# US 2026/0085373 A1 · High strength steel sheet having superior workability and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0085373 A1
- Document ID: US20260085373A1
- Status: Published application
- Kind: A1
- Application number: 19/409,457
- Filed: 2025-12-04
- Published: 2026-03-26
- Earliest claimed: 2019-12-18
- Assignees: Posco
- Applicants: Posco
- Inventors: Jae-Hoon LEE; Tae-Kyo HAN; Sang-Hwan LEE
- Web page: https://patentgrep.com/patent/US20260085373A1

## CPC

- C21D 1/19: by interrupted quenching
- C21D 9/46: for sheet metals
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/007: {containing Co}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0426: {Hot rolling}
- C21D 8/0436: {Cold rolling}
- C21D 8/0473: {Final recrystallisation annealing}
- C21D 9/48: deep-drawing sheets
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/10: containing cobalt
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/38: with more than 1.5% by weight of manganese
- C21D 1/185: {from an intercritical temperature}
- C21D 8/04: to produce plates or strips for drawing, e.g. for deep-drawing
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided is a method for manufacturing a steel steel sheet having superior workability. The method includes: providing a cold-rolled steel sheet; primarily heating the cold-rolled steel sheet to Ac1-Ac3, and primarily maintaining the primarily heated steel sheet for 50 seconds or more; primarily cooling the primarily heated steel sheet to 600-850° C. at an average cooling rate of 1° C./s or more; secondarily cooling the primarily cooled steel sheet to 300-500° C. at an average cooling rate of 2° C./s or more, and secondarily maintaining the secondarily cooled steel sheet for 5 seconds or more; tertiarily cooling the secondarily cooled steel sheet to 100-300° C. at an average cooling rate of 2° C./s or more; secondarily heating the tertiarily cooled steel sheet to 300-500° C. at an average temperature increase rate of 5° C./s or more, and tertiarily maintaining the secondarily heated steel sheet for 50 seconds or more; and quaternarily cooling to room temperature.

## Claims

### Claim 1

A method for manufacturing a steel strength steel sheet having superior workability, the method comprising:
providing a cold-rolled steel sheet including, by wt %, C: 0.25 to 0.75%, Si: 4.0% or less, Mn: 0.9 to 5.0%, Al: 5.0% or less, P: 0.15% or less, S: 0.03% or less, N: 0.03% or less, and a balance of Fe and unavoidable impurities;
heating (primarily heating) the cold-rolled steel sheet to a temperature within a range of Ac1 or higher and less than Ac3, and maintaining (primarily maintaining) the primarily heated steel sheet for 50 seconds or more;
cooling (primarily cooling) the primarily heated steel sheet to a temperature within a range (primarily cooling stop temperature) of 600 to 850° C. at an average cooling rate of 1° C./s or more;
cooling (secondarily cooling) the primarily cooled steel sheet to a temperature within a range of 300 to 500° C. at an average cooling rate of 2° C./s or more, and maintaining (secondarily maintaining) the secondarily cooled steel sheet in the temperature within a range for 5 seconds or more;
cooling (tertiarily cooling) the secondarily cooled steel sheet to a temperature within a range (secondarily cooling stop temperature) of 100 to 300° C. at an average cooling rate of 2° C./s or more;
heating (secondarily heating) the tertiarily cooled steel sheet to a temperature within a range of 300 to 500° C. at an average temperature increase rate of 5° C./s or more, and maintaining (tertiarily maintaining) the secondarily heated steel sheet in the temperature within a range for 50 seconds or more; and
cooling (quaternarily cooling) the secondarily heated steel sheet to room temperature.

### Claim 2 (depends on 1)

The high strength steel sheet of claim 1, wherein the cold-rolled steel sheet further includes any one or more of the following (1) to (9):
(1) one or more of Ti: 0 to 0.5%, Nb: 0 to 0.5%, and V: 0 to 0.5%,
(2) one or more of Cr: 0 to 3.0% and Mo: 0 to 3.0%,
(3) one or more of Cu: 0 to 4.5% and Ni: 0 to 4.5%,
(4) B: 0 to 0.005%,
(5) one or more of Ca: 0 to 0.05%, REM: 0 to 0.05% excluding Y, and Mg: 0 to 0.05%,
(6) one or more of W: 0 to 0.5% and Zr: 0 to 0.5%,
(7) one or more of Sb: 0 to 0.5% and Sn: 0 to 0.5%,
(8) one or more of Y: 0 to 0.2% and Hf: 0 to 0.2%, and
(9) Co: 0 to 1.5%.

### Claim 3 (depends on 1)

The high strength steel sheet of claim 1, wherein a total content (Si+Al) of Si and Al included in the cold-rolled steel sheet is 1.0 to 6.0 wt %.

### Claim 4 (depends on 1)

The method of claim 1, wherein the cold-rolled steel sheet is provided by:
heating a steel slab to 1000 to 1350° C.;
performing finishing hot rolling in a temperature within a range of 800 to 1000° C.;
coiling the hot-rolled steel sheet in a temperature within a range of 300 to 600° C.;
performing hot-rolled annealing heat treatment on the coiled steel sheet in a temperature within a range of 650 to 850° C. for 600 to 1700 seconds; and
cold rolling the hot-rolled annealing heat-treated steel sheet at a reduction ratio of 30 to 90%.

### Claim 5 (depends on 1)

The high strength steel sheet of claim 1, wherein a cooling rate Vc1 of the primary cooling and a cooling rate Vc2 of the secondary cooling satisfy a relationship of Vc1<Vc2.