges from zero to one; L is one or more lanthanide elements chosen from lanthanum, cerium, praseodymium, neodymium, samarium, europium, gadolinium, terbium, dysprosium, holmium, erbium, thulium, ytterbium, and lutetium; z ranges from zero to one; M is one or more elements chosen from scandium, titanium, vanadium, chromium, manganese, iron, cobalt, nickel, copper, zinc, yttrium, zirconium, niobium, molybdenum, ruthenium, rhodium, palladium, silver, cadmium, lanthanum, hafnium, tantalum, tungsten, rhenium, osmium, iridium, platinum, gold, mercury, aluminum, gallium, indium, thallium, tin, lead, bismuth, carbon, nitrogen, fluorine, phosphorus, sulfur, chlorine, selenium, bromine, iodine, boron, silicon, germanium, arsenic, antimony, and tellurium; O is oxygen; u ranges from 0.95 to 6; and
a noble metal enriched region having an average crystallite size with a diameter ranging from ten nanometers to one thousand nanometers.

### Claim 2 (depends on 1)

The coated component of claim 1, wherein A is barium or strontium, E is lithium, sodium, or potassium, L is lanthanum, cerium, praseodymium, neodymium, samarium, gadolinium, or ytterbium, and M is scandium, titanium, vanadium, chromium, manganese, iron, cobalt, nickel, copper, zinc, yttrium, zirconium, niobium, molybdenum, tungsten, aluminum, gallium, indium, thallium, tin, lead, silicon, or germanium.

### Claim 3 (depends on 1)

The coated component of claim 1, wherein the metal oxide is one or more composition chosen from Co3O4, NixCo3−xO4, FexCo3−xO4, CuxCo3−xO4, CrxCo3−xO4, Pr6O11, LiMn2O4, Al2O3, PbO, Pb1−xSrxCoO3, Pb1−xBaxCoO3, SrCoOu, BaCoOu, LnxA1−xCoOu, Sr0.8Pr0.2CoO3, Ba0.8Ce0.2CoO3, Ba0.8Pr0.2CoO3, LnxCaySrzBa[1−(x+y+z)]CoO3, LnxLiySrzBa[1−(x+y+z)]CoO3, a cobaltite, a manganite, a chromite, a ferrite perovskite, xMoO3-yCo3O4-zLi2O, MxEyCo3−(x+y)Ou, MxEyAzCo3−(x+y+z)Ou, Mn2O3, Mn3O4, Mn2O7, Mn doped TiO2, Fe2O3, Fe3O4, ZnFe2O4, BixSn1−xOu, InxSnyOz, Bi2O3—Co3O4, and CeO2.

### Claim 4 (depends on 1)

The coated component of claim 1, wherein the metal oxide enriched region comprises an amount of a noble metal.

### Claim 5 (depends on 1)

The coated component of claim 1, wherein the diameter of the average crystallite size of the metal oxide enriched region ranges from twenty nanometers to five hundred nanometers and the diameter of the average crystallite size of the noble metal enriched region ranges from twenty nanometers to five hundred nanometers.

### Claim 6 (depends on 1)

The coated component of claim 1, wherein the metal oxide has an optical basicity ranging from 0.8 to 1.95.

### Claim 7 (depends on 1)

The coated component of claim 1, wherein the catalytic coating comprises:
a plurality of metal oxide enriched regions, wherein each of the plurality of metal oxide enriched regions is a crystallite having a diameter ranging from ten nanometers to one thousand nanometers; and
a plurality of noble metal enriched regions, wherein each of the plurality of noble metal enriched regions is a crystallite having a diameter ranging from ten nanometers to one thousand nanometers,
wherein the plurality of metal oxide enriched regions and the plurality of noble metal enriched regions are distributed throughout the catalytic coating.

### Claim 8 (depends on 1)

The coated component of claim 1, wherein the catalytic coating comprises:
two or more metal oxide enriched regions each having an average crystallite size with a diameter ranging from ten nanometers to one thousand nanometers wherein each metal oxide enriched region is enriched in a metal oxide of formula AxEyLzMOu; and
two or more noble metal enriched regions each having an average crystallite size with a diameter ranging from ten nanometers to one thousand nanometers.

### Claim 9 (depends on 1)

The coated component of claim 1, wherein the catalytic coating comprises:
two or more metal oxide enriched regions each having an average crystallite size with a diameter ranging from ten nanometers to one thousand nanometers wherein each metal oxide enriched region is enriched in a metal oxide of formula AxEyLzMOu; and
two or more noble metal enriched regions each having an average crystallite size with a diameter ranging from ten nanometers to one thousand nanometers,
wherein the two or more metal oxide enriched regions are in a layered arrangement with the two or more noble metal enriched regions.

### Claim 10 (depends on 1)

The coated component of claim 1, wherein the substrate is a metal substrate, a ceramic substrate, a metal substrate coated with a ceramic layer, or a ceramic substrate coated with a metal layer.

### Claim 11 (depends on 1)

The coated component of claim 1, wherein the substrate is a metal substrate chosen from iron-based alloys, nickel-based alloys, cobalt-based alloys, alloys containing cobalt and chromium, alloys containing platinum and aluminum, alloys containing nickel and aluminum, and alloys containing nickel, chromium, aluminum, and yttrium.

### Claim 12 (depends on 1)

The coated component of claim 1, wherein the coated component is a gas turbine engine component.

### Claim 13 (depends on 1)

The coated component of claim 1, wherein the coated component is an aircraft component chosen from a fluid passage, a nozzle, a valve orifice, a vane, a pilot orifice, a main orifice, a valve, a swirler, a venturi, a heat exchanger, an aft heat shield, and a lube oil system component.

### Claim 14 (depends on 1)

The coated component of claim 1, wherein the catalytic coating has a thickness ranging from 0.02 micron to ten microns.

### Claim 15 (depends on 1)

The coated component of claim 1, wherein the substrate is a metal substrate coated with a ceramic layer and the ceramic layer is a thermal barrier coating.

### Claim 16 (depends on 1)

The coated component of claim 1, wherein the substrate is a metal substrate coated with a ceramic layer and the ceramic layer is a thermal barrier coating comprising (ZrO2)(1−q)(Y2O3)q, wherein q ranges from 0.04 to 0.5.

### Claim 17 (depends on 1)

The coated component of claim 1, wherein u ranges from 0.95 to three.

### Claim 18 (depends on 1)

A method of oxidizing coke, the method comprising:
contacting the coke with the coated component of claim 1 at a temperature ranging from three hundred degrees Fahrenheit to one thousand one hundred degrees Fahrenheit,
wherein the coke is selectively oxidized by the catalytic coating in the presence of a hydrocarbon fuel.

### Claim 19 (depends on 1)

A method of making the coated component of claim 1, the method comprising:
at least one metal oxide depositing step, wherein the metal oxide of formula AxEyLzMOu is deposited as a metal oxide layer;
at least one noble metal depositing step, wherein the noble metal is deposited as a noble metal layer; and
a heating step at a temperature ranging from three hundred degrees Fahrenheit to one thousand seven hundred degrees Fahrenheit, wherein the heating step occurs after the at least one metal oxide depositing step and after the at least one noble metal depositing step,
wherein one of the at least one noble metal depositing step deposits the noble metal on the substrate or one of the at least one metal oxide depositing step deposits the metal oxide on the substrate.

### Claim 20 (depends on 19)

The method of claim 19, wherein a duration of the heating step and the temperature of the heating step are sufficient to form metal oxide enriched crystallites and noble metal enriched crystallites that are homogenously distributed throughout the catalytic coating.