# US 2026/0085414 A1 · Method and apparatus for forming metal silicide layer on substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0085414 A1
- Document ID: US20260085414A1
- Status: Published application
- Kind: A1
- Application number: 19/304,635
- Filed: 2025-08-20
- Published: 2026-03-26
- Earliest claimed: 2024-08-27
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Tatsuya SANO; Liang Kai ONG
- Web page: https://patentgrep.com/patent/US20260085414A1

## CPC

- C23C 16/14: Deposition of only one other metal element
- C23C 16/45527: {characterized by the ALD cycle, e.g. different flows or temperatures during half-reactions, unusual pulsing sequence, use of precursor mixtures or auxiliary reactants or activations}
- C23C 16/0209: {by heating}
- C23C 16/08: from metal halides
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- C23C 16/42: Silicides
- C23C 16/45512: {Premixing before introduction in the reaction chamber}
- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C 16/45544: {characterized by the apparatus}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/45557: {Pulsed pressure or control pressure}
- C23C 16/45561: {Gas plumbing upstream of the reaction chamber}
- C23C 16/45565: {Shower nozzles}
- C23C 16/45574: {Nozzles for more than one gas}
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method for forming a metal silicide layer on a substrate, the method including: heating the substrate from which a silicon layer is exposed to a temperature in a range of 490 degrees C. or higher and 600 degrees C. or lower; preliminarily supplying a raw material gas, which is a metal halide gas containing a metal that constitutes the metal silicide and a halogen, to the heated substrate; and forming a layer of the metal on a surface of the silicon layer by alternately and repeatedly supplying the raw material gas and a reactive gas, which reacts with the metal halide to obtain the metal, to the substrate to which the raw material gas has been preliminarily supplied, wherein the metal silicide layer is formed by diffusing silicon from the silicon layer into the layer of the metal.

## Claims

### Claim 1

A method for forming a metal silicide layer on a substrate, the method comprising:
heating the substrate from which a silicon layer is exposed to a temperature in a range of 490 degrees C. or higher and 600 degrees C. or lower;
preliminarily supplying a raw material gas, which is a metal halide gas containing a metal that constitutes the metal silicide and a halogen, to the heated substrate; and
forming a layer of the metal on a surface of the silicon layer by alternately and repeatedly supplying the raw material gas and a reactive gas, which reacts with the metal halide to obtain the metal, to the substrate to which the raw material gas has been preliminarily supplied,
wherein the metal silicide layer is formed by diffusing silicon from the silicon layer into the layer of the metal.

### Claim 2 (depends on 1)

The method of claim 1, wherein a supply time of the raw material gas which has been preliminarily supplied is longer than a supply time of the raw material gas in each cycle of alternately supplying the raw material gas and the reactive gas.

### Claim 3 (depends on 2)

The method of claim 2, wherein the supply time of the raw material gas which has been preliminarily supplied is in a range of 5 seconds or more and 90 seconds or less.

### Claim 4 (depends on 2)

The method of claim 2, wherein the supply time of the raw material gas in each cycle of alternately supplying the raw material gas and the reactive gas is in a range of 0.1 second or more and 1 second or less.

### Claim 5 (depends on 1)

The method of claim 1, wherein a pressure of a processing atmosphere in which the substrate is placed when the raw material gas is preliminarily supplied is higher than a pressure of a processing atmosphere in which the substrate is placed when the raw material gas and the reactive gas are alternately supplied.

### Claim 6 (depends on 5)

The method of claim 5, wherein the pressure of the processing atmosphere in which the substrate is placed when the raw material gas is preliminarily supplied is in a range of 1.33 kPa or more and 5.33 kPa or less.

### Claim 7 (depends on 5)

The method of claim 5, wherein the pressure of the processing atmosphere in which the substrate is placed when the raw material gas and the reactive gas are alternately supplied is in a range of 133.3 Pa or more and 266.6 Pa or less.

