# US 2026/0085446 A1 · Silicon carbide semiconductor device including a buffer layer and manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0085446 A1
- Document ID: US20260085446A1
- Status: Published application
- Kind: A1
- Application number: 19/317,296
- Filed: 2025-09-03
- Published: 2026-03-26
- Earliest claimed: 2024-09-23
- Assignees: Infineon Technologies AG
- Applicants: Infineon Technologies AG
- Inventors: Christian Zmölnig; Thomas Söllradl; Christoffer Erbert
- Web page: https://patentgrep.com/patent/US20260085446A1

## CPC

- C30B 25/183: {being provided with a buffer layer, e.g. a lattice matching layer}
- C30B 25/20: the substrate being of the same materials as the epitaxial layer
- C30B 29/36: Carbides
- H10D 62/157: {Impurity concentrations or distributions}
- H10D 62/60: Impurity distributions or concentrations
- H10D 62/8325: {Silicon carbide}
- H10P 14/20: of semiconductor materials
- H10P 14/2904: {Silicon carbide}
- H10P 14/3208: {Silicon carbide}
- H10P 14/3408: {Silicon carbide}
- H10D 12/032: {of vertical IGBTs}
- H10D 12/417: {having a drift region having a doping concentration that is higher at the collector side relative to other parts of the drift region}
- H10D 12/441: {Vertical IGBTs}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A silicon carbide (SiC) semiconductor device is proposed. The SiC semiconductor device includes a buffer layer of a first conductivity type and a drift layer of the first conductivity type arranged, along a vertical direction, on the buffer layer. A vertical profile of a doping concentration of the buffer layer includes at least a first valley portion, a first plateau portion and a first transition portion extending from the first valley portion to the first plateau portion. The doping concentration of each of the first valley portion or the first plateau portion varies by less than 20 %. A vertical extent of the first transition portion ranges from 1 % to 30 % of a vertical extent of the first valley portion.

## Claims

### Claim 1

A silicon carbide (SiC) semiconductor device, comprising:
a buffer layer of a first conductivity type;
a drift layer of the first conductivity type arranged, along a vertical direction, on the buffer layer,
wherein a vertical profile of a doping concentration of the buffer layer includes at least a first valley portion, a first plateau portion and a first transition portion extending from the first valley portion to the first plateau portion,
wherein a doping concentration of each of the first valley portion or the first plateau portion varies by less than 20 %, and
wherein a vertical extent of the first transition portion ranges from 1 % to 30 % of a vertical extent of the first valley portion.

### Claim 2 (depends on 1)

The SiC semiconductor device of claim 1, wherein the vertical extent of the first transition portion ranges from 1 % to 30 % of a vertical extent of the first plateau portion.

### Claim 3 (depends on 1)

The SiC semiconductor device of claim 1, wherein the doping concentration of the first plateau portion ranges from 1×1017 cm−3 to 1×1019 cm−3.

### Claim 4 (depends on 1)

The SiC semiconductor device of claim 1, wherein a doping concentration of the first valley portion ranges from 1×1016 cm−3 to 1×1018 cm−3.

### Claim 5 (depends on 1)

The SiC semiconductor device of claim 1, wherein a vertical extent of the first plateau portion and the vertical extent of the first valley portion differ by less than 20 %.

### Claim 6 (depends on 1)

The SiC semiconductor device of claim 1, wherein the vertical extent of the first valley portion ranges from 100 nm to 2 μm.

### Claim 7 (depends on 1)

The SiC semiconductor device of claim 1, wherein the buffer layer further includes an end portion adjoining the drift layer, and wherein a profile of a doping concentration of the end portion continuously decreases toward the drift layer.

### Claim 8 (depends on 1)

The SiC semiconductor device of claim 1, wherein the buffer layer further includes a second plateau portion and a second transition portion extending from the second plateau portion to the first valley portion.

### Claim 9 (depends on 8)

The SiC semiconductor device of claim 8, wherein a doping concentration of the second plateau portion varies by less than 20 %, and wherein a vertical extent of the second transition portion ranges from 1 % to 30 % of the vertical extent of the first valley portion.

### Claim 10 (depends on 8)

The SiC semiconductor device of claim 8, wherein an average doping concentration of the second plateau portion and an average doping concentration of the first plateau portion differ by less than 20 %.

### Claim 11 (depends on 8)

The SiC semiconductor device of claim 8, wherein an average doping concentration of the second plateau portion is a factor of 1.5 to 30 larger than an average doping concentration of the first plateau portion.

### Claim 12 (depends on 8)

The SiC semiconductor device of claim 8, wherein a vertical extent of the second plateau portion and the vertical extent of the first valley portion differ by less than 20 %.

### Claim 13 (depends on 1)

The SiC semiconductor device of claim 1, wherein the buffer layer further includes a second valley portion and an additional transition portion extending from the first plateau portion to the second valley portion, wherein a doping concentration of the second valley portion varies by less than 20 %, and wherein a vertical extent of the additional transition portion ranges from 1 % to 30 % of a vertical extent of the second valley portion.

### Claim 14 (depends on 13)

The SiC semiconductor device of claim 13, wherein an average doping concentration of the second valley portion and an average doping concentration of the first valley portion differ by less than 20 %.

### Claim 15 (depends on 13)

The SiC semiconductor device of claim 13, wherein an average doping concentration of the first valley portion is a factor of 1.5 to 30 larger than an average doping concentration of the second valley portion.

### Claim 16 (depends on 1)

The SiC semiconductor device of claim 1, wherein a vertical profile of the doping concentration of the first valley portion, the first plateau portion and the first transition portion is an in-situ doping concentration profile.

### Claim 17

A method of manufacturing a silicon carbide (SiC) semiconductor device, the method comprising:
forming a buffer layer of a first conductivity type; and
forming a drift layer of the first conductivity type arranged, along a vertical direction, on the buffer layer,
wherein a vertical profile of a doping concentration of the buffer layer includes at least a first valley portion, a first plateau portion and a first transition portion extending from the first valley portion to the first plateau portion,
wherein a doping concentration of each of the first valley portion or the first plateau portion varies by less than 20 %, and
wherein a vertical extent of the first transition portion ranges from 1 % to 30 % of a vertical extent of the first valley portion.

### Claim 18 (depends on 17)

The method of claim 17, wherein a vertical profile of the doping concentration of the first valley portion, the first plateau portion and the first transition portion is formed by in-situ doping.

### Claim 19 (depends on 17)

The method of claim 17, wherein the buffer layer is formed on a SiC substrate by an epitaxial layer deposition process, and wherein the drift layer is formed on the buffer layer by an epitaxial layer deposition process.