### Claim 8 (depends on 1)

The method of claim 1, wherein the metal is molybdenum, and the metal silicide is molybdenum silicide.

### Claim 9

A method for forming a metal silicide layer on a substrate, the method comprising:
heating the substrate from which a silicon layer is exposed to a temperature in a range of 400 degrees C. or higher and 510 degrees C. or lower; and
forming a layer of the metal on a surface of the silicon layer by alternately supplying a raw material gas, which is a metal halide gas containing a metal that constitutes the metal silicide and a halogen, and a reactive gas, which reacts with the metal halide to obtain the metal, to the heated substrate,
wherein the metal silicide layer is formed by diffusing silicon from the silicon layer into the metal layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein a supply time of the raw material gas in each cycle of alternately supplying the raw material gas and the reactive gas is in a range of 0.1 second or more and 1 second or less.

### Claim 11 (depends on 9)

The method of claim 9, wherein a pressure of a processing atmosphere in which the substrate is placed when the raw material gas and the reactive gas are alternately supplied is in a range of 133.3 Pa or more and 266.6 Pa or less.

### Claim 12 (depends on 9)

The method of claim 9, wherein the metal is molybdenum, and the metal silicide is molybdenum silicide.

### Claim 13 (depends on 12)

The method of claim 12, wherein the molybdenum silicide includes a tetragonal crystal.

### Claim 14 (depends on 12)

The method of claim 12, wherein the raw material gas is a molybdenum pentachloride gas, and the reactive gas is a hydrogen gas.

### Claim 15

An apparatus for forming a metal silicide layer on a substrate, comprising:
a processing container including a stage on which the substrate is placed, wherein a silicon layer is exposed from the substrate;
a heater configured to heat the substrate placed on the stage;
a raw material gas supply configured to supply a raw material gas, which is a metal halide gas containing a metal that constitutes the metal silicide and a halogen, into the processing container;
a reactive gas supply configured to supply a reactive gas, which reacts with the metal halide to obtain the metal, into the processing container; and
a controller,
wherein the controller is configured to output control signals to execute:
heating the substrate to a temperature in a range of 490 degrees C. or higher and 600 degrees C. or lower;
preliminarily supplying the raw material gas to the heated substrate; and
forming a layer of the metal on a surface of the silicon layer by alternately and repeatedly supplying the raw material gas and the reactive gas to the substrate to which the raw material gas has been preliminarily supplied, and
wherein the metal silicide layer is formed by diffusing silicon from the silicon layer into the layer of the metal.

### Claim 16 (depends on 15)

The apparatus of claim 15, wherein the metal is molybdenum, and the metal silicide is molybdenum silicide.

### Claim 17

An apparatus for forming a metal silicide layer on a substrate, comprising:
a processing container including a stage on which the substrate is placed, wherein a silicon layer is exposed from the substrate;
a heater configured to heat the substrate placed on the stage;
a raw material gas supply configured to supply a raw material gas, which is a metal halide gas containing a metal that constitutes the metal silicide and a halogen, to the processing container;
a reactive gas supply configured to supply a reactive gas, which reacts with the metal halide to obtain the metal, to the processing container; and
a controller,
wherein the controller is configured to output control signals to execute:
heating the substrate to a temperature in a range of 400 degrees C. or higher and 510 degrees C. or lower; and
forming a layer of the metal on a surface of the silicon layer by alternately and repeatedly supplying the raw material gas and the reactive gas to the heated substrate, and
wherein metal silicide layer is formed by diffusing silicon from the silicon layer into the layer of the metal.

### Claim 18 (depends on 17)

The apparatus of claim 17, wherein the metal is molybdenum, and the metal silicide is molybdenum silicide.

### Claim 19 (depends on 18)

The apparatus of claim 18, wherein the raw material gas is a molybdenum pentachloride gas, and the reactive gas is a hydrogen gas